摘要:
To provide a toner, which contains a binder resin, a colorant, and a releasing agent, wherein the binder resin contains a low molecular weight resin component, where the low molecular weight resin component has a resin softening coefficient (A), represented by the following formula (1), satisfying A>0.165, and has storage elastic modulus (dyne/cm2) G′(Tfb) satisfying G′(Tfb)≦1×104 where Tfb is a flow onset temperature (° C.) of the low molecular weight resin component as measured by a capillary rheometer: A=|[(r1)−ln G′(r2)]/(T1−T2)| Formula (1) (where T1 is temperature (° C.) at which storage elastic modulus G′(r1) is 1×105 (dyne/cm2) and T2 is temperature (° C.) at which storage elastic modulus G′(r2) is 1×103 (dyne/cm2) as measured by means of a viscoelasticity measuring device with measuring frequency of 1 Hz, and measuring distortion of 1 deg; and | | represents an absolute value.).
摘要翻译:为了提供含有粘合剂树脂,着色剂和脱模剂的调色剂,其中粘合剂树脂含有低分子量树脂组分,其中低分子量树脂组分具有树脂软化系数(A),由 (1)满足A> 0.165,并且具有满足G'(Tfb)≦̸ 1×104的储能弹性模量(dyne / cm 2)G'(Tfb),其中Tfb是流动起始温度(℃) 通过毛细管流变仪测量的低分子量树脂组分:A = | [(r1)-ln G'(r2)] /(T1-T2)| 储存弹性模量G'(r1)为1×10 5(达因/ cm 2)且T2为储存弹性模量G'(℃)的温度(℃)的式(1)(其中,T1为温度(℃) r2)是通过测量频率为1Hz的粘弹性测量装置测量的1×10 3(dyne / cm 2),测量失真度为1度,| |表示绝对值。
摘要:
A toner is provided that contains a binder resin; a colorant; a release agent; and an external additive, wherein the toner has an average circularity of from 0.940 to 0.965 and a crater having a depth of from 0.02 to 0.1 μm, and wherein the crater has an amount of the external additive larger than an average amount thereof on the toner, along with a two-component developer containing the toner and an image forming apparatus using the toner.
摘要:
A toner is provided that contains a particulate toner material (mother toner) having an average circularity of from 0.93 to 0.99, and including a modified polyester resin and a colorant; and an external additive in an amount of from 0.3 to 5.0 parts by weight per 100 parts by weight of the mother toner, wherein the toner has a melting viscosity of from 70 to 140 Pa·s at 160° C., a weight-average particle diameter of from 3 to 7 μm, a ratio thereof to a number-average particle diameter of from 1.91 to 1.25, wherein particles satisfy at least one of (I) and (II): (I) particles having a diameter of 4 μm or less in an amount less than 10% by number; or (II) particles having a diameter of 8 μm or more in an amount less than 2% by volume, along with a one or two component developer containing the toner, a cartridge containing the toner, an image forming method using the toner and an image forming apparatus using the toner.
摘要:
A method for producing a toner, containing: dispersing, in an aqueous medium, an oil phase which contains an organic solvent, and a binder resin component contained in the organic solvent, where the binder resin component contains a crystalline polyester resin and an amorphous polyester resin; and removing the organic solvent from the dispersion to obtain the toner, in which the dispersing further contains heating and dissolving the crystalline polyester and the amorphous polyester in the organic solvent to obtain a solution, cooling the solution so as to recrystallize the crystalline polyester resin, and mechanically pulverizing the recrystallized crystalline polyester resin so as to obtain a crystalline polyester dispersion.
摘要:
To provide a toner, which contains a binder resin, a colorant, and a releasing agent, wherein the binder resin contains a low molecular weight resin component, where the low molecular weight resin component has a resin softening coefficient (A), represented by the following formula (1), satisfying A>0.165, and has storage elastic modulus (dyne/cm2) G′(Tfb) satisfying G′(Tfb)≦1×104 where Tfb is a flow onset temperature (° C.) of the low molecular weight resin component as measured by a capillary rheometer: A=|[ln G′(r1)−ln G′(r2)]/(T1−T2)| Formula (1) (where T1 is temperature (° C.) at which storage elastic modulus G′(r1) is 1×105 (dyne/cm2) and T2 is temperature (° C.) at which storage elastic modulus G′(r2) is 1×103 (dyne/cm2) as measured by means of a viscoelasticity measuring device with measuring frequency of 1 Hz, and measuring distortion of 1 deg; and ∥ represents an absolute value.)
摘要翻译:为了提供含有粘合剂树脂,着色剂和脱模剂的调色剂,其中粘合剂树脂含有低分子量树脂组分,其中低分子量树脂组分具有树脂软化系数(A),由 (1)满足A> 0.165,并且具有满足G'(Tfb)≦̸ 1×104的储能弹性模量(dyne / cm 2)G'(Tfb),其中Tfb是流动起始温度(℃) 通过毛细管流变仪测量的低分子量树脂组分:A = | [ln G'(r1)-ln G'(r2)] /(T1-T2)| 储存弹性模量G'(r1)为1×10 5(达因/ cm 2)且T2为储存弹性模量G'(℃)的温度(℃)的式(1)(其中,T1为温度(℃) r2)是通过测量频率为1Hz的粘弹性测量装置测量的1×103(dyne / cm 2),测量失真度为1度,∥表示绝对值。
摘要:
An image forming apparatus including an image bearing member; a charger; a light irradiator; a developing device; a transfer device; an image bearing member's cleaner; and a fixing device, wherein the fixing device includes a fixing member configured to fix a toner image upon application of heat and pressure thereto; a pressing member configured to press the recording material toward the fixing member; and a cleaning member configured to clean a surface of the fixing member and/or the pressing member, wherein the cleaning member has an outermost layer including a reactive material which increases viscoelasticity of a binder resin of the toner by reacting with the binder resin.
摘要:
A toner which includes a toner material, wherein the toner satisfies the following formula: 0° C.≦ΔTm≦20° C. where ΔTm represents Tma (° C.)−Tmb (° C.), Tma (° C.) is ½ flown-out temperature of the toner by a capillary type flow tester, and Tmb (° C.) is ½ flown-out temperature of a melt kneaded mixture of the toner by the capillary type flow tester, and wherein Tma is from 130° C. to 200° C.
摘要:
An image forming apparatus including an image bearing member; a charger; a light irradiator; a developing device; a transfer device; an imagebearingmember's cleaner; anda fixing device, wherein the fixing device includes a fixing member configured to fix a toner image upon application of heat and pressure thereto; a pressing member configured to press the recording material toward the fixing member; and a cleaning member configured to clean a surface of the fixing member and/or the pressing member, wherein the cleaning member has an outermost layer including a reactive material which increases viscoelasticity of a binder resin of the toner by reacting with the binder resin.
摘要:
The present invention provides a method for producing a toner, the method including: preparing a wax dispersion liquid by cooling a wax solution, in which a wax is heated and dissolved or dispersed in an organic solvent, in a container so that a standard deviation σ of a temperature distribution between a center portion of the container and an inner wall of the container is 0.5 or less and the cooling rate is 2.0° C./min or more, to precipitate wax particles in the wax solution; forming toner base precursor particles by adding an aqueous phase containing resin fine particles into an oil phase containing at least the wax dispersion liquid, a colorant and a binder resin and mixing the oil phase and the aqueous phase with each other; and preparing toner base particles by removing the solvent from the toner base precursor particles.
摘要:
A toner, comprising a colorant, a crystalline polyester resin, and an amorphous polyester resin, in which the crystalline polyester resin satisfies the following relations: 60≦(T2-cp)