    摘要: A sulfur-sand limestone mortar and methods of preparing the sulfur-sand limestone mortar and disposing of elemental sulfur, are disclosed. In embodiments, the sulfur-sand limestone mortar includes elemental sulfur, limestone powder, and sand. Modifiers, such as plasticizers, are not required and are not used in embodiments of the sulfur-sand limestone mortar. In embodiments of the method to prepare the sulfur-sand limestone mortar, each of the elemental sulfur, limestone powder, and sand are heated to at least 140 C, then combined, and then allowed to solidify.

    摘要翻译: 公开了一种硫砂石灰石砂浆和硫砂石灰石砂浆的制备方法和单质硫的处理方法。 在实施例中,硫砂石灰石砂浆包括元素硫,石灰石粉和砂。 不需要改性剂,例如增塑剂,在硫砂石灰石砂浆的实施方案中不使用改性剂。 在制备硫砂石灰石砂浆的方法的实施方案中,将每种元素硫,石灰石粉和砂加热至至少140℃,然后合并,然后使其固化。

    SULFUR STEEL-SLAG AGGREGATE CONCRETE
    9.
    发明申请
    SULFUR STEEL-SLAG AGGREGATE CONCRETE 有权
    SULFUR钢渣混凝土

    公开(公告)号:US20130192495A1

    公开(公告)日:2013-08-01

    申请号:US13751885

    申请日:2013-01-28

    IPC分类号: C04B7/153

    摘要: A sulfur-steel slag aggregate concrete, and methods of preparing the sulfur-steel slag aggregate concrete and disposing of elemental sulfur, are disclosed. In embodiments, the sulfur-steel slag aggregate concrete includes elemental sulfur, steel slag aggregate, limestone powder, and sand. Modifiers, such as plasticizers, are not required and are not used in embodiments of the sulfur-sand limestone mortar. In embodiments of the method to prepare the sulfur-steel slag aggregate concrete, each of the elemental sulfur, limestone powder, steel-slag, and sand are heated to at least 140 C, then combined, and then allowed to solidify.

    摘要翻译: 公开了一种硫钢渣骨料混凝土,以及硫钢渣骨料混凝土的制备方法和单质硫的处理方法。 在实施方案中,硫钢渣骨料混凝土包括元素硫,钢渣骨料,石灰石粉和砂。 不需要改性剂,例如增塑剂,在硫砂石灰石砂浆的实施方案中不使用改性剂。 在制备硫钢渣骨料混凝土的方法的实施方案中,将元素硫,石灰石粉末,钢渣和砂子中的每一种加热至至少140℃,然后合并,然后使其固化。