摘要:
An electrostatic image forming toner including: toner base particles each containing at least a colorant, a binder resin, and a releasing agent, wherein the binder resin contains a non-crystalline polyester resin A and a crystalline polyester resin B, wherein a ratio of B/(A+B)×100 is 10 or more but less than 50 where (A+B) is a total mass of the non-crystalline polyester resin A and the crystalline polyester resin B and “B” is a mass of the crystalline polyester resin B, and wherein the toner base particles have a TMA compression deformation amount (TMA %) of 10% or less which is measured at 50° C. and a relative humidity of 90%.
摘要:
A method for producing a polymer, including: (i) bringing a compressive fluid and raw materials containing a ring-opening polymerizable monomer into contact with each other at a mixing ratio represented by the following formula, to thereby allow the ring-opening polymerizable monomer to carry out ring-opening polymerization in the presence of a metal catalyst: 1{Mass of the raw materials/(Mass of the raw materials+Mass of the compressive fluid)}0.5.
摘要:
An electrophotographic toner including: a binder resin, wherein the binder resin has one glass transition temperature Tg and the glass transition temperature Tg of the binder resin is within 25° C. to 65° C. as measured in second heating with a differential scanning calorimeter at a heating rate of 5° C./min, and wherein a phase image of the binder resin obtained with an atomic force microscope (AFM) of tapping mode contains first phase difference regions and a second phase difference region such that the first phase difference regions are dispersed in the second phase difference region, where the first phase difference regions correspond to greater phase difference regions and the second phase difference region corresponds to a smaller phase difference region when an intermediate value between a maximum value and a minimum value of the phase differences is used as a threshold.
摘要:
A toner, including: a crystalline resin; a non-crystalline resin; and a colorant, wherein the toner has a sea-island structure which includes a sea containing the crystalline resin and an island containing the non-crystalline resin and the colorant, wherein the island is 1.0 μm or less in domain diameter, and wherein the toner is 1.7×104 Pa or less in storage elastic modulus at 160° C.
摘要:
The toner includes a pigment; and a block copolymer having a polyester block A including a residual group of a hydroxycarboxylic acid, and a polyester block B including an anionic group. When cross-section of the block copolymer is observed by a tapping mode atomic force microscope to obtain a phase image of the cross-section, the polyester block B, which has relatively large phase delay, is dispersed as domains having an average size of from 20 nm to 100 nm in a domain of the polyester block A, which has relatively small phase delay. The block copolymer has a first glass transition temperature of from −20° C. to 20° C., and a second glass transition temperature of from 35° C. to 65° C. when the first and second glass transition temperatures are determined from a thermogram obtained by subjecting the block copolymer to differential scanning calorimetry (DSC) at a temperature rising speed of 5° C./min.
摘要:
To provide a toner including at least a binder resin and a colorant, wherein the binder resin has two glass transition temperatures Tg1 and Tg2 in a differential scanning calorimetry at a heating speed of 5° C./min, the glass transition temperature Tg1 is −20° C. to 20° C., and the glass transition temperature Tg2 is 35° C. to 65° C., wherein the binder resin comprises a polyester skeleton and a ring-containing skeleton molecule at ends thereof, and wherein the binder resin is obtained by block copolymerization of: a polyester skeleton A which includes a structural unit obtained by dehydration condensation of a hydroxycarboxylic acid in a repeating structure; and a skeleton B which does not include a structural unit obtained by dehydration condensation of a hydroxycarboxylic acid in a repeating structure.
摘要:
A toner including a colorant and a first binder resin is provided. The first binder resin has first and second glass transition points at a temperature Tg1 of −20 to 20° C. and a temperature Tg2 of 35 to 65° C., respectively, measured by a differential scanning calorimeter at a heating rate of 5° C./min. A ratio h1/h2 of a baseline displacement h1 observed in the first glass transition point to a baseline displacement h2 observed in the second glass transition point is less than 1.0. The first binder resin has a structure in which a first phase is dispersed in a second phase. The first and second phases consist of portions having larger and smaller phase difference values, respectively, than an intermediate value between maximum and minimum phase difference values in a binarized phase image obtained by an atomic force microscope with a tapping mode method.
摘要:
Toner contains a binder resin, wherein the binder resin contains a block copolymer A containing a crystalline segment X and a non-crystalline segment Y, wherein the toner has a thermo-mechanical analysis (TMA) compressive deformation amount (TMA %) of 10% or less at 50° C. and a relative humidity of 90%, wherein the toner has a spin-spin relaxation time (t130) of 10 ms or greater at 130° C. as measured by pulse nuclear magnetic resonance (NMR), wherein the toner has a spin-spin relaxation time (t′70) of 1 ms or less at 70° C. as measured by pulse NMR when descending from 130° C. to 70° C.
摘要:
The toner includes a pigment; and a block copolymer having a polyester block A including a residual group of a hydroxycarboxylic acid, and a polyester block B including an anionic group. When cross-section of the block copolymer is observed by a tapping mode atomic force microscope to obtain a phase image of the cross-section, the polyester block B, which has relatively large phase delay, is dispersed as domains having an average size of from 20 nm to 100 nm in a domain of the polyester block A, which has relatively small phase delay. The block copolymer has a first glass transition temperature of from −20° C. to 20° C., and a second glass transition temperature of from 35° C. to 65° C. when the first and second glass transition temperatures are determined from a thermogram obtained by subjecting the block copolymer to differential scanning calorimetry (DSC) at a temperature rising speed of 5° C./min.