摘要:
Set forth herein are electrolyte compositions that include both organic and inorganic constituent components and which are suitable for use in rechargeable batteries. Also set forth herein are methods and systems for making and using these composite electrolytes.
摘要:
A current collector layer for an all-solid-state battery is provided with which a good electron path can be easily formed and rate characteristic can be improved. A current collector layer 5 for an all-solid-state battery 1, the current collector layer 5 including: a carbon material; and a solid electrolyte, the all-solid-state battery 1 including a group 1 or 2 ion conductive solid electrolyte layer 2, the carbon material being mixed with Si at a weight ratio of 1:1 to produce a mixture, the mixture having an X-ray diffraction spectrum having a ratio of a peak height a to a peak height b, a/b, of 0.2 or more and 10.0 or less as being measured, the peak height a being highest in a range of 2θ of 24° or more and less than 28°, and the peak height b being highest in a range of 2θ of 28° or more and less than 30°.
摘要:
A voltage source includes two electrically conductive terminals (101, 102) with an electrolyte (103) between them. Said electrolyte (103) is a mixture in which the main component is ash produced in a power plant or an incineration plant.
摘要:
An example composition is disclosed. For example, the composition includes a ultra-violet (UV) curable mixture of water, an acid, a phosphine oxide with one or more photoinitiators, a water miscible polymer, a salt, and a neutralizing agent. The composition can be used to form an electrolyte layer that can be cured in the presence of air when printing the thin-film battery.
摘要:
An energy storage capacitor has a solid dielectric sandwiched between two electrodes. The solid dielectric is a lanthanum-doped barium titanate-based ceramic material. A dopant is selected from the group consisting of lanthanum hydroxide and lanthanum oxide, and a co-dopant is an alkali hydroxide selected from the group consisting of potassium hydroxide, sodium hydroxide, rubidium hydroxide, and lithium hydroxide.
摘要:
In accordance with the present invention, deposition of LiCoO2 layers in a pulsed-dc physical vapor deposition process is presented. Such a deposition can provide a low-temperature, high deposition rate deposition of a crystalline layer of LiCoO2 with a desired or orientation. Some embodiments of the deposition address the need for high rate deposition of LiCoO2 films, which can be utilized as the cathode layer in a solid state rechargeable Li battery. Embodiments of the process according to the present invention can eliminate the high temperature (>700° C.) anneal step that is conventionally needed to crystallize the LiCoO2 layer.
摘要:
The present disclosure provides an electrochemical storage cell including a battery. The battery includes an alkali metal anode having an anode Fermi energy, an electronically insulating, amorphous, dried solid electrolyte able to conduct alkali metal, having the general formula A3-xHxOX, in which 0≦x≦1, A is the alkali metal, and X is at least one halide, and a cathode including a cathode current collector having a cathode Fermi energy lower than the anode Fermi energy. During operation of the electrochemical storage cell, the alkali metal plates dendrite-free from the solid electrolyte onto the alkali metal anode. Also during operation of the electrochemical storage cell, the alkali metal further plates on the cathode current collector.
摘要:
A lithium ion conductor represented by Formula 1: Li1+x+2yAlxMgyM2−x−y(PO4)3 Formula 1 wherein, in Formula 1, M includes at least one of titanium (Ti), germanium (Ge), zirconium (Zr), hafnium (Hf), and tin (Sn), 0
摘要:
A lithium-lanthanum-titanium oxide sintered material has a lithium ion conductivity 3.0×10−4 Scm−1 or more at a measuring temperature of 27° C., the material is described by one of general formulas (1-a)LaxLi2-3xTiO3-aSrTiO3, (1-a)LaxLi2-3xTiO3-aLa0.5K0.5TiO3, LaxLi2-3xTi1-aMaO3-a, and Srx-1.5aLaaLi1.5-2xTi0.5Ta0.5O3 (0.55≦x≦0.59, 0≦a≦0.2, M=at least one of Al, Fe and Ga), and concentration of S is 1500 ppm or less. The material is obtained by sintering raw material powder mixture having S content amount of 2000 ppm or less in the entirety of raw material powders for mixture, that is, titanium raw material, lithium raw material, and lanthanum raw material.
摘要:
A solid electrolyte suitable for use in all solid type lithium ion secondary battery is made by sintering a form, particularly a greensheet, comprising at least lithium ion conductive inorganic substance powder. The solid electrolyte has porosity of 20 vol % or over.