摘要:
A friction stir welding anvil and method of producing a friction stir welding anvil that precludes diffusion or mechanical bonding of the anvil to the work pieces are provided. The alternatives for producing such an anvil comprise coating the anvil with diffusion barriers such as oxides, nitrides, intermetallics, and/or refractory metals; manufacturing an anvil either completely or partially from the same; or placing a coating of such materials in the form of a thin sheet or a powder between the anvil and the work pieces. The anvil disclosed herein exhibits high strength and hardness even at elevated temperatures, such as those greater than 800° C., so as to prevent the anvil from mechanically or diffusion bonding to the work pieces and so as to minimize, or eliminate altogether, anvil deformation.
摘要:
A method comprising a bulk processing technique for joining different metals and alloys using friction stir welding, wherein a block of a first material has at least two apertures disposed therein, wherein at least a first tube and a second tube are disposed in the at least two apertures, wherein friction stir welding is performed to join the block, the first tube and the second tube together in a solid state form, and the resulting workpiece is then machined to produce the completed joint.
摘要:
A probe for friction stir welding MMCs, ferrous alloys, non-ferrous alloys, and superalloys, as well as non-ferrous alloys, the probe including a shank, a shoulder, and a pin disposed through the shoulder and into the shank, wherein the pin and the shoulder at least include a coating comprised of a superabrasive material, the pin and shoulder being designed to reduce stress risers, disposing a collar around a portion of the shoulder and the shank to thereby prevent movement of the shoulder relative to the shank, and incorporating thermal management by providing a thermal flow barrier between the shoulder and the shank, and between the collar and the tool.
摘要:
This invention comprises a diamond insert grinding process to remove stress riser cracks formed in a critical area of a tungsten carbide insert body. The cracks are caused by leaching of cobalt from the carbide during the process of brazing a tungsten carbide backed polycrystalline diamond disc to the body. A grinding wheel selectively removes material from the intersection of the braze below the depth of the cracks in the tungsten carbide body thereby relieving the stress riser in the critical area of the body.