公开(公告)号:US12084745B2
公开(公告)日:2024-09-10
申请号:US17192125
申请日:2021-03-04
发明人: Ryusuke Tsubota , Yohei Oka , Akira Okamoto , Takayuki Nakamoto , Takahiro Sugahara , Naruaki Shinomiya , Mamoru Takemura , Sohei Uchida
IPC分类号: C22C1/04 , B22F3/24 , B22F10/00 , B22F10/25 , B22F10/28 , B22F10/32 , B22F10/36 , B22F10/64 , B33Y10/00 , B33Y70/00 , C22C9/00 , C22C9/06 , C22F1/08 , B22F10/80 , B22F12/41 , B22F12/67 , B33Y80/00
CPC分类号: C22C1/0425 , B22F3/24 , B22F10/00 , B22F10/28 , B22F10/64 , B33Y70/00 , C22C9/00 , C22C9/06 , C22F1/08 , B22F2003/248 , B22F10/25 , B22F10/32 , B22F10/36 , B22F10/80 , B22F12/41 , B22F12/67 , B22F2998/10 , B33Y10/00 , B33Y80/00 , Y02P10/25 , B22F2998/10 , B22F10/00 , B22F2003/248 , B22F2998/10 , B22F10/28 , B22F2003/248
摘要: A copper alloy powder is a copper alloy powder for additive manufacturing. The copper alloy powder contains more than 1.00 mass % and not more than 2.80 mass % of chromium, and a balance of copper. A method for producing an additively-manufactured article includes a first step of preparing a copper alloy powder containing more than 1.00 mass % and not more than 2.80 mass % of chromium and a balance of copper and a second step of producing the additively-manufactured article from the copper alloy powder, and the additively-manufactured article is produced such that forming a powder layer including the copper alloy powder, and solidifying the copper alloy powder at a predetermined position in the powder layer to form a shaped layer are sequentially repeated to stack such shaped layers to thus produce the additively-manufactured article.
-
公开(公告)号:US10981226B2
公开(公告)日:2021-04-20
申请号:US15791675
申请日:2017-10-24
发明人: Ryusuke Tsubota , Yohei Oka , Akira Okamoto , Takayuki Nakamoto , Takahiro Sugahara , Naruaki Shinomiya , Mamoru Takemura , Sohei Uchida
IPC分类号: B22F3/105 , C22C1/04 , B33Y70/00 , C22C9/00 , B33Y10/00 , B33Y80/00 , C22F1/08 , B22F3/24 , C22C9/06
摘要: A copper alloy powder is a copper alloy powder for additive manufacturing. The copper alloy powder contains more than 1.00 mass % and not more than 2.80 mass % of chromium, and a balance of copper. A method for producing an additively-manufactured article includes a first step of preparing a copper alloy powder containing more than 1.00 mass % and not more than 2.80 mass % of chromium and a balance of copper and a second step of producing the additively-manufactured article from the copper alloy powder, and the additively-manufactured article is produced such that forming a powder layer including the copper alloy powder, and solidifying the copper alloy powder at a predetermined position in the powder layer to form a shaped layer are sequentially repeated to stack such shaped layers to thus produce the additively-manufactured article.
-
公开(公告)号:US11077495B2
公开(公告)日:2021-08-03
申请号:US15657348
申请日:2017-07-24
发明人: Ryusuke Tsubota , Junichi Tanaka , Yohei Oka , Takayuki Nakamoto , Takahiro Sugahara , Mamoru Takemura , Sohei Uchida
IPC分类号: B22F1/00 , C22C1/04 , C22C9/00 , C22C9/10 , C22C9/06 , B22F12/00 , B22F3/24 , B22F10/10 , B33Y10/00 , B33Y70/00 , B33Y80/00 , B22F9/08
摘要: A metal powder contains not less than 0.10 mass % and not more than 1.00 mass % of at least one of chromium and silicon, and a balance of copper. The total content of the chromium and the silicon is not more than 1.00 mass %. In accordance with an additive manufacturing method for this metal powder, an additively-manufactured article made from a copper alloy is provided. The additively-manufactured article has both an adequate mechanical strength and an adequate electrical conductivity.
-
公开(公告)号:US10421122B2
公开(公告)日:2019-09-24
申请号:US15657300
申请日:2017-07-24
发明人: Ryusuke Tsubota , Junichi Tanaka , Yohei Oka , Takayuki Nakamoto , Takahiro Sugahara , Mamoru Takemura , Sohei Uchida
IPC分类号: B22F1/00 , B22F3/105 , C22C1/04 , C22C9/00 , C22C9/10 , B22F3/24 , C22C9/06 , B33Y10/00 , B33Y70/00 , B33Y80/00 , B22F9/08
摘要: A metal powder contains not less than 0.10 mass % and not more than 1.00 mass % of at least one of chromium and silicon, and a balance of copper. The total content of the chromium and the silicon is not more than 1.00 mass %. In accordance with an additive manufacturing method for this metal powder, an additively-manufactured article made from a copper alloy is provided. The additively-manufactured article has both an adequate mechanical strength and an adequate electrical conductivity.
-
-
-