ABS-moulding compounds with an improved combination of properties
    52.
    发明授权
    ABS-moulding compounds with an improved combination of properties 失效
    ABS成型化合物具有改进的性能组合

    公开(公告)号:US06384133B1

    公开(公告)日:2002-05-07

    申请号:US09831853

    申请日:2001-05-15

    IPC分类号: C08L5502

    摘要: A thermoplastic molding composition having improved mechanical properties is disclosed. The ABS composition that comprise a graft rubber polymer obtained by emulsion polymerization in the presence of specifically defined butadiene polymer latices and a rubber-free copolymer is suitable for making molded articles.

    摘要翻译: 公开了具有改进的机械性能的热塑性模塑组合物。 在具体限定的丁二烯聚合物胶乳和无橡胶共聚物的存在下,通过乳液聚合获得的包含接枝橡胶聚合物的ABS组合物适于制备模制品。

    Polymer alloys of high ageing resistance
    54.
    发明授权
    Polymer alloys of high ageing resistance 失效
    耐老化的聚合物合金

    公开(公告)号:US5274031A

    公开(公告)日:1993-12-28

    申请号:US435057

    申请日:1989-11-13

    CPC分类号: C08L51/04 C08L51/085

    摘要: Molding compounds ofA) 5 to 95 parts by weight of a graft product of resin-forming monomers on a particulate silicone rubber having a total rubber content of from 30 to 90% by weight andB) 95 to 5 parts by weight of resin-forming monomers on a particulate EPDM rubber having a total rubber content of 10 to 50% by weight andC) 10 to 200 parts by weight (based on 100 parts by weight A+B) of a graft product of resin-forming monomers on a particulate acrylate rubber having a total rubber content of from 30 to 80% by weight.

    摘要翻译: A)成型化合物A)5至95重量份的树脂形成单体的接枝产物在总橡胶含量为30至90重量%的颗粒状硅橡胶上,B)95至5重量份树脂 - 在总橡胶含量为10至50重量%的颗粒状EPDM橡胶上形成单体,C)10至200重量份(基于100重量份A + B)的树脂形成单体的接枝产物 总橡胶含量为30至80重量%的颗粒状丙烯酸酯橡胶。

    Polymeric dihydroxy compounds and their use as stabilizers for polymers
    55.
    发明授权
    Polymeric dihydroxy compounds and their use as stabilizers for polymers 失效
    聚合二羟基化合物及其作为聚合物稳定剂的用途

    公开(公告)号:US4859731A

    公开(公告)日:1989-08-22

    申请号:US223541

    申请日:1988-07-25

    IPC分类号: C08F8/00

    CPC分类号: C08F8/00

    摘要: Polymer dihydroxy compounds corresponding to the following formula ##STR1## in whichR.sup.1, R.sup.2, R.sup.3 =H or C.sub.1 -C.sub.4 alkyl,R.sup.4 =H or C.sub.1 -C.sub.4 alkyl,R.sup.5 =--C.sub.6 H.sub.5, --C.sub.6 H.sub.4 CH.sub.3, --CH.dbd.CH.sub.2, or --CO.sub.2 R.sup.7,R.sup.6 =C.sub.1 -C.sub.4 alkyl, aryl, or H,R.sup.7 =C.sub.1 -C.sub.4 alkyl,m=0 or 1,n=5 to 100,q=0 or 1,a process for their production and their use in thermoplastic molding compositions.

    摘要翻译: 对应于下式的化合物二羟基化合物,其中R1,R2,R3 = H或C1-C4烷基,R4 = H或C1-C4烷基,R5 = -C6H5,-C6H4CH3,-CH = CH2或 - CO 2 R 7,R 6 = C 1 -C 4烷基,芳基或H,R 7 = C 1 -C 4烷基,m = 0或1,n = 5〜100,q = 0或1,其制备方法及其在热塑性成型 组合物。

    Elastic-thermoplastic graft polymers prepared by multi-stage free radical polymerization

    公开(公告)号:US06569951B2

    公开(公告)日:2003-05-27

    申请号:US09967311

    申请日:2001-09-28

    IPC分类号: C08F27904

    摘要: An elastic-thermoplastic graft polymer prepared by a multi-stage free radical polymerization is described. The elastic-thermoplastic graft polymer is prepared by polymerizing (i) one or more monomers containing vinyl groups, and (ii) at least one molecular weight regulating compound, in the presence of (iii) at least one rubber in latex form. The ratio of monomers (M) to the molecular weight regulating compound (MWR) is altered throughout the various stages of the polymerization method. The M:MWR ratio is: from 50:1 to 400:1 in the first stage; from 100:1 to 800:1 in the second stage; and from 200:1 to 2000:1 in the third stage of the polymerization. In at least one further reaction stage of the polymerization, the monomers, in the absence of the molecular weight regulating compound, are polymerized in the presence of the rubber. This further reaction stage occurs before the first stage and/or after the third stage of the polymerization. The multi-stage polymerization is conducted such that: M:MWR (first stage)≦M:MWR (second stage)

    ABS type thermoplastic moulding compounds
    60.
    发明授权
    ABS type thermoplastic moulding compounds 失效
    ABS型热塑性成型料

    公开(公告)号:US5719232A

    公开(公告)日:1998-02-17

    申请号:US424656

    申请日:1995-04-19

    IPC分类号: C08F2/22 C08L55/02

    CPC分类号: C08L55/02 Y10S525/902

    摘要: ABS type thermoplastic moulding compounds obtainable by A) producing a rubber latex with an average particle diameter d.sub.50 of 30 to 160 nm and a gel content of 75 to 100 wt. % B) emulsion polymerization of an amount of butadiene and optionally up to 50 wt. % (with reference to the total amount of monomer in stage B) of a comonomer in the presence of the rubber obtained in stage A, such that a rubber latex (B) with an average particle diameter d.sub.50 =220 to 330 nm and a gel content of 25 to 70 wt. % is produced, C) emulsion polymerization of 40 to 95 parts by wt. of a mixture of styrene and acrylonitrile, which optionally contains up to 50 wt. % (with reference to the total amount of monomers used in stage C) of one or more comonomers, in the presence of 5 to 60 parts by wt. (with reference to the solids) of the rubber obtained in stage B by introducing the monomer in such a way that 55 to 90 wt. % of the monomers are added within the first half of the total monomer introduction time, and D) mixing the polymer obtained in stage C, preferably after first converting it into a powder, with at least one thermoplastic vinyl resin.

    摘要翻译: ABS型热塑性成型化合物,其可通过以下方法得到:A)制备平均粒径d50为30〜160nm,凝胶含量为75〜100重量%的橡胶胶乳。 B)一定量的丁二烯的乳液聚合和任选的至多50wt。 在阶段A中获得的橡胶存在下,共聚单体的%(相对于阶段B中的单体的总量),使得平均粒径d 50 = 220〜330nm的橡胶胶乳(B)和凝胶 含量为25〜70wt。 产生%,C)乳液聚合40〜95重量份。 的苯乙烯和丙烯腈的混合物,其任选地含有至多50重量% 在5至60重量份存在下,一种或多种共聚单体的%(相对于阶段C中使用的单体的总量)。 (相对于固体),通过以55〜90重量%的比例引入单体,得到阶段B中得到的橡胶。 在全部单体引入时间的前半部分内加入%的单体,和D)将在阶段C中获得的聚合物,优选在首先将其转化为粉末之后,与至少一种热塑性乙烯基树脂混合。