摘要:
A thin polarizing plate is disclosed that includes a polarizer, a protective layer formed on at least one side of the polarizer, and a pressure sensitive adhesive layer formed on the protective layer, wherein the thickness A of the polarizer, the thickness B of the protective layer, the modulus of elasticity C of a pressure sensitive adhesive of the pressure sensitive adhesive layer, a numerical value 1 and a numerical value 2 satisfy the following relationships: (numerical value 1)=B/A
摘要翻译:公开了一种薄偏振片,其包括偏振器,形成在偏振器的至少一侧上的保护层和形成在保护层上的压敏粘合剂层,其中偏振器的厚度A,保护层的厚度B 层数,压敏粘合剂层的压敏粘合剂的弹性模量C,数值1和数值2满足以下关系:(数值1)= B / A <2.0(数值2)= (数值1)/℃<20,通过提供薄且轻的偏振片。 还公开了使用所述偏振片的薄且轻的液晶显示器。
摘要:
A polarizing plate having excellent moisture durability and a liquid crystal display using the same are disclosed. The polarizing plate is produced by covering all surfaces and sides of a polarizer with low moisture-permeable layers having moisture permeability of 310 g/m2·24 h or less. The rate of change in dimension of the polarizer in the uniaxially stretched direction is ±0.1% or less after left at a temperature of 60° C. and humidity of 95% for 100 hours.
摘要翻译:公开了一种具有优异的耐湿性的偏光板和使用其的液晶显示器。 偏光板通过覆盖具有310g / m 2以下的透湿性低的透湿层的偏振片的所有表面和侧面.24小时以下。 偏振器在单轴向拉伸方向上的尺寸变化率在离开温度60℃,湿度95%100小时后为±0.1%以下。
摘要:
A polarizing plate having excellent moisture durability and a liquid crystal display using the same are disclosed. The polarizing plate is produced by covering all surfaces and sides of a polarizer with low moisture-permeable layers having moisture permeability of 310 g/m2·24 h or less. The rate of change in dimension of the polarizer in the uniaxially stretched direction is ±0.1% or less after left at a temperature of 60° C. and humidity of 95% for 100 hours.
摘要翻译:公开了一种具有优异的耐湿性的偏光板和使用其的液晶显示器。 偏光板通过覆盖具有310g / m 2·24小时以下的透湿性低透湿层的偏振片的所有表面和侧面来制造。 偏振器在单轴向拉伸方向上的尺寸变化率在离开温度60℃,湿度95%100小时后为±0.1%以下。
摘要:
A polarizing plate having excellent moisture durability and a liquid crystal display using the same are disclosed. The polarizing plate is produced by covering all surfaces and sides of a polarizer with low moisture-permeable layers having moisture permeability of 310 g/m2·24 h or less. The rate of change in dimension of the polarizer in the uniaxially stretched direction is ±0.1% or less after left at a temperature of 60° C. and humidity of 95% for 100 hours.
摘要翻译:公开了一种具有优异的耐湿性的偏光板和使用其的液晶显示器。 偏光板通过覆盖具有310g / m 2·24小时以下的透湿性低透湿层的偏振片的所有表面和侧面来制造。 偏振器在单轴向拉伸方向上的尺寸变化率在离开温度60℃,湿度95%100小时后为±0.1%以下。
摘要:
The present invention provides a polarizer and a polarizing plate having less dimensional changes to heat stress. The present invention provides also a liquid crystal display that includes the polarizer and the polarizing plate, and is free of color irregularity or decoloration. The polarizer has shrinkage force of not more than 4.0 N/cm in the absorption axis direction after being heated at 80° C. for 30 minutes. A protective film is laminated on at least one surface of the polarizer in order to form a polarizing plate, and the polarizing plate has a following relationship of 0.01≦A/B≦0.16 when A denotes a thickness of the polarizer and B denotes a thickness of the protective film.
摘要翻译:本发明提供一种偏振片和偏振片,其具有较小的热应力尺寸变化。 本发明还提供一种液晶显示器,其包括偏振片和偏振片,并且没有颜色不规则或脱色。 在80℃下加热30分钟后,偏振片的吸收轴方向的收缩力为4.0N / cm以下。 在偏振片的至少一个表面上层叠保护膜以形成偏振片,并且当A表示偏振片的厚度时,偏振片的关系为0.01 <= A / B <= 0.16,B表示 保护膜的厚度。
摘要:
A polarizing plate produced according to the present invention includes a polarizing film and a protective layer bonded to a surface of the polarizing film, where the protective layer has no irregularities like record grooves caused by stretching of the polarizing film, so that the polarizing plate with an improved appearance provides clear images even when reflected light is applied. Such a polarizing plate is produced by laminating a protective layer on at least one surface of a polarizer while limiting moisture content of the polarizer to a range from 5% to 30%. A value for the moisture content is obtained by a calculation based on an equation of moisture content (%)=[(A−B)/B]×100, when A denotes weight of the polarizer before bonding and B denotes weight of the polarizer after being kept in a dryer of 120° C. for seven hours.
摘要:
A polarizing plate produced according to the present invention includes a polarizing film and a protective layer bonded to a surface of the polarizing film, where the protective layer has no irregularities like record grooves caused by stretching of the polarizing film, so that the polarizing plate with an improved appearance provides clear images even when reflected light is applied. Such a polarizing plate is produced by laminating a protective layer on at least one surface of a polarizer while limiting moisture content of the polarizer to a range from 5% to 30%. A value for the moisture content is obtained by a calculation based on an equation of moisture content (%)=[(A−B)/B]×100, when A denotes weight of the polarizer before bonding and B denotes weight of the polarizer after being kept in a dryer of 120° C. for seven hours.
摘要:
A polarizing plate produced according to the present invention includes a polarizing film and a protective layer bonded to a surface of the polarizing film, where the protective layer has no irregularities like record grooves caused by stretching of the polarizing film, so that the polarizing plate with an improved appearance provides clear images even when reflected light is applied. Such a polarizing plate is produced by laminating a protective layer on at least one surface of a polarizer while limiting moisture content of the polarizer to a range from 5% to 30%. A value for the moisture content is obtained by a calculation based on an equation of moisture content (%)=[(A−B)/B]×100, when A denotes weight of the polarizer before bonding and B denotes weight of the polarizer after being kept in a dryer of 120° C. for seven hours.
摘要:
A polarizing plate excellent in polarization performance in all wavebands from a short wavelength region to a long wavelength region and a liquid crystal display using such a polarizing plate. The polarizing plate including a polarizer has a portion having a polarization degree of 99% or more at each wavelength of light for wavelengths of 420 to 550 nm and a portion having a polarization degree of 99% or more at each wavelength of light for wavelengths of 550 to 700 nm.
摘要:
A polarizer having good durability that is dyed by iodine, and is given boric acid processing, and moreover contains zinc without generating fault by deposit of boric acid or zinc, may be produced by a process of producing, comprising the steps of: conducting a dyeing processing by iodine to a non-stretched poly vinylalcohol film; conducting an uniaxial stretching processing and a boric acid processing; subsequently conducting a zinc impregnation processing; and furthermore, conducting an iodine ion impregnation processing.