COLORED ALKALI ALUMINOSILICATE GLASS ARTICLES

    公开(公告)号:US20190071345A1

    公开(公告)日:2019-03-07

    申请号:US16180563

    申请日:2018-11-05

    Abstract: A glass article including at least about 40 mol % SiO2 and, optionally, a colorant imparting a preselected color is disclosed. In general, the glass includes, in mol %, from about 40-70 SiO2, 0-25 Al2O3, 0-10 B2O3; 5-35 Na2O, 0-2.5 K2O, 0-8.5 MgO, 0-2 ZnO, 0-10% P2O5 and 0-1.5 CaO. As a result of ion exchange, the glass includes a compressive stress (σs) at at least one surface and, optionally, a color. In one method, communicating a colored glass with an ion exchange bath imparts σs while in another; communicating imparts σs and a preselected color. In the former, a colorant is part of the glass batch while in the latter; it is part of the bath. In each, the colorant includes one or more metal containing dopants formulated to impart to a preselected color. Examples of one or more metal containing dopants include one or more transition and/or rare earth metals.

    Chemically-strengthened borosilicate glass articles
    15.
    发明授权
    Chemically-strengthened borosilicate glass articles 有权
    化学强化硼硅玻璃制品

    公开(公告)号:US09145333B1

    公开(公告)日:2015-09-29

    申请号:US13905409

    申请日:2013-05-30

    CPC classification number: C03C21/002 C03C3/091

    Abstract: Methods are disclosed for producing chemically-strengthened, borosilicate, glass articles. The articles are produced from batch components which are selected, at least in part, based on measured and/or estimated values for the coordination state of B2O3 in the glass. In this way, such chemical-strengthening properties as mutual diffusivity, maximum surface compressive stress, and/or indentation threshold can be improved.

    Abstract translation: 公开了用于生产化学强化的硼硅酸盐玻璃制品的方法。 这些制品是由批量成分制成的,至少部分基于玻璃中B2O3的配位状态的测量值和/或估计值。 以这种方式,可以提高相互扩散性,最大表面压缩应力和/或压痕阈值等化学强化性能。

    Colored alkali aluminosilicate glass articles

    公开(公告)号:US11912620B2

    公开(公告)日:2024-02-27

    申请号:US17971721

    申请日:2022-10-24

    CPC classification number: C03C4/02 C03C3/087 C03C3/11 C03C21/002 Y10T428/315

    Abstract: A glass article including at least about 40 mol % SiO2 and, optionally, a colorant imparting a preselected color is disclosed. In general, the glass includes, in mol %, from about 40-70 SiO2, 0-25 Al2O3, 0-10 B2O3; 5-35 Na2O, 0-2.5 K2O, 0-8.5 MgO, 0-2 ZnO, 0-10% P2O5 and 0-1.5 CaO. As a result of ion exchange, the glass includes a compressive stress (σs) at at least one surface and, optionally, a color. In one method, communicating a colored glass with an ion exchange bath imparts σs while in another; communicating imparts σs and a preselected color. In the former, a colorant is part of the glass batch while in the latter; it is part of the bath. In each, the colorant includes one or more metal containing dopants formulated to impart to a preselected color. Examples of one or more metal containing dopants include one or more transition and/or rare earth metals.