公开(公告)号:US20130207040A1
公开(公告)日:2013-08-15
申请号:US13759104
申请日:2013-02-05
Applicant: Rolex SA
Inventor: Detlef Berner , Hans U. Güdel , Isabelle Rigot , Romain Girod , Christoph Kenzelmann
IPC: C09K11/77
CPC classification number: C09K11/7792
Abstract: The present invention relates to long decay phosphors comprising rare earth activated strontium aluminates and methods for producing them. The phosphors comprise a matrix of the formula Sr4Al14O25 comprising europium as an activator and a further rare earth element as a co-activator, wherein the molar ratio of Al/Sr in the starting materials is in the range of 3.1 to less than 3.5 and the ratio of Eu/Sr is in the range of 0.0015 to 0.01. The process for the preparation of a phosphor comprises the steps of milling the starting materials for the synthesis of the phosphor, the starting materials comprising a boron compound selected from boric acid, boric oxide or a borate salt in an amount such that the B/Sr molar ratio is between 0.1 and to 0.3, treating the milled composition with heat, grinding the block material which is obtained through the heat treatment, ball-milling the crushed material, sieving the material, and washing the material with an aqueous solution.
Abstract translation: 本发明涉及包含稀土活化的锶铝酸盐的长衰减磷光体及其制备方法。 磷光体包含式Sr4Al14O25的基质,其包含作为活化剂的铕和作为助活化剂的另外的稀土元素,其中原料中Al / Sr的摩尔比在3.1至小于3.5的范围内, Eu / Sr的比例在0.0015〜0.01的范围内。 制备荧光体的方法包括以下步骤:研磨用于合成荧光体的原料,所述起始材料包含选自硼酸,氧化硼或硼酸盐的硼化合物,其量使得B / Sr 摩尔比在0.1和0.3之间,用热处理研磨的组合物,研磨通过热处理获得的块材料,球磨研磨破碎的材料,筛分材料,并用水溶液洗涤材料。
-
公开(公告)号:US20160137919A1
公开(公告)日:2016-05-19
申请号:US15004209
申请日:2016-01-22
Applicant: Rolex SA
Inventor: Detlef Berner , Romain Girod , Olliver Pujol , Isabelle Rigot
IPC: C09K11/77
CPC classification number: C09K11/7792 , C04B35/44 , C04B35/48 , C04B35/481 , C04B35/486 , C04B35/488 , C04B35/4885 , C04B35/6263 , C04B35/62635 , C04B35/62655 , C04B35/634 , C04B2235/3206 , C04B2235/3208 , C04B2235/3213 , C04B2235/3215 , C04B2235/3222 , C04B2235/3224 , C04B2235/3225 , C04B2235/3227 , C04B2235/3229 , C04B2235/3246 , C04B2235/3436 , C04B2235/3445 , C04B2235/3454 , C04B2235/3481 , C04B2235/40 , C04B2235/5436 , C04B2235/5463 , C04B2235/656 , C04B2235/6567 , C04B2235/6582 , C04B2235/6583 , C04B2235/661 , C04B2235/664 , C04B2235/76 , C04B2235/762 , C04B2235/765 , C04B2235/77 , C04B2235/80 , C04B2235/96 , C04B2235/9646 , C04B2235/9661 , C09K11/025 , G04B19/12 , G04B37/225 , Y10T428/24917 , Y10T428/24926
Abstract: The invention relates to a persistent phosphorescent ceramic composite material which is a sintered dense body comprising two or more phases, a first phase consisting of at least one metal oxide and a second phase consisting of a metal oxide containing at least one activating element in a reduced oxidation state. The invention furthermore relates to a method for the preparation of a phosphorescent ceramic composite material as defined in any of the previous claims, the method comprising the following steps: preparing a mixture of a metal oxide and a phosphor; fabricating a green body from the mixture; and heat treating the green body in a reducing atmosphere.
Abstract translation: 本发明涉及一种持续性磷光陶瓷复合材料,其是包含两相或多相的烧结致密体,第一相由至少一种金属氧化物组成,第二相由金属氧化物组成,所述第二相含有至少一种还原的活化元素 氧化态。 本发明还涉及一种制备前述权利要求中任一项所述的磷光陶瓷复合材料的方法,所述方法包括以下步骤:制备金属氧化物和磷光体的混合物; 从混合物制造一个绿色的身体; 并在还原气氛中对生坯进行热处理。
-
公开(公告)号:US09284485B2
公开(公告)日:2016-03-15
申请号:US14070616
申请日:2013-11-04
Applicant: Rolex SA
Inventor: Detlef Berner , Romain Girod , Ollivier Pujol , Isabelle Rigot
IPC: C09K11/08 , C09K11/02 , C04B35/486 , C04B35/626 , C09K11/77 , C04B35/44 , G04B19/12 , G04B37/22
CPC classification number: C09K11/7792 , C04B35/44 , C04B35/48 , C04B35/481 , C04B35/486 , C04B35/488 , C04B35/4885 , C04B35/6263 , C04B35/62635 , C04B35/62655 , C04B35/634 , C04B2235/3206 , C04B2235/3208 , C04B2235/3213 , C04B2235/3215 , C04B2235/3222 , C04B2235/3224 , C04B2235/3225 , C04B2235/3227 , C04B2235/3229 , C04B2235/3246 , C04B2235/3436 , C04B2235/3445 , C04B2235/3454 , C04B2235/3481 , C04B2235/40 , C04B2235/5436 , C04B2235/5463 , C04B2235/656 , C04B2235/6567 , C04B2235/6582 , C04B2235/6583 , C04B2235/661 , C04B2235/664 , C04B2235/76 , C04B2235/762 , C04B2235/765 , C04B2235/77 , C04B2235/80 , C04B2235/96 , C04B2235/9646 , C04B2235/9661 , C09K11/025 , G04B19/12 , G04B37/225 , Y10T428/24917 , Y10T428/24926
Abstract: The invention relates to a persistent phosphorescent ceramic composite material which is a sintered dense body comprising two or more phases, a first phase consisting of at least one metal oxide and a second phase consisting of a metal oxide containing at least one activating element in a reduced oxidation state. The invention furthermore relates to a method for the preparation of a phosphorescent ceramic composite material as defined in any of the previous claims, the method comprising the following steps: preparing a mixture of a metal oxide and a phosphor; fabricating a green body from the mixture; and heat treating the green body in a reducing atmosphere.
Abstract translation: 本发明涉及一种持续性磷光陶瓷复合材料,其是包含两相或多相的烧结致密体,第一相由至少一种金属氧化物组成,第二相由金属氧化物组成,所述第二相含有至少一种还原的活化元素 氧化态。 本发明还涉及一种制备前述权利要求中任一项所述的磷光陶瓷复合材料的方法,所述方法包括以下步骤:制备金属氧化物和磷光体的混合物; 从混合物制造一个绿色的身体; 并在还原气氛中对生坯进行热处理。
-
公开(公告)号:US10196566B2
公开(公告)日:2019-02-05
申请号:US15004209
申请日:2016-01-22
Applicant: Rolex SA
Inventor: Detlef Berner , Romain Girod , Olliver Pujol , Isabelle Rigot
IPC: C04B35/44 , C04B35/48 , C09K11/02 , C09K11/77 , G04B19/12 , G04B37/22 , C04B35/486 , C04B35/488 , C04B35/626 , C04B35/634
Abstract: The invention relates to a persistent phosphorescent ceramic composite material which is a sintered dense body comprising two or more phases, a first phase consisting of at least one metal oxide and a second phase consisting of a metal oxide containing at least one activating element in a reduced oxidation state. The invention furthermore relates to a method for the preparation of a phosphorescent ceramic composite material as defined in any of the previous claims, the method comprising the following steps: preparing a mixture of a metal oxide and a phosphor; fabricating a green body from the mixture; and heat treating the green body in a reducing atmosphere.
-
公开(公告)号:US09394480B2
公开(公告)日:2016-07-19
申请号:US13759104
申请日:2013-02-05
Applicant: Rolex SA
Inventor: Detlef Berner , Hans U. Güdel , Isabelle Rigot , Romain Girod , Christoph Kenzelmann
IPC: C09K11/77
CPC classification number: C09K11/7792
Abstract: The present invention relates to long decay phosphors comprising rare earth activated strontium aluminates and methods for producing them. The phosphors comprise a matrix of the formula Sr4Al14O25 comprising europium as an activator and a further rare earth element as a co-activator, wherein the molar ratio of Al/Sr in the starting materials is in the range of 3.1 to less than 3.5 and the ratio of Eu/Sr is in the range of 0.0015 to 0.01. The process for the preparation of a phosphor comprises the steps of milling the starting materials for the synthesis of the phosphor, the starting materials comprising a boron compound selected from boric acid, boric oxide or a borate salt in an amount such that the B/Sr molar ratio is between 0.1 and to 0.3, treating the milled composition with heat, grinding the block material which is obtained through the heat treatment, ball-milling the crushed material, sieving the material, and washing the material with an aqueous solution.
Abstract translation: 本发明涉及包含稀土活化的锶铝酸盐的长衰减磷光体及其制备方法。 磷光体包含式Sr4Al14O25的基质,其包含作为活化剂的铕和作为助活化剂的另外的稀土元素,其中原料中Al / Sr的摩尔比在3.1至小于3.5的范围内, Eu / Sr的比例在0.0015〜0.01的范围内。 制备荧光体的方法包括以下步骤:研磨用于合成荧光体的原料,所述起始材料包含选自硼酸,氧化硼或硼酸盐的硼化合物,其量使得B / Sr 摩尔比在0.1和0.3之间,用热处理研磨的组合物,研磨通过热处理获得的块材料,球磨研磨破碎的材料,筛分材料,并用水溶液洗涤材料。
-
公开(公告)号:US20140124702A1
公开(公告)日:2014-05-08
申请号:US14070616
申请日:2013-11-04
Applicant: Rolex SA
Inventor: Detlef Berner , Romain Girod , Ollivier Pujol , Isabelle Rigot
IPC: C09K11/02
CPC classification number: C09K11/7792 , C04B35/44 , C04B35/48 , C04B35/481 , C04B35/486 , C04B35/488 , C04B35/4885 , C04B35/6263 , C04B35/62635 , C04B35/62655 , C04B35/634 , C04B2235/3206 , C04B2235/3208 , C04B2235/3213 , C04B2235/3215 , C04B2235/3222 , C04B2235/3224 , C04B2235/3225 , C04B2235/3227 , C04B2235/3229 , C04B2235/3246 , C04B2235/3436 , C04B2235/3445 , C04B2235/3454 , C04B2235/3481 , C04B2235/40 , C04B2235/5436 , C04B2235/5463 , C04B2235/656 , C04B2235/6567 , C04B2235/6582 , C04B2235/6583 , C04B2235/661 , C04B2235/664 , C04B2235/76 , C04B2235/762 , C04B2235/765 , C04B2235/77 , C04B2235/80 , C04B2235/96 , C04B2235/9646 , C04B2235/9661 , C09K11/025 , G04B19/12 , G04B37/225 , Y10T428/24917 , Y10T428/24926
Abstract: The invention relates to a persistent phosphorescent ceramic composite material which is a sintered dense body comprising two or more phases, a first phase consisting of at least one metal oxide and a second phase consisting of a metal oxide containing at least one activating element in a reduced oxidation state. The invention furthermore relates to a method for the preparation of a phosphorescent ceramic composite material as defined in any of the previous claims, the method comprising the following steps: preparing a mixture of a metal oxide and a phosphor; fabricating a green body from the mixture; and heat treating the green body in a reducing atmosphere.
Abstract translation: 本发明涉及一种持续性磷光陶瓷复合材料,其是包含两相或多相的烧结致密体,第一相由至少一种金属氧化物组成,第二相由金属氧化物组成,所述第二相含有至少一种还原的活化元素 氧化态。 本发明还涉及一种制备前述权利要求中任一项所述的磷光陶瓷复合材料的方法,所述方法包括以下步骤:制备金属氧化物和磷光体的混合物; 从混合物制造一个绿色的身体; 并在还原气氛中对生坯进行热处理。
-
-
-
-
-