公开(公告)号:US20180195907A1
公开(公告)日:2018-07-12
申请号:US15865297
申请日:2018-01-09
Inventor: Chao WANG , Jun HU , Fei WANG , Zezhan ZHANG , Jing JIANG , Jie XIONG , Yueming WANG , Tiezhong MA , Dong YAN , Xueke GOU , Ting ZHOU , Yi NIU , Pei HUANG
Abstract: A device for measuring surface-temperature of a turbine blade, the device including a probe having a front-end mirror for receiving infrared radiation of a surface on the blade, a collimation lens for refracted the infrared radiation, a PD detector to receive the infrared radiation, and a focal-length servo; and a radial-scanning servo connected to the probe. The front-end mirror, the collimation lens, and PD detector are disposed along the optical axis of the collimation lens. The focal-length servo is adapted to move the collimation lens along the optical axis of the collimation lens. The radial-scanning servo is adapted to move the probe along the optical axis of the collimation lens. The device of the invention is capable of accurately targeting a particular point on the blade having an irregular shape for temperature measurement to accurately detect the temperature distribution on the surface of the blade.
-
公开(公告)号:US20180185923A1
公开(公告)日:2018-07-05
申请号:US15862606
申请日:2018-01-04
Inventor: Chao WANG , Yi NIU , Jing JIANG , Yide CHEN , Junfeng XIA , Rui ZHANG , Ting ZHOU , Hanqing TIAN
CPC classification number: B22F9/04 , B22F1/0085 , B22F3/105 , B22F3/14 , B22F2003/145 , B22F2203/11 , B22F2301/35 , B22F2998/10 , C01G49/12 , C01P2002/72 , C01P2006/40 , H01L35/16
Abstract: A method of preparing a thermoelectric material comprising an iron-sulfur compound, the method including: 1) weighing, grinding, and mixing an iron salt and a sulfur-containing source to obtain a mixed powder; 2) carrying out a hydrothermal reaction with the mixed powder to obtain a black precipitate; 3) washing the precipitate; 4) drying the precipitate under vacuum to obtain FeS2 powder; 5) annealing the FeS2 powder under inert atmosphere to obtain annealed powder, where a heating temperature is from 300° C. to 1000° C., a heating time is from 2 hours to 24 hours, and a flow rate of an inert gas is from 30 mL/min to 200 mL/min; and 6) sintering the annealed powder to obtain a thermoelectric material including an iron-sulfur compound.
-