Anti-glare optical multilayer body
    11.
    发明授权
    Anti-glare optical multilayer body 有权
    防眩光光学多层体

    公开(公告)号:US07661832B2

    公开(公告)日:2010-02-16

    申请号:US11884378

    申请日:2006-02-21

    IPC分类号: G02B27/00

    CPC分类号: G02B5/02 G02F1/133502

    摘要: An optical laminate having a light transparent base material and an anti-dazzling layer provided on the light transparent base material, wherein the outermost surface of the anti-dazzling layer has a concavoconvex surface. The concavoconvex shape simultaneously satisfies the following formulae (I) 1.2≦θa≦2.5 and (II) 0.004≦ψ≦0.18, wherein θa represents the average inclination angle of the concavoconvex part; Rz represents the average roughness of concavoconvexes; Sm represents the average spacing of the concavoconvexes; and ψ represents the ratio, between Rz and Sm, defined by ψ=Rz/Sm. The optical laminate has an internal haze value of not less than 0% and not more than 50%, and the optical laminate has a surface haze value of not less than 0.5% and not more than 4.5%.

    摘要翻译: 一种具有透光基材和防透光层的光学层叠体,其设置在透光基材上,其中防炫目层的最外表面具有凹凸表面。 凹凸形状同时满足以下公式(I)1.2 <=θa<= 2.5和(II)0.004 <= psi <= 0.18,其中θa表示凹凸部分的平均倾斜角; Rz表示凹凸的平均粗糙度; Sm表示凹凸的平均间距; psi表示由psi = Rz / Sm定义的Rz和Sm之间的比率。 光学层叠体的内部雾度值为0%以上且50%以下,光学层叠体的表面雾度值为0.5%以上且4.5%以下。

    Method and Apparatus For Producing Optical Multilayer Body
    12.
    发明申请
    Method and Apparatus For Producing Optical Multilayer Body 有权
    用于制造光学多层体的方法和装置

    公开(公告)号:US20080218865A1

    公开(公告)日:2008-09-11

    申请号:US11884394

    申请日:2006-02-21

    摘要: An optical laminate produced by a process for producing an anti-dazzling laminate comprising a light transparent base material and an anti-dazzling layer provided on the light transparent base material. The process includes providing the light transparent base material and forming the anti-dazzling layer having a concavoconvex shape on the light transparent base material, wherein the concavoconvex shape of the anti-dazzling layer satisfies the following requirements: Sm is not less than 100 μm and not more than 600 μm, θa is not less than 0.1 degree and not more than 1.2 degrees, and Rz is more than 0.2 μm and not more than 1 μm, wherein Sm represents the average spacing of concavoconvexes or profile irregularities in the anti-dazzling layer; θa represents the average inclination angle of the concavoconvexes or profile irregularities; and Rz represents the average roughness of the concavoconvexes or profile irregularities.

    摘要翻译: 一种通过用于制造抗光泽层压体的方法制造的光学层压材料,其包含透光基材和设置在透光基材上的防炫目层。 该方法包括提供光透明基材并在透光基材上形成具有凹凸形状的防眩光层,其中抗眩光层的凹凸形状满足以下要求:Sm不小于100μm, 不超过600μm,θa不小于0.1度且不大于1.2度,Rz大于0.2mum且不大于1um,其中Sm表示抗晕眼中凹凸或平均间隙的平均间距 层; thetaa表示凹凸或轮廓不规则的平均倾斜角; 并且Rz表示凹凸或轮廓不规则的平均粗糙度。

    Method and apparatus for producing optical multilayer body
    13.
    发明授权
    Method and apparatus for producing optical multilayer body 有权
    光学多层体制造方法及装置

    公开(公告)号:US08304071B2

    公开(公告)日:2012-11-06

    申请号:US12695262

    申请日:2010-01-28

    IPC分类号: B32B3/30

    摘要: An optical laminate produced by a process for producing an anti-dazzling laminate comprising a light transparent base material and an anti-dazzling layer provided on the light transparent base material. The process includes providing the light transparent base material and forming the anti-dazzling layer having a concavoconvex shape on the light transparent base material, wherein the concavoconvex shape of the anti-dazzling layer satisfies the following requirements: Sm is not less than 100 μm and not more than 600 μm, θa is not less than 0.1 degree and not more than 1.2 degrees, and Rz is more than 0.2 μm and not more than 1 μm, wherein Sm represents the average spacing of concavoconvexes or profile irregularities in the anti-dazzling layer; θa represents the average inclination angle of the concavoconvexes or profile irregularities; and Rz represents the average roughness of the concavoconvexes or profile irregularities.

    摘要翻译: 一种通过用于制造抗光泽层压体的方法制造的光学层压材料,其包含透光基材和设置在透光基材上的防炫目层。 该方法包括提供透光基材,并在透光基材上形成具有凹凸形状的防眩光层,其中抗晕眼层的凹凸形状满足以下要求:Sm不小于100μm, 不超过600μm,a不小于0.1度且不大于1.2度,Rz大于0.2μm且不大于1μm,其中Sm表示抗反射层中凹凸或凹凸的平均间距 炫耀层; &thetas; a表示凹凸或轮廓不规则的平均倾角; 并且Rz表示凹凸或轮廓不规则的平均粗糙度。

    Optical multilayer body, polarization plate using same, and image display

    公开(公告)号:US08187699B2

    公开(公告)日:2012-05-29

    申请号:US11884319

    申请日:2006-02-21

    IPC分类号: G02B5/02 G02B1/11 G02B5/30

    摘要: An optical laminate is provided which has anti-dazzling properties and can realize excellent glare preventive properties and black reproducibility (gradation rendering of black at low brightness). The optical laminate includes a light transparent base material and an anti-dazzling layer or a light diffusion layer provided on the light transparent base material, wherein the outermost surface of the anti-dazzling layer or light diffusion layer has a concavoconvex surface. The anti-dazzling layer satisfies the requirements that Sm is not less than 100 μm and not more than 600 μm, θa is not less than 0.1 degree and not more than 1.2 degrees, and Rz is more than 0.2 μm and not more than 1 μm, wherein Sm represents the average spacing of concavoconvexes in the anti-dazzling layer, θa represents the average inclination angle of the concavoconvexes, and Rz represents the average roughness of the concavoconvexes.

    METHOD AND APPARATUS FOR PRODUCING OPTICAL MULTILAYER BODY

    公开(公告)号:US20100255291A1

    公开(公告)日:2010-10-07

    申请号:US12695262

    申请日:2010-01-28

    IPC分类号: B32B5/16 B32B1/00

    摘要: An optical laminate produced by a process for producing an anti-dazzling laminate comprising a light transparent base material and an anti-dazzling layer provided on the light transparent base material. The process includes providing the light transparent base material and forming the anti-dazzling layer having a concavoconvex shape on the light transparent base material, wherein the concavoconvex shape of the anti-dazzling layer satisfies the following requirements: Sm is not less than 100 μm and not more than 600 μm, θa is not less than 0.1 degree and not more than 1.2 degrees, and Rz is more than 0.2 μm and not more than 1 μm, wherein Sm represents the average spacing of concavoconvexes or profile irregularities in the anti-dazzling layer; θa represents the average inclination angle of the concavoconvexes or profile irregularities; and Rz represents the average roughness of the concavoconvexes or profile irregularities.

    METHOD FOR PRODUCING OPTICAL LAYERED BODY, PRODUCTION APPARATUS OF OPTICAL LAYERED BODY, OPTICAL LAYERED BODY, POLARIZER AND IMAGE DISPLAY DEVICE
    16.
    发明申请
    METHOD FOR PRODUCING OPTICAL LAYERED BODY, PRODUCTION APPARATUS OF OPTICAL LAYERED BODY, OPTICAL LAYERED BODY, POLARIZER AND IMAGE DISPLAY DEVICE 有权
    光学层体的制造方法,光学层体的生产装置,光学层体,偏光镜和图像显示装置

    公开(公告)号:US20100097705A1

    公开(公告)日:2010-04-22

    申请号:US12377711

    申请日:2007-08-16

    摘要: There is provided a method for manufacturing an optical laminate in which properties such as a glare-proof property, an antidazzle property, and a black reproducible property for obtaining, for example, glossy black, can be simultaneously obtained. Manufacturing equipment for the optical laminate is also provided. The method for manufacturing an optical laminate having a light-transmitting substrate and a glare-proof layer formed on the light-transmitting substrate comprises a step of forming the glare-proof layer having an uneven shape on the light-transmitting substrate. When an average pitch of the surface unevenness of the optical laminate is denoted by Sm, an average slope angle of the unevenness by θa, and an average roughness of the unevenness by Rz, the uneven shape satisfies the following conditions: Sm is greater than or equal to 50 μm and less than 100 μm; θa is greater than or equal to 0.1 degrees and less than or equal to 1.0 degree; and Rz exceeds 0.2 μm and is less than or equal to 1.0 μm.

    摘要翻译: 提供了一种制造光学层叠体的方法,其中可以同时获得其中诸如防眩性,防眩性和用于获得例如光泽黑的黑色再现性质。 还提供了用于光学层压板的制造设备。 在透光性基板上形成有透光性基板和防眩光层的光学层叠体的制造方法包括在透光性基板上形成具有凹凸形状的防眩光层的工序。 当光学层叠体的表面凹凸的平均间距由Sm表示时,不均匀度的平均倾斜角度α和凹凸的平均粗糙度为Rz,凹凸形状满足以下条件:Sm较大 50μm以下且小于100μm; &thetas; a大于或等于0.1度且小于或等于1.0度; Rz超过0.2μm,小于等于1.0μm。

    Glare-proofing optical laminate
    17.
    发明授权
    Glare-proofing optical laminate 有权
    防眩光学层压板

    公开(公告)号:US08999463B2

    公开(公告)日:2015-04-07

    申请号:US11817818

    申请日:2006-03-29

    IPC分类号: C09K19/00 G02B5/02 G02B5/30

    摘要: An anti-dazzling laminate made of an optical laminate including a light transparent base material and an anti-dazzling layer having a concavoconvex shape provided on the material. The laminate simultaneously satisfies formulae: 0≦G100≦15 (I), 0.1≦Hs≦5.0 (II), 0.3≦Rz≦1.8 (III) wherein G100 represents a scintillation value which is a standard deviation of a variation in brightness distribution at a resolution of 100 ppi measured on the surface of the laminate; Hs represents the surface haze value of the laminate; and Rz represents the average roughness of the concavoconvex shape of the anti-dazzling layer.

    摘要翻译: 由光学层压制品制成的防光泽层压材料,该层压材料包括透明基材和具有凹凸形状的抗眩光层。 层压板同时满足公式:0&nlE; G100&nlE; 15(I),0.1&nlE; Hs&nlE; 5.0(II),0.3&nlE; Rz&nlE; 1.8(III)其中G100表示​​闪烁值,其是亮度变化的标准偏差 在层压板的表面上测量的分辨率为100ppi的分布; Hs表示层压板的表面雾度值; Rz表示防炫目层的凹凸形状的平均粗糙度。

    OPTICAL MULTILAYER BODY, POLARIZATION PLATE USING SAME, AND IMAGE DISPLAY
    19.
    发明申请
    OPTICAL MULTILAYER BODY, POLARIZATION PLATE USING SAME, AND IMAGE DISPLAY 有权
    光学多层体,使用相同的偏光板和图像显示

    公开(公告)号:US20120002397A1

    公开(公告)日:2012-01-05

    申请号:US13230961

    申请日:2011-09-13

    IPC分类号: G09F13/04 G02B5/02 G02B5/30

    摘要: An optical laminate is provided which has anti-dazzling properties and can realize excellent glare preventive properties and black reproducibility (gradation rendering of black at low brightness). The optical laminate includes a light transparent base material and an anti-dazzling layer or a light diffusion layer provided on the light transparent base material, wherein the outermost surface of the anti-dazzling layer or light diffusion layer has a concavoconvex surface. The anti-dazzling layer satisfies the requirements that Sm is not less than 100 μm and not more than 600 μm, θa is not less than 0.1 degree and not more than 1.2 degrees, and Rz is more than 0.2 μm and not more than 1 μm, wherein Sm represents the average spacing of concavoconvexes in the anti-dazzling layer, θa represents the average inclination angle of the concavoconvexes, and Rz represents the average roughness of the concavoconvexes.

    摘要翻译: 提供具有防炫目性能并且可以实现优异的防眩性和黑色再现性(低亮度下的黑色的渐变渲染)的光学层叠体。 光学层叠体包括透光基材和防透光层或设置在透光基材上的光漫射层,其中抗炫目层或光扩散层的最外表面具有凹凸表面。 抗眩光层满足Sm为100μm以上且600μm以下的要求,a为0.1度以上1.2以下,Rz为0.2μm以上, 1μm,其中Sm表示抗眩光层中的凹凸的平均间距,a表示凹凸的平均倾斜角,Rz表示凹凸的平均粗糙度。

    Optical multilayer body
    20.
    发明授权
    Optical multilayer body 有权
    光学多层体

    公开(公告)号:US07931953B2

    公开(公告)日:2011-04-26

    申请号:US11884403

    申请日:2006-02-21

    IPC分类号: G02B1/10 G02B5/30

    摘要: The present invention provides an anti-dazzling laminate which has anti-dazzling properties and can realize excellent glare preventive properties and black color reproducibility, such as gradation rendering of black color at low brightness. The optical laminate comprises a light transparent base material and an anti-dazzling layer provided on the light transparent base material. The outermost surface of the anti-dazzling layer has a concavoconvex surface, and the average spacing S determined by calculation based on data obtained by measuring a roughness curve of a concavoconvex shape of the anti-dazzling layer is not less than 0.04 mm and not more than 0.30 mm.

    摘要翻译: 本发明提供了具有防炫目性能的抗眩光层压材料,并且能够实现优异的防眩性和黑色再现性,例如低亮度下黑色的渐变渲染。 光学层叠体包括透光基材和设置在透光基材上的防炫光层。 防眩光层的最外表面具有凹凸面,通过基于通过测定抗眩光层的凹凸形状的粗糙度曲线得到的数据的计算确定的平均间隔S为0.04mm以上,不大于 大于0.30毫米。