21.
公开(公告)号:US4390460A
公开(公告)日:1983-06-28
申请号:US306600
申请日:1981-09-28
申请人: Katsuki Miyauchi , Tetsu Oi , Tsuneo Suganuma
发明人: Katsuki Miyauchi , Tetsu Oi , Tsuneo Suganuma
CPC分类号: G02F1/1525 , C03C3/097 , C03C4/18 , H01M6/18 , H01M6/185
摘要: Disclosed is a lithium oxide based amorphous material having a composition included in a region defined by lines connecting points A, B, C and D in the composition diagram of the ternary system of Li.sub.2 O.SiO.sub.2.P.sub.2 O.sub.5 shown in FIG. 1 of the accompanying drawings. This amorphous material can be formed by performing sputtering by using as a target a mixture of a lithium silicate/lithium phosphate composition and LiO.sub.2. This amorphous material is excellent in the ionic conductivity.
摘要翻译: 公开了一种氧化锂基非晶材料,其组成包括在图3所示的Li 2 O·SiO 2·P 2 O 5的三元体系的组成图中由连接点A,B,C和D的线所限定的区域中。 附图1。 可以通过使用硅酸锂/磷酸锂组合物和LiO 2的混合物作为靶来进行溅射来形成该非晶材料。 该无定形材料的离子导电性优异。
-
公开(公告)号:US4259101A
公开(公告)日:1981-03-31
申请号:US17025
申请日:1979-03-02
申请人: Yasuo Tsukuda , Katsuyuki Imoto , Kenzo Susa , Iwao Matsuyama , Tsuneo Suganuma
发明人: Yasuo Tsukuda , Katsuyuki Imoto , Kenzo Susa , Iwao Matsuyama , Tsuneo Suganuma
IPC分类号: C03B37/018 , C03B37/014 , G02B6/00 , C03C25/02 , C03B37/02
CPC分类号: C03B37/01406
摘要: A method for producing an optical fiber preform comprising the steps of blowing, through at least one nozzle, gaseous material producing glass material soot by a CVD reaction to permit the glass material soot to be deposited on a target to produce a soot rod which grows in size, and heating and rendering transparent the soot rod produced in the first step, wherein a pipe is arranged substantially concentrically with the glass material soot so as to permit gas to flow through a clearance between the deposited glass material soot and the inner wall surface of the pipe in a direction in which the soot rod grows in size. The method makes it possible to prevent the outer peripheral portion of the soot rod from becoming porous and to satisfactorily control the diameter of the soot rod.
摘要翻译: 一种制造光纤预制棒的方法,包括以下步骤:通过至少一个喷嘴吹送通过CVD反应产生玻璃材料烟灰的气态材料,以允许玻璃材料烟灰沉积在目标上以产生烟炱棒,其生长在 尺寸和加热并使第一步骤中产生的烟灰杆透明,其中管道与玻璃材料烟灰基本上同心地布置,以允许气体流过沉积的玻璃材料烟灰和内壁表面之间的间隙 管子在烟炱杆生长的方向上。 该方法可以防止烟炱杆的外周部变得多孔,并且令人满意地控制烟炱杆的直径。
-