THERMOPLASTIC POLYCARBONATE COPOLYMER COMPOSITIONS, METHODS OF THEIR MANUFACTURE, AND USES THEREOF
    42.
    发明申请
    THERMOPLASTIC POLYCARBONATE COPOLYMER COMPOSITIONS, METHODS OF THEIR MANUFACTURE, AND USES THEREOF 审中-公开
    热塑性聚碳酸酯共聚物组合物,其制造方法及其用途

    公开(公告)号:US20140335298A1

    公开(公告)日:2014-11-13

    申请号:US14445175

    申请日:2014-07-29

    CPC classification number: B32B5/00 C08K5/523 C09K21/12 C09K21/14 Y10T428/1397

    Abstract: This disclosure relates to thermoplastic compositions comprising a polycarbonate copolymer, the polycarbonate copolymer comprising first repeating carbonate units and second repeating units selected from carbonate units that are different from the first carbonate units, polysiloxane units, and a combination comprising at least one of the foregoing unit; and an organophosphorus flame retardant in an amount effective to provide 0.1 to 1.0 wt % phosphorus based on the total weight of the composition, wherein an article molded from the composition has a smoke density after 4 minutes (Ds-4) of less than or equal to 600 determined according to ISO 5659-2 on a 3 mm thick plaque, and a material heat release of less than or equal to 160 kW/m2 determined according to ISO 5660-1 on a 3 mm thick plaque.

    Abstract translation: 本公开涉及包含聚碳酸酯共聚物的热塑性组合物,聚碳酸酯共聚物包含第一重复碳酸酯单元和选自不同于第一碳酸酯单元的碳酸酯单元的第二重复单元,聚硅氧烷单元,以及包含至少一个上述单元 ; 和有机磷阻燃剂,其量有效地提供0.1至1.0重量%的磷,基于组合物的总重量,其中由该组合物模制的制品在4分钟后具有小于或等于4分钟的烟密度(Ds-4) 至600根据ISO 5659-2测定,厚度为3毫米厚,根据ISO 5660-1测定的材料放热量小于或等于160千瓦/平方米,厚度为3毫米厚。