Abstract:
A method for producing β-sialon fluorescent material having excellent emission intensity is provided. The method for producing β-sialon fluorescent material includes providing a composition comprising silicon nitride that contains aluminium, an oxygen atom, and europium, heat treating the composition, contacting the heat-treated composition with a basic substance, and washing the composition, which has been contacted with the basic substance, with an acidic liquid medium.
Abstract:
A phosphor is provided which is represented by the general formula MxCeySi6−zBzN8+w. M is at least one element selected from the group consisting of La, Y, Tb and Lu. And w, x, y, and z satisfy 2.0
Abstract:
Provided a method of producing a β-sialon fluorescent material having excellent emission intensity. The method includes providing a first composition containing aluminum, an oxygen atom, and a europium-containing silicon nitride, heat treating the first composition, contacting the heat-treated composition and a basic substance to obtain a second composition, and contacting the second composition resulting from contacting the heat-treated composition with the basic substance and an acidic liquid medium containing an acidic substance.
Abstract:
A wavelength converting member comprising a first wavelength converting layer containing: a first fluorescent material having a light emission peak wavelength in a range of 620 nm or more and 660 nm or less; a second fluorescent material having a light emission peak wavelength in a range of 510 nm or more and 560 nm or less; and a resin, wherein the average particle diameter, as measured according to a Fisher Sub-Sieve Sizer method, of the first fluorescent material is in a range of 2 μm or more and 30 μm or less, wherein the second fluorescent material comprises a β-SiAlON fluorescent material, the circularity of the β-SiAlON fluorescent material is 0.7 or more, and the volume average particle diameter, as measured according to a laser diffraction scattering particle size distribution measuring method, of the β-SiAlON fluorescent material is in a range of 2 μm or more and 30 μm or less, and wherein the thickness of the first wavelength converting layer is in a range of 50 μm or more and 200 μm or less.
Abstract:
A method for producing a β-sialon fluorescent material is provided. The method includes heat-treating a mixture containing an aluminium compound, a first europium compound, and silicon nitride to obtain a first heat-treated product; and heat-treating the first heat-treated product with a second europium compound in a rare gas atmosphere to obtain a second heat-treated product.
Abstract:
A method for producing a β-sialon fluorescent material superior in light emitting luminance is provided. The method includes heat-treating a first mixture containing an aluminum compound, a europium compound, and a first silicon oxynitride compound to obtain a first heat-treated product, and heat-treating a second mixture containing the first heat-treated product, an aluminum compound, a europium compound, and a second silicon oxynitride compound, which has a larger oxygen content than the first silicon oxynitride compound, to obtain a second heat-treated product.
Abstract:
A phosphor, which is represented by the general formula containing M, Ce, Pr, Si, and N, is provided. M is at least one element selected from the group consisting of La, Y, Tb and Lu. A molar ratio of M is greater than 2.0 and smaller than 3.5. A molar ratio of Ce is greater than 0 and smaller than 1.0. A molar ratio of Pr is greater than 0 and smaller than 0.05. A molar ratio of N is greater than 10 and smaller than 12, under the condition that a molar ratio of Si is set to 6. The phosphor further contains 10 to 10,000 ppm of fluorine.
Abstract:
A β-SiAlON fluorescent material includes fluorescent material particles having a composition represented by the following formula (I), and a coating layer formed on the surface of the fluorescent material particles and having a refractive index smaller than that of the fluorescent material particles, wherein when the β-SiAlON fluorescent material is measured by inductively coupled plasma-atomic emission spectroscopy, an amount of the coating layer is 0.4% by mass or more relative to a total amount of the fluorescent material particles and the coating layer being 100% by mass: Si6-zAlzOzN8-z:Euy (I), wherein y and z satisfy 0
Abstract:
A method for producing a β-sialon fluorescent material can be provided. The method includes preparing a composition containing silicon nitride that contains aluminium, an oxygen atom, and europium, heat-treating the composition in a rare gas atmosphere or in a vacuum, and contacting the heat-treated composition with a gas containing elemental fluorine.
Abstract:
A fluorescent material is provided that has improved luminance and can generate fluorescence by excitation light in wider wavelength range. A fluorescent material represented by a general formula LaxCeySi6N8+x+y, wherein 2.0≦x≦3.5, 0
Abstract translation:提供了具有改善的亮度的荧光材料,并且可以通过在较宽波长范围内的激发光产生荧光。 由通式LaxCeySi6N8 + x + y表示的荧光材料,其中2.0和nlE; x和nlE; 3.5,0