11.
公开(公告)号:US20140209169A1
公开(公告)日:2014-07-31
申请号:US14228353
申请日:2014-03-28
Applicant: ASAHI GLASS COMPANY, LIMITED
Inventor: Yu HANAWA , Yutaka KUROIWA , Tetsuya NAKASHIMA , Yuki KONDO
IPC: C03C3/093 , H01L31/048 , C03C3/087
CPC classification number: H01L31/0488 , C03C3/087 , C03C3/093 , H01L31/03925 , H01L31/03928 , Y02E10/541 , Y02P70/521
Abstract: A glass substrate for a CdTe solar cell includes a base composition includes, in terms of mol % on a basis of following oxides: from 60 to 75% of SiO2; from 1 to 7.5% of Al2O3; from 0 to 1% of B2O3; from 8.5 to 12.5% of MgO; from 1 to 6.5% of CaO; from 0 to 3% of SrO; from 0 to 3% of BaO; from 0 to 3% of ZrO2; from 1 to 8% of Na2O; and from 2 to 12% of K2O, wherein MgO+CaO+SrO+BaO is from 10 to 24%, Na2O+K2O is from 5 to 15%, MgO/Al2O3 is 1.3 or more, (2Na2O+K2O+SrO+BaO)/(Al2O3+ZrO2) is 3.3 or less, Na2O/K2O is from 0.2 to 2.0, Al2O3≧−0.94MgO+11, and CaO≧0.48MgO+6.5.
Abstract translation: 用于CdTe太阳能电池的玻璃基板包括基于以下氧化物的摩尔%的基础组成:60至75%的SiO 2; 1〜7.5%的Al2O3; 0〜1%的B2O3; 8.5〜12.5%的MgO; 1〜6.5%的CaO; 0〜3%的SrO; 0〜3%的BaO; 0〜3%的ZrO2; 1〜8%的Na2O; 和2〜12%的K2O,其中MgO + CaO + SrO + BaO为10〜24%,Na2O + K2O为5〜15%,MgO / Al2O3为1.3以上,(2Na2O + K2O + SrO + BaO )/(Al 2 O 3 + ZrO 2)为3.3以下,Na 2 O / K 2 O为0.2〜2.0,Al 2 O 3≥0.94MgO+ 11,CaO≥0.48MgO+ 6.5。