Abstract:
A foam concrete with elemental sulfur has constituents that include a cement, a fine filler, an elemental sulfur in powder form, a coarse aggregate, a water, and a foam solution. The foam solution includes a foaming agent and a foaming water. The foam concrete has a compressive strength of at least 26 MPa, a thermal conductivity of less than 0.30 W/mK and a maximum dry weight of 1620 kg/m3.
Abstract:
A heavy oil ash self-compacting concrete can include aggregate, heavy oil ash fines, water, and cement. The heavy oil ash can include more than 90% carbon, by weight. In an embodiment, the heavy oil ash self-compacting concrete can flow under its own weight and yet maintain a stable mixture consistency.
Abstract:
A concrete mixture that includes aggregates, water and cement can include heavy oil ash instead of or in addition to a portion of the cement. In one embodiment, the heavy oil ash originates from heavy fuel oil burned in a power generation plant. The weight of the heavy oil ash used in the concrete mixture can be from greater than 0 to about 10% of the weight of the cement.
Abstract:
A sulfur-sand limestone mortar and methods of preparing the sulfur-sand limestone mortar and disposing of elemental sulfur, are disclosed. In embodiments, the sulfur-sand limestone mortar includes elemental sulfur, limestone powder, and sand. Modifiers, such as plasticizers, are not required and are not used in embodiments of the sulfur-sand limestone mortar. In embodiments of the method to prepare the sulfur-sand limestone mortar, each of the elemental sulfur, limestone powder, and sand are heated to at least 140 C, then combined, and then allowed to solidify.
Abstract:
A sulfur-steel slag aggregate concrete, and methods of preparing the sulfur-steel slag aggregate concrete and disposing of elemental sulfur, are disclosed. In embodiments, the sulfur-steel slag aggregate concrete includes elemental sulfur, steel slag aggregate, limestone powder, and sand. Modifiers, such as plasticizers, are not required and are not used in embodiments of the sulfur-sand limestone mortar. In embodiments of the method to prepare the sulfur-steel slag aggregate concrete, each of the elemental sulfur, limestone powder, steel-slag, and sand are heated to at least 140 C, then combined, and then allowed to solidify.