Abstract:
A glass composition, glass article prepared from the glass composition, and display device are provided. The glass article includes, as a glass composition, about 45 to about 65 mol % of SiO2, about 15 to about 25 mol % of Al2O3, about 15 to about 25 mol % of Na2O, and 0 to about 10 mol % of B2O3 based on a total weight of the glass composition, where the glass composition has a thermal expansion coefficient of about 70*10−7 K−1 to about 85*10−7 K−1.
Abstract:
A glass article includes a first surface, a second surface opposed to the first surface, a first compressive region extending from the first surface to a first compression depth, a second compressive region extending from the second surface to a second compression depth and a tensile region between the first compression depth and the second compression depth. A stress profile of the first compressive region includes a first segment located between the first surface and a first transition point and a second segment located between the first transition point and the first compression depth. A depth from the first surface to the first transition point ranges from 6.1 μm to 8.1 μm. A compressive stress at the first transition point ranges from 207 MPa to 254 MPa. A stress-depth ratio of the first transition point ranges from 28 MPa/μm to 35 MPa/μm.
Abstract:
A glass article includes first and second surfaces opposed to each other; a first compressive region extending from the first surface to a point at a first compression depth; a second compressive region extending from the second surface to a point a second compression depth; and a tensile region disposed between the first and second compressive regions. A stress profile of the first compressive region includes a first segment between the first surface and a first transition point and a second segment between the first transition point and the first compression depth. A depth from the first surface to the first transition point is 8.1 μm to 9.5 μm, a stress at the first transition point is greater than or equal to 197 MPa, and a stress at a point of 50 μm in a depth direction from the first surface is greater than or equal to 75 MPa.
Abstract:
A glass article includes lithium aluminosilicate, includes a first surface, a second surface opposed to the first surface, a first compressive region extending from the first surface to a first compression depth, a second compressive region extending from the second surface to a second compression depth, and, a tensile region disposed between the first compression depth and the second compression depth, where a stress profile of the first compressive region has a first local minimum point at which the stress profile is convex downward and a first local maximum point at which the stress profile is convex upward, where a depth of the first local maximum point is greater than a depth of the first local minimum point, and where a stress of the first local maximum point is greater than a compressive stress of the first local minimum point.
Abstract:
A method of treating a glass substrate includes providing a glass substrate and strengthening the glass substrate by providing a mixed molten salt including a strengthening molten salt and an aluminum salt to the glass substrate.
Abstract:
A method for fabricating a reinforced glass substrate includes forming a plurality of groove patterns in at least one surface of a plate glass, applying an ion exchange paste to the at least one surface in which the groove patterns are formed, applying an electric field to the plate glass coated with the ion exchange paste to form a reinforced plate glass, and cutting the reinforced plate glass to form a reinforced glass substrate.
Abstract:
The present disclosure relates to a method of preparing an antimicrobial glass, which includes: preparing a glass substrate; preparing a dry paste; selectively coating the dry paste at least a portion of the glass substrate; heat-treating the coated glass substrate after the coating; and cleaning the heat -treated glass substrate, wherein the preparation of the dry paste includes preparing a diluted solution by diluting a salt including silver ions or copper ions in water, and adding a metal oxide to the diluted solution, and an antimicrobial glass prepared according to the method.
Abstract:
Provided is a flexible display device, including at least one flexible substrate on which a display unit is formed and a filling portion at a curved portion of the at least one flexible substrate.
Abstract:
A window includes a base region and a compressive stress region disposed on the base region. The compressive stress region includes Li+, Na+, and K+ ions. The compressive stress region includes a first compressive stress portion in which a concentration of the K+ ions decreases, a concentration of Na+ ions increases, and a concentration of the Li+ ions increases, from a surface of the window toward the base region. A second compressive stress portion is adjacent to the first compressive stress portion. In the second compressive stress portion, the concentration of the Na+ ion decreases and the concentration of the Li+ ion increases, from the first compressive stress portion toward the base region. The window thereby has a high surface compressive stress value and impact resistance.
Abstract:
A method for manufacturing a glass article for a display device includes: providing a LAS-based glass; a first step of immersing the LAS-based glass in a first molten salt; a second step of immersing the LAS-based glass subjected to the first step in a second molten salt; and a third step of immersing the LAS-based glass subjected to the second step in a third molten salt, wherein the concentrations of the first, second, and third molten salts and manufacturing conditions are defined herein.