公开(公告)号:US20140100300A1
公开(公告)日:2014-04-10
申请号:US14103192
申请日:2013-12-11
Applicant: FINA TECHNOLOGY, INC.
Inventor: John Gaustad , Juan Aguirre , Joe Shuler
IPC: C08F30/04
CPC classification number: C08F30/04 , C08F212/08 , C08F220/06 , C08F230/04 , C08J5/18 , C08J9/00 , C08J9/04 , C08J2325/14 , C08K5/0091 , C08L35/06 , C08L35/00 , C08F220/14 , C08F222/10
Abstract: Embodiments of the present invention include a branched aromatic ionomer, and a process of making it, by co-polymerizing a first monomer comprising an aromatic moiety and an unsaturated alkyl moiety and a second monomer represented by the general formula: [R-AZ]y-MX wherein R is a hydrocarbon chain having from 2 to 40 carbons and at least one polymerizable unsaturation; A is an anionic group; M is a cationic group; Z is −1 or −2; X is +1, +2, +3, +4, or +5; and y is an integer having a value of from 1 to 4. The branched aromatic ionomer has a melt flow index ranging from 1.0 g/10 min. to 13 g/10 min. Optionally the melt flow index ranges from 1.3 g/10 min. to 1.9 g/10 min.
Abstract translation: 本发明的实施方案包括支链芳族离聚物及其制备方法,通过共聚合包含芳族部分和不饱和烷基部分的第一单体和由通式[R-AZ] y表示的第二单体 -MX,其中R是具有2至40个碳的烃链和至少一个可聚合不饱和度; A是阴离子基团; M是阳离子基团; Z为-1或-2; X是+1,+2,+3,+4或+5; y为1〜4的整数。支链芳族离聚物的熔体流动指数为1.0g / 10min。 至13g / 10min。 任选地,熔体流动指数为1.3g / 10min。 至1.9g / 10分钟。
-
公开(公告)号:US20200262946A1
公开(公告)日:2020-08-20
申请号:US16795790
申请日:2020-02-20
Applicant: FINA TECHNOLOGY, INC.
Inventor: Michael McLeod , Russell McDonald , Joe Shuler , Mahesh Patkar , Marc Mayhall
Abstract: A process forming a high MFR polypropylene includes providing a reactor powder polypropylene, the reactor powder polypropylene having a melt flow rate of less than 100 dg/min. The process also includes mixing the reactor powder polypropylene with a free-radical initiator to form a powder/initiator mixture and subjecting the powder/initiator mixture to post-reactor forming. The present disclosure further provides for a vis-broken polypropylene and a polymer article.
-
公开(公告)号:US08889755B2
公开(公告)日:2014-11-18
申请号:US14103192
申请日:2013-12-11
Applicant: Fina Technology, Inc.
Inventor: John Gaustad , Juan Aguirre , Joe Shuler
IPC: C08F30/04 , C08J5/18 , C08K5/00 , C08J9/04 , C08J9/00 , C08L35/06 , C08F230/04 , C08F212/08 , C08F220/06
CPC classification number: C08F30/04 , C08F212/08 , C08F220/06 , C08F230/04 , C08J5/18 , C08J9/00 , C08J9/04 , C08J2325/14 , C08K5/0091 , C08L35/06 , C08L35/00 , C08F220/14 , C08F222/10
Abstract: Embodiments of the present invention include a branched aromatic ionomer, and a process of making it, by co-polymerizing a first monomer comprising an aromatic moiety and an unsaturated alkyl moiety and a second monomer represented by the general formula: [R-AZ]y-MX wherein R is a hydrocarbon chain having from 2 to 40 carbons and at least one polymerizable unsaturation; A is an anionic group; M is a cationic group; Z is −1 or −2; X is +1, +2, +3, +4, or +5; and y is an integer having a value of from 1 to 4. The branched aromatic ionomer has a melt flow index ranging from 1.0 g/10 min. to 13 g/10 min. Optionally the melt flow index ranges from 1.3 g/10 min. to 1.9 g/10 min.
Abstract translation: 本发明的实施方案包括支链芳族离聚物及其制备方法,通过共聚合包含芳族部分和不饱和烷基部分的第一单体和由通式[R-AZ] y表示的第二单体 -MX,其中R是具有2至40个碳的烃链和至少一个可聚合不饱和度; A是阴离子基团; M是阳离子基团; Z为-1或-2; X是+1,+2,+3,+4或+5; y为1〜4的整数。支链芳族离聚物的熔体流动指数为1.0g / 10min。 至13g / 10min。 任选地,熔体流动指数为1.3g / 10min。 至1.9g / 10分钟。
-
公开(公告)号:US08653212B2
公开(公告)日:2014-02-18
申请号:US13964781
申请日:2013-08-12
Applicant: Fina Technology, Inc.
Inventor: John Gaustad , Juan Aguirre , Joe Shuler
CPC classification number: C08F30/04 , C08F212/08 , C08F220/06 , C08F230/04 , C08J5/18 , C08J9/00 , C08J9/04 , C08J2325/14 , C08K5/0091 , C08L35/06 , C08L35/00 , C08F220/14 , C08F222/10
Abstract: Embodiments of the present invention include a branched aromatic ionomer, and a process of making it, by co-polymerizing a first monomer comprising an aromatic moiety and an unsaturated alkyl moiety and a second monomer represented by the general formula: [R-AZ]y-MX wherein R is a hydrocarbon chain having from 2 to 40 carbons and at least one polymerizable unsaturation; A is an anionic group; M is a cationic group; Z is −1 or −2; X is +1, +2, +3, +4, or +5; and y is an integer having a value of from 1 to 4. The branched aromatic ionomer has a melt flow index ranging from 1.0 g/10 min. to 13 g/10 min. Optionally the melt flow index ranges from 1.3 g/10 min. to 1.9 g/10 min.
Abstract translation: 本发明的实施方案包括支链芳族离聚物及其制备方法,通过共聚合包含芳族部分和不饱和烷基部分的第一单体和由通式[R-AZ] y表示的第二单体 -MX,其中R是具有2至40个碳的烃链和至少一个可聚合不饱和度; A是阴离子基团; M是阳离子基团; Z为-1或-2; X是+1,+2,+3,+4或+5; y为1〜4的整数。支链芳族离聚物的熔体流动指数为1.0g / 10min。 至13g / 10min。 任选地,熔体流动指数为1.3g / 10min。 至1.9g / 10分钟。
-
公开(公告)号:US20130331471A1
公开(公告)日:2013-12-12
申请号:US13964781
申请日:2013-08-12
Applicant: Fina Technology, Inc.
Inventor: John Gaustad , Juan Aguirre , Joe Shuler
IPC: C08F230/04 , C08L35/06
CPC classification number: C08F30/04 , C08F212/08 , C08F220/06 , C08F230/04 , C08J5/18 , C08J9/00 , C08J9/04 , C08J2325/14 , C08K5/0091 , C08L35/06 , C08L35/00 , C08F220/14 , C08F222/10
Abstract: Embodiments of the present invention include a branched aromatic ionomer, and a process of making it, by co-polymerizing a first monomer comprising an aromatic moiety and an unsaturated alkyl moiety and a second monomer represented by the general formula: [R-AZ]y-MX wherein R is a hydrocarbon chain having from 2 to 40 carbons and at least one polymerizable unsaturation; A is an anionic group; M is a cationic group; Z is −1 or −2; X is +1, +2, +3, +4, or +5; and y is an integer having a value of from 1 to 4. The branched aromatic ionomer has a melt flow index ranging from 1.0 g/10 min. to 13 g/10 min. Optionally the melt flow index ranges from 1.3 g/min. to 1.9 g/10 min.
Abstract translation: 本发明的实施方案包括支链芳族离聚物及其制备方法,通过共聚合包含芳族部分和不饱和烷基部分的第一单体和由通式[R-AZ] y表示的第二单体 -MX,其中R是具有2至40个碳的烃链和至少一个可聚合不饱和度; A是阴离子基团; M是阳离子基团; Z为-1或-2; X是+1,+2,+3,+4或+5; y为1〜4的整数。支链芳族离聚物的熔体流动指数为1.0g / 10min。 至13g / 10min。 任选地,熔体流动指数为1.3g / min。 至1.9g / 10分钟。
-
-
-
-