摘要:
A dielectric ceramic composition comprising a main component of BaTiO3, a first subcomponent including at least one compound selected from MgO, CaO, BaO, SrO and Cr2O3, a second subcomponent of (Ba, Ca)xSiO2+x (where, x=0.8 to 1.2), a third subcomponent including at least one compound selected from V2O5, MoO3, and WO3, and a fourth subcomponent including an oxide of R1 (where R1 is at least one element selected from Sc, Er, Tm, Yb, and Lu), a fifth subcomponent including an oxide of R2 (where R2 is at least one element selected from Y, Dy, Ho, Tb, Gb and Eu), wherein the ratios of the subcomponents to 100 moles of the main component of BaTiO3 are first subcomponent of 0.1 to 3 moles, second subcomponent of 2 to 10 moles, third subcomponent of 0.01 to 0.5 mole, fourth subcomponent of 0.5 to 7 moles, and fifth subcomponent of 2 to 9 moles (where the number of moles of the fourth and fifth subcomponents are respectively the ratio of R1 and R2 alone).
摘要:
Provided are dielectric ceramics and an electronic component capable of enhancing the longevity of insulation resistance under load at high temperature, namely, the so-called lifetime of IR degradation. A dielectric layer comprises dielectric ceramics containing BaTiO3 that is a main component; a first auxiliary component containing at least one element in a group consisting of Mg, Ca, Ba, Sr and Cr; a second auxiliary component containing SiO2; a third auxiliary component containing at least one element in a group consisting of V, Mo and W; and a fourth auxiliary component containing at least one element in a group consisting of Er, Tm, Yb, Y, Dy and Ho. Preferably, the rate of existence of crystal particles having voids in the dielectric ceramics is 10% or lower in terms of the count rate, and an average crystal particle diameter is more than 0.1 &mgr;m and not more than 0.7 &mgr;m. Thus, the lifetime of IR degradation is improved. Preferably, BaTiO3 powders synthesized by oxalate process or solid phase method and having a Ba/Ti ratio of more than 1 and less than 1.007 are used as a raw material.
摘要:
A method of manufacturing a dielectric ceramic composition comprising at least BaTiO3 as a main component, a second subcomponent having SiO2 as a main component and at least one type selected from MO (note that M is at least one type of element selected from Ba, Ca, Sr and Mg), Li2O and B2O3 and other subcomponents, comprising the steps of mixing in the main component at least part of other subcomponents except for the second subcomponent to prepare a pre-calcination powder, calcining said pre-calcination powder to prepare a calcined powder, and mixing at least said second subcomponent in said calcined powder to obtain a dielectric ceramic composition having ratios of the subcomponents to BaTiO3 as the main component of predetermined molar ratios.
摘要:
A dielectric ceramic composition including a dielectric base phase containing BaTiO3 as a main component, and plate-shaped or acicula deposition phase existing together in the dielectric base phase. Preferably, the dielectric ceramic composition includes a main component of BaTiO3, a first subcomponent including at least one compound selected from MgO, CaG, BaG, SrO and Cr2O3, a second subcomponent of (Ba, Ca)xSiO2+x (where, x=0.8 to 1.2), a third subcomponent including at least one compound selected from V2O5, MoO3, and WO3, and a fourth subcomponent including an oxide of R1 (where R1 is at least one element selected from Sc, Er, Tm, Yb, and Lu), a fifth subcomponent including an oxide of R2 (where R2 is at least one element selected from Y, Dy, Ho, Tb, Gb and Eu), wherein the ratios of the subcomponents to 100 moles of the main component of BaTiO3 are first subcomponent of 0.1 to 3 moles, second subcomponent of 2 to 10 moles, third subcomponent of 0.01 to 0.5 mole, fourth subcomponent of 0.5 to 7 moles, and fifth subcomponent of 2 to 9 moles (where the number of moles of the fourth and fifth subcomponents are respectively the ratio of R1 and R2 alone).
摘要:
A dielectric ceramic composition comprising a main component of composed mainly of barium titanate, a first subcomponent including at least one compound selected from MgO, CaO, BaO, SrO and Cr2O3, a second subcomponent containing silicone oxide as a main composition, a third subcomponent including at least one compound selected from V2O5, MoO3, and WO3, a fourth subcomponent including an oxide of R1 (where R1 is at least one element selected from Sc, Er, Tm, Yb, and Lu), and a fifth subcomponent including CaZrO3 or CaO+ZrO2, wherein the ratios of the subcomponents to 100 moles of the main component of composed mainly of barium titanate are the first subcomponent of 0.1 to 3 moles, the second subcomponent of 2 to 10 moles, the third subcomponent of 0.01 to 0.5 moles, the fourth subcomponent of 0.5 to 7 moles (where the number of moles of the fourth subcomponent is the ratio of R1 alone), and the fifth subcomponent of 0
摘要翻译:一种包含主要由钛酸钡组成的主要成分的电介质陶瓷组合物,包含至少一种选自MgO,CaO,BaO,SrO和Cr 2 O 3的化合物的第一副成分,含有氧化硅作为主要成分的第二副成分,第三副成分, 至少一种选自V 2 O 5,MoO 3和WO 3的化合物,包含R 1的氧化物(其中R 1为选自Sc,Er,Tm,Yb和Lu中的至少一种元素)的第四副成分,以及包含CaZrO 3的第五副成分或 CaO + ZrO 2,其中副成分与100摩尔主要由钛酸钡组成的主成分的比例为0.1〜3摩尔的第1副成分,2〜10摩尔的第2副成分,第2副成分为0.01〜0.5摩尔 ,第四副成分为0.5〜7摩尔(其中第四副成分的摩尔数为单独的R1的比例),第五副成分为0 <第五副成分<= 5摩尔。 根据介电陶瓷组合物,介电常数高,电容温度特性可以达到EIA标准的X8R特性(-55〜150℃,DELTAC =±15%),在 减少的气氛是可能的。
摘要:
A main object of the present invention is to provide an anode active material capable of increasing energy density at the same time increasing battery safety, and a metal ion battery prepared with the anode active material. The present invention is an anode active material including an element that belongs to alunite group capable to insert and remove an ion(s) of at least one metal element selected from the group consisting of alkali metal elements and alkaline-earth metal elements, and a metal ion battery having a cathode, an anode, and an electrolyte filled between the cathode and the anode, the electrolyte conducting a metal ion(s), wherein the anode active material is contained in the anode.
摘要:
The main object of the present invention is to provide a cathode active material capable of reducing the initial interface resistance against a solid electrolyte material. The present invention solves the above-mentioned problems by providing a cathode active material comprising a cathode active substance exhibiting strong basicity and a coat layer formed so as to cover the surface of the above-mentioned cathode active substance and provided with a polyanionic structural part exhibiting acidity.
摘要:
A main object of the present invention is to provide an anode active material capable of increasing energy density at the same time increasing battery safety, and a metal ion battery prepared with the anode active material. The present invention is an anode active material including an element that belongs to alunite group capable to insert and remove an ion(s) of at least one metal element selected from the group consisting of alkali metal elements and alkaline-earth metal elements, and a metal ion battery having a cathode, an anode, and an electrolyte filled between the cathode and the anode, the electrolyte conducting a metal ion(s), wherein the anode active material is contained in the anode.
摘要:
An object of the present invention is to provide a high-capacity, low cycle deterioration lithium secondary battery in which the positive electrode is provided with a titanium composite oxide such as Li2NiTiO4. A lithium secondary battery 100 provided by the present invention includes a positive electrode 10 and a negative electrode 20. The positive electrode 10 has a solid solution between Li2M1TiO4 (where M1 is at least one metal element selected from the group consisting of Mn, Fe, Co, and Ni) and LiM2O2 (where M2 is at least one metal element selected from the group consisting of Mn, Co, and Ni).
摘要翻译:本发明的目的是提供一种高容量,低循环劣化的锂二次电池,其中正极设置有诸如Li 2 NiTiO 4的钛复合氧化物。 本发明提供的锂二次电池100包括正极10和负极20.正极10具有Li 2 M 1 TiO 4之间的固溶体(其中,M1为选自Mn,Fe, Co和Ni)和LiM 2 O 2(其中M2是选自Mn,Co和Ni中的至少一种金属元素)。
摘要:
An electronic device having an element body comprising an internal electrode layer, wherein the internal electrode layer includes an alloy, the alloy contains a nickel (Ni) element and at least one kind of element selected from ruthenium (Ru), rhodium (Rh), rhenium (Re) and platinum (Pt), and a content of each component is Ni: 80 to 100 mol % (note that 100 mol % is excluded) and a total of Ru, Rh, Re and Pt: 0 to 20 mol % (note that 0 mol % is excluded).