公开(公告)号:US06399538B1
公开(公告)日:2002-06-04
申请号:US09717867
申请日:2000-11-21
申请人: Dennis A. Hucul
发明人: Dennis A. Hucul
IPC分类号: B01J2300
摘要: A hydrogenation catalyst and a process for hydrogenating an unsaturated polymer comprising contacting the unsaturated polymer with a hydrogenating agent in the presence of a mixed hydrogenation catalyst, characterized in that the mixed hydrogenation catalyst comprises a Group VIII metal component and at least one component selected from the group consisting of a rhenium, molybdenum, tungsten, tantalum and niobium component.
摘要翻译: 氢化催化剂和用于氢化不饱和聚合物的方法,包括在混合氢化催化剂存在下使不饱和聚合物与氢化剂接触,其特征在于混合氢化催化剂包含VIII族金属组分和至少一种选自 由铼,钼,钨,钽和铌组分组成的组。
-
公开(公告)号:US5336822A
公开(公告)日:1994-08-09
申请号:US75962
申请日:1993-06-14
申请人: Dennis A. Hucul
发明人: Dennis A. Hucul
摘要: 4-Vinylcyclohexene is converted to styrene in the presence of a catalyst comprising tin, antimony, and oxygen. The feed stream to be contacted with the catalyst comprises water, 4-vinylcyclohexene, and oxygen. A ratio of water to 4-vinylcyclohexene above about 12:1, preferably above about 14:1, significantly increases the half-life of the catalyst. The catalyst is prepared by coprecipitating a tin chloride and an antimony chloride followed by calcination of the precipitate at a temperature in the range from 850.degree. C. to 1000.degree. C.
摘要翻译: 在包含锡,锑和氧的催化剂存在下,将4-乙烯基环己烯转化为苯乙烯。 与催化剂接触的进料流包括水,4-乙烯基环己烯和氧。 高于约12:1,优选高于约14:1的水与4-乙烯基环己烯的比率显着增加了催化剂的半衰期。 催化剂通过将氯化锡和氯化锑共沉淀,然后在850℃至1000℃的温度下煅烧沉淀物来制备。
-
公开(公告)号:US5110779A
公开(公告)日:1992-05-05
申请号:US696676
申请日:1991-05-07
申请人: Dennis A. Hucul
发明人: Dennis A. Hucul
CPC分类号: C08C19/02 , B01J23/40 , B01J35/002 , B01J35/0053 , B01J35/1009 , B01J35/1014 , B01J35/1047 , B01J35/108 , C08F8/04
摘要: The hydrogenation of unsaturated polymers is effected employing a heterogeneous catalyst comprising a Group VIII metal and a porous support wherein the porous support is characterized by a pore size distribution such that at least 95% of the pore volume is defined by pores having diameters greater than 450 angstroms and the ratio of metal surface area to carrier surface area is in the range from about 0.07-0.75:1.
摘要翻译: 使用包含VIII族金属和多孔载体的多相催化剂进行不饱和聚合物的氢化,其中多孔载体的特征在于孔径分布,使得至少95%的孔体积由直径大于450的孔限定 埃和金属表面积与载体表面积的比例在约0.07-0.75:1的范围内。
-
公开(公告)号:US4554391A
公开(公告)日:1985-11-19
申请号:US642989
申请日:1984-08-22
IPC分类号: C07C17/08
CPC分类号: C07C17/08
摘要: The invention is a process for preparing a 2-halo-1-alkene comprising contacting a hydrocarbon stream with a hydrogen halide, in the presence of water and an effective amount of a catalyst, at a temperature between about 100.degree. C. and about 400.degree. C., wherein; the hydrocarbon stream comprises a 1,2-diene, a terminal acetylene or mixtures thereof, represented by the formulas CH.sub.2 .dbd.C.dbd.CH--R or CH.tbd.C--CH.sub.2 --R wherein R is hydrogen, alkyl, cycloalkyl or aryl and may be substituted or unsubstituted; the water is present in an amount of between about 1,000 and 100,000 parts per million by weight; and the catalyst comprises carbon, silica alumina, aluminosilicates, silica gel, silica, silica magnesia, silicalite, group IIIA, IIIB, IVA, IVB or V metal oxides or rare earth oxides.
摘要翻译: 本发明是一种制备2-卤代-1-烯烃的方法,包括在约100℃至约400℃的温度下,在水和有效量的催化剂存在下使烃流与卤化氢接触 ℃。 烃流包含由式CH 2 = C = CH-R或CH 3 CH 2 CH 2 -R表示的1,2-二烯,末端乙炔或其混合物,其中R是氢,烷基,环烷基或芳基,并且可以是 取代或未取代的; 水的存在量为每百万重量约1,000至100,000份; 催化剂包括碳,二氧化硅氧化铝,硅铝酸盐,硅胶,二氧化硅,二氧化硅氧化镁,硅沸石,IIIA,IIIB,IVA,IVB或V族金属氧化物或稀土氧化物。
-
-
-