GLASS-BASED ARTICLES INCLUDING A STRESS PROFILE COMPRISING TWO REGIONS

    公开(公告)号:US20230057346A1

    公开(公告)日:2023-02-23

    申请号:US17961188

    申请日:2022-10-06

    Abstract: Glass-based article including a first surface and a second surface opposing the first surface defining a thickness (t), and a stress profile are disclosed having a thickness (t) of about 3 millimeters or less, and wherein all points of the stress profile between a thickness range from about 0·t up to 0.3·t and from greater than 0.7·t, comprise a tangent with a slope that is less than about −0.1 MPa/micrometers or greater than about 0.1 MPa/micrometers. Also disclosed are glass-based articles having a thickness (t) in a range of 0.1 mm and 2 mm; and wherein at least one point of the stress profile in a first thickness range from about 0·t up to 0.020·t and greater than 0.98·t comprises a tangent with a slope of from about −200 MPa/micrometer to about −25 MPa/micrometer or about 25 MPa/micrometer to about 200 MPa/micrometer, and wherein all points of the stress profile in a second thickness range from about 0.035·t and less than 0.965·t comprise a tangent with a slope of from about −15 MPa/micrometer to about 15 MPa/micrometer.

    DEEP NON-FRANGIBLE STRESS PROFILES AND METHODS OF MAKING

    公开(公告)号:US20220315485A1

    公开(公告)日:2022-10-06

    申请号:US17848752

    申请日:2022-06-24

    Abstract: A non-frangible glass article strengthened by a dual or two-step ion exchange (IOX) process, where the first IOX step leads to a depth of compressive layer FSM_DOL>0.1·t or, in some embodiments, FSM_DOL>0.15·t, where t is the thickness of the glass, is provided. The glass article has a compressive stress CS1 after the first IOX step at the surface of from 100 MPa to 400 MPa or, in some embodiments, from 150 MPa to 300 MPa. The first IOX step is followed by a second IOX step, leading to a “spike” compressive stress CS2 after the second IOX step at the surface of greater than 500 MPa or, in some embodiments, 700 MPa. The width of the spike generated by the second IOX is between 1 μm and 30 μm, or between 8 μm and 15 μm, using the criteria where the magnitude (absolute value) of the slope of the spike is higher than 20 MPa/μm.

    Methods for regenerating lithium-enriched salt baths

    公开(公告)号:US11161781B2

    公开(公告)日:2021-11-02

    申请号:US16043442

    申请日:2018-07-24

    Abstract: Methods for regenerating poisoned salt bath comprising providing a salt bath comprising at least one of KNO3 and NaNO3, providing an ion-exchangeable substrate comprising lithium cations, contacting at least a portion of the ion-exchangeable substrate with the salt bath, whereby lithium cations in the salt bath diffuse from the ion-exchangeable substrate and are dissolved in the salt bath, and selectively precipitating dissolved lithium cations from the salt bath using phosphate salt. The methods further include preventing or reducing the formation of surface defects in the ion-exchangeable substrate by preventing or reducing the formation of crystals on the surface of the ion-exchangeable substrate upon removal from the salt bath.

    METHODS FOR REGENERATING LITHIUM-ENRICHED SALT BATHS

    公开(公告)号:US20200181011A1

    公开(公告)日:2020-06-11

    申请号:US16786452

    申请日:2020-02-10

    Abstract: Methods for regenerating poisoned salt bath comprising providing a salt bath comprising at least one of KNO3 and NaNO3, providing an ion-exchangeable substrate comprising lithium cations, contacting at least a portion of the ion-exchangeable substrate with the salt bath, whereby lithium cations in the salt bath diffuse from the ion-exchangeable substrate and are dissolved in the salt bath, and selectively precipitating dissolved lithium cations from the salt bath using phosphate salt. The methods further include preventing or reducing the formation of surface defects in the ion-exchangeable substrate by preventing or reducing the formation of crystals on the surface of the ion-exchangeable substrate upon removal from the salt bath.