摘要:
A toner containing a colorant, a binder resin and a laminar inorganic mineral in which part or all of the ions present between layers are modified by organic ions. The toner can be prepared by a method including dispersing or emulsifying a toner constituent mixture liquid containing the colorant, the binder resin and/or a precursor thereof, and the laminar inorganic mineral, in an aqueous medium. The density of the laminar inorganic mineral measured by XPS for the toner surface before (A) and after(B) mixing and kneading satisfies the following relationship: A>B.
摘要:
A toner including a binder resin, wherein a toner extract obtained by drying an extraction liquid obtained through Soxhlet extraction of the toner with tetrahydrofuran (THF) has glass transition temperature Tg in a range of from 35° C. through 55° C., and a moisture-content change rate of the toner extract before and after leaving the toner extract to stand for 3 days in an environment of 40° C. and 70% RH is 0.5% or less, and wherein a specific-surface-area change rate of the toner before and after leaving the toner to stand for 3 days in an environment of 40° C. and 70% RH is in a range of from 15% through 50%.
摘要:
A toner including a binder resin, wherein a toner extract obtained by drying an extraction liquid obtained through Soxhlet extraction of the toner with tetrahydrofuran (THF) has glass transition temperature Tg in a range of from 35° C. through 55° C., and a moisture-content change rate of the toner extract before and after leaving the toner extract to stand for 3 days in an environment of 40° C. and 70% RH is 0.5% or less, and wherein a specific-surface-area change rate of the toner before and after leaving the toner to stand for 3 days in an environment of 40° C. and 70% RH is in a range of from 15% through 50%.
摘要:
A toner housing container includes: a container body housing a toner; a conveying portion; a pipe receiving port; and an uplifting portion. Flow rate index of the toner measured by powder rheometer and represented by “flow rate index=(total energy at a rotation speed of 10 mm/s)/(total energy at a rotation speed of 100 mm/s)” is in a range of “1.8≦flow rate index≦6.5”. Container body includes protruding portion protruding from container body interior side of container opening portion toward one end of container body. Uplifting portion includes: uplifting wall surface extending from container body internal wall surface toward protruding portion; and curving portion curving to conform to protruding portion. When the toner housing container is mounted on the toner conveying device, the protruding portion is present between the curving portion and the toner receiving port of the conveying pipe being inserted.
摘要:
A toner including at least one polyester resin serving as a binder resin, a colorant, a releasing agent, and a fixing aid, wherein the fixing aid includes a fatty acid amide-based compound, and the fatty acid amide-based compound is at least one of a fatty acid amide compound having a mono- or higher valent amide bond and a fatty acid amide-based compound having a mono- or higher valent amino group or a hydroxyl group.
摘要:
A set of toners including yellow, cyan, magenta, and black toner, each of which containing a binder resin containing a crystalline resin and a non-crystalline resin, a releasing agent, and a corresponding coloring agent, wherein the following relationship is satisfied: 0.8
摘要:
A toner including: a binder resin containing a non-crystalline resin and a crystalline resin; a colorant; and, a releasing agent, wherein the releasing agent has a melting point of 55° C. to 80° C., and wherein the toner satisfies the following Expressions 1 and 2: (Expression 1): 20,000 Pa·s≦G1≦50,000 Pa·s; and (Expression 2): (G4/G2)/(G3/G1) 1.00, where G1 is a storage modulus, G2 is a loss modulus, G3 is a storage modulus and G4 is a loss modulus, and the storage modulus G1 and the loss modulus G2 are measured at 80° C. when the toner is heated from 70° C. to 150° C. and the storage modulus G3 and the loss modulus G4 are measured at 80° C. when the toner heated to 150° C. is cooled to 70° C.
摘要:
A method for producing a toner, containing: dispersing, in an aqueous medium, an oil phase which contains an organic solvent, and a binder resin component contained in the organic solvent, where the binder resin component contains a crystalline polyester resin and an amorphous polyester resin; and removing the organic solvent from the dispersion to obtain the toner, in which the dispersing further contains heating and dissolving the crystalline polyester and the amorphous polyester in the organic solvent to obtain a solution, cooling the solution so as to recrystallize the crystalline polyester resin, and mechanically pulverizing the recrystallized crystalline polyester resin so as to obtain a crystalline polyester dispersion.
摘要:
A toner including a core particle, an inner shell layer covering the core, and an outer shell layer covering the inner shell layer is provided. The core particle includes a resin P. The inner shell layer includes fine particles of a resin A. The outer shell layer includes fine particles of a resin B. The toner satisfies the following formulae (1) to (3): 4.5≦T½(P)−Tfb(P)≦14 (1) 20≦T½(A)−Tfb(A)≦40 (2) 23.5≦T½(B)−Tfb(B)≦40 (3) wherein T½(P), T½(A), and T½(B) represent ½ method temperatures of the resins P, A, and B, respectively, and Tfb(P), Tfb(A), and Tfb(B) represent flow beginning temperatures of the resins P, A, and B, respectively, and wherein the ½ method temperatures and the flow beginning temperatures are measured by a flowtester.
摘要翻译:提供了包括芯颗粒,覆盖芯的内壳层和覆盖内壳层的外壳层的调色剂。 核心颗粒包括树脂P.内壳层包括树脂A的细颗粒。外壳层包括树脂B的细颗粒。调色剂满足下式(1)至(3):4.5@T 1/2( P)-Tfb(P)@ 14(1)20 @ T 1/2(A)-Tfb(A)@ 40(2)23.5@T½(B)-Tfb(B)@ 40(3) T 1/2(A)和T 1/2(B)分别表示树脂P,A和B的1/2方法温度,Tfb(P),Tfb(A)和Tfb(B)表示树脂P的流动开始温度 ,A和B,并且其中1/2方法温度和流动开始温度由流动器测量。
摘要:
To provide a toner, which contains a binder resin, a colorant, and a releasing agent, wherein the binder resin contains a low molecular weight resin component, where the low molecular weight resin component has a resin softening coefficient (A), represented by the following formula (1), satisfying A>0.165, and has storage elastic modulus (dyne/cm2) G′(Tfb) satisfying G′(Tfb)≦1×104 where Tfb is a flow onset temperature (° C.) of the low molecular weight resin component as measured by a capillary rheometer: A=|[ln G′(r1)−ln G′(r2)]/(T1−T2)| Formula (1) (where T1 is temperature (° C.) at which storage elastic modulus G′(r1) is 1×105 (dyne/cm2) and T2 is temperature (° C.) at which storage elastic modulus G′(r2) is 1×103 (dyne/cm2) as measured by means of a viscoelasticity measuring device with measuring frequency of 1 Hz, and measuring distortion of 1 deg; and ∥ represents an absolute value.)
摘要翻译:为了提供含有粘合剂树脂,着色剂和脱模剂的调色剂,其中粘合剂树脂含有低分子量树脂组分,其中低分子量树脂组分具有树脂软化系数(A),由 (1)满足A> 0.165,并且具有满足G'(Tfb)≦̸ 1×104的储能弹性模量(dyne / cm 2)G'(Tfb),其中Tfb是流动起始温度(℃) 通过毛细管流变仪测量的低分子量树脂组分:A = | [ln G'(r1)-ln G'(r2)] /(T1-T2)| 储存弹性模量G'(r1)为1×10 5(达因/ cm 2)且T2为储存弹性模量G'(℃)的温度(℃)的式(1)(其中,T1为温度(℃) r2)是通过测量频率为1Hz的粘弹性测量装置测量的1×103(dyne / cm 2),测量失真度为1度,∥表示绝对值。