Abstract:
The invention provides aqueous thermosetting binder compositions exhibiting both of improved flame retardation and wet tensile strength comprising a reducing sugar, a diprimary diamine or a polyprimary diamine, a phosphorus acid salt and from 3 to 20 wt. %, based on total solids, of an aqueous polymeric polyacid solution polymer containing phosphorus or its salt, wherein the aqueous thermosetting binder composition comprises from 0.7% P (s/s) to 5% P (s/s).
Abstract:
The present invention provides compositions comprising particles or agglomerates of one or more telomer or cotelomer ((co)telomer) of one or more methacrylic acids or anhydrides having a mean average particle size of from 2 μm to 1 mm, preferably from 5 to 500 μm. In addition, the present invention provides methods comprising aqueous solution addition polymerizing a monomer mixture of one or more methacrylic acid in the presence of a heteroatom containing compound, drying the resulting copolymer at a temperature of from 120 to 230° C. and reducing its particle size to make a (co)telomer particle or agglomerate; the methods may further comprise reacting the (co)telomer particle or agglomerate with one or more polyether polyol, alkyl polyether polyol, polyether amine or alkyl polyether amine, with heating, to form a comb polymer useful, e.g. as a superplasticizer or dispersant.
Abstract:
The present invention provides thermosetting aqueous binder compositions comprising one or more reducing sugar, one or more diprimary diamine or poly(primary amine), and from 7 to 45 wt. %, based on total solids, of one or more polysaccharide having a dextrose equivalent (DE) value of from 5 to 30. The compositions provide treated articles, such as fiberglass mat. The binders provide articles having a dramatically reduced binder weight loss upon cure and a reduction in cure energy needed to achieve early dry strength.
Abstract:
The present invention provides thermosetting aqueous binder compositions comprising a diprimary amine or poly(primary amine) and one or more water soluble oxidized dextrin made by oxidizing a dextrin having a DE value of from 2 to 25 and having from 2 to 10 millieq CHO/g of dry oxidized dextrin or a larger oxidized dextrin or an oxidized dextrin made by oxidizing a dextrin having a DE value of below 2 and having from 0.25 to 5 millieq CHO/g of dry oxidized dextrin. The aqueous biobased binders provide hot wet tensile strength when heat cured.
Abstract translation:本发明提供了包含二原子胺或聚(伯胺)和一种或多种水溶性氧化糊精的热固性水性粘合剂组合物,其通过氧化DE值为2至25的糊精和具有2至10毫克CHO / g 的干氧化糊精或通过氧化DE值低于2的糊精和0.25至5毫克CHO / g干氧化糊精制成的较大氧化糊精或氧化糊精。 水性生物基粘合剂在热固化时提供热湿拉伸强度。