摘要:
A thermoplastic cellulose derivative composition of the present invention contains, as a main component, a cellulose ester having an aliphatic polyester side chain having a repeat unit having 2 to 5 carbon atoms, wherein a rate of heating loss at 200° C. is 5 wt % or less, a melt viscosity at 200° C. and 1000 sec−1 is 50 to 300 Pa·sec, and a melt tension at the time of take-up at 200° C. and 100 m/min is 0.1 to 40 mN. The present invention can provide excellent fiber products by melt spinning of the composition.
摘要翻译:本发明的热塑性纤维素衍生物组合物含有具有碳原子数2〜5的重复单元的脂肪族聚酯侧链的纤维素酯作为主要成分,其中200℃下的加热损失率为5重量% %以下,200℃,1000秒-1下的熔融粘度为50〜300Pa·s,在200℃和100℃下卷取时的熔融张力 m / min为0.1〜40mN。 本发明可以通过组合物的熔融纺丝提供优异的纤维产品。
摘要:
This invention provides fibers made from a thermoplastic cellulose ester composition, which can maintain excellent mechanical properties still after high temperature dyeing treatment, especially suitable as fibers mixed with polyester fibers or as fabrics woven or knitted together with polyester fibers, and also provides the thermoplastic cellulose ester composition constituting the fibers. For example, this invention provides a thermoplastic cellulose ester composition containing at least 70 to 95 wt % of a cellulose fatty acid mixed ester with an average substitution degree of 2.4 to 2.8, 5 to 25 wt % of a plasticizer and 1 to 10 wt % of a cellulose acetate with an average substitution degree of 2.3 to 2.6, and also provides fibers made from the thermoplastic cellulose ester composition.
摘要:
This invention provides fibers made from a thermoplastic cellulose ester composition, which can maintain excellent mechanical properties still after high temperature dyeing treatment, especially suitable as fibers mixed with polyester fibers or as fabrics woven or knitted together with polyester fibers, and also provides the thermoplastic cellulose ester composition constituting the fibers. For example, this invention provides a thermoplastic cellulose ester composition containing at least 70 to 95 wt % of a cellulose fatty acid mixed ester with an average substitution degree of 2.4 to 2.8, 5 to 25 wt % of a plasticizer and 1 to 10 wt % of a cellulose acetate with an average substitution degree of 2.3 to 2.6, and also provides fibers made from the thermoplastic cellulose ester composition.
摘要:
A fabric consisting of a cellulose mixed ester fiber having an appropriate strength, fiber diameter, uniformity of fineness, and Tg, is used. A fiber consisting of 80 to 95 wt % of said cellulose mixed ester and 5 to 20 wt % of one or more water-soluble plasticizers selected from the group of polyethylene glycol, polypropylene glycol, poly(ethylene-propylene) glycol, and end-capped polymers produced from them, is produced and said water-soluble plasticizers are removed by aqueous treatment to improve the heat resistance and strength, thereby providing a fabric having beautiful appearance achieved by color development properties and uniform fineness.
摘要:
A manufacturing method for an esterification product of a cellulose derivative by comprising esterification of a cellulose derivative in a mixture of an ionic liquid, cellulose derivative and agent that is at least one selected from the group consisting of carboxylic anhydride, carboxylic acid halide, and carboxylic acid.
摘要:
A fabric consisting of a cellulose mixed ester fiber having an appropriate strength, fiber diameter, uniformity of fineness, and Tg, is used. A fiber consisting of 80 to 95 wt % of said cellulose mixed ester and 5 to 20 wt % of one or more water-soluble plasticizers selected from the group of polyethylene glycol, polypropylene glycol, poly(ethylene-propylene) glycol, and end-capped polymers produced from them, is produced and said water-soluble plasticizers are removed by aqueous treatment to improve the heat resistance and strength, thereby providing a fabric having beautiful appearance achieved by color development properties and uniform fineness.