摘要:
The invention relates to a method of producing elongate metal strands or fibres with a crucible, the method comprising the steps of; directing molten metal through a nozzle having a nozzle direction in a deposition direction at a regulated pressure difference between the inside and the outside of the crucible; depositing said molten metal from said nozzle on a rotating planar surface having an axis of rotation; entraining said molten metal in one plane via said rotating planar surface to form elongate metal strands, wherein said rotating surface is aligned at an alignment angle, to the deposition direction during the entraining of the molten metal; cooling said elongate metal strands to form solidified metal strands; and guiding said metal strands to collecting means to collect the solidified metal strands formed on the rotating planar surface.
摘要:
A mold used for centrifugal casting includes a mold body formed in a cylindrical shape and a lid member (40) that is detachably assembled to an end part of the mold body in an axial direction. The lid member includes a lid body (41) that is attached to an opening part formed at the end part of the mold body, a protrusion part (450) that is fitted to the mold body, and a spring that applies elastic force to the lid body in a direction in which the lid body closely contacts the mold body.
摘要:
A method for manufacturing a high-strength blade-type golf iron head with a thin blade includes placing a shell mold onto a rotary table. At least one metal ingot is placed into a crucible portion of the shell mold and is heated to melt in a vacuum environment. The rotary table rotates to cause the molten metal to flow into a cavity portion of the shell mold. The rotating shaft is slowly stopped, and the shell mold is removed after pouring. The shell mold is destroyed after the molten metal cools and solidifies, obtaining a casting. A cast product portion is separated from the casting to obtain at least one blade-type golf iron head having the blade with a minimum thickness of 3.5-5.0 mm. The weight of the blade-type golf iron head is reduced by 0.9-2.5%, and the center of gravity of the blade-type golf iron head is lowered by 0.2-0.75 mm.
摘要:
A method of assembling a centrifugal casting apparatus includes positioning a wedge on a rotatable axis and positioning at least two molds into sealing engagement with the wedge. Each of the at least two molds includes a front face and defines at least two cavities extending from the front face into the mold. A sprue chamber is defined and is structured to receive molten material, and at least a portion of the sprue chamber is defined by at least a portion of the front faces of the at least two molds.
摘要:
Various enhanced features are provided for centrifugal casting apparatuses, rotatable assemblies, and molds for casting products from molten material. These enhanced features include, among others, tapered gate portions positioned adjacent to the cavities of a mold, extended and shared gating systems, and detachable mold structures for modifying the thermodynamic characteristics and behavior of molds during casting operations.
摘要:
Various enhanced features are provided for centrifugal casting apparatuses, rotatable assemblies, and molds for casting products from molten material. These enhanced features include, among others, tapered gate portions positioned adjacent to the cavities of a mold, extended and shared gating systems, and detachable mold structures for modifying the thermodynamic characteristics and behavior of molds during casting operations.
摘要:
A method for manufacturing a high-strength blade-type golf iron head with a thin blade includes placing a shell mold onto a rotary table. At least one metal ingot is placed into a crucible portion of the shell mold and is heated to melt in a vacuum environment. The rotary table rotates to cause the molten metal to flow into a cavity portion of the shell mold. The rotating shaft is slowly stopped, and the shell mold is removed after pouring. The shell mold is destroyed after the molten metal cools and solidifies, obtaining a casting. A cast product portion is separated from the casting to obtain at least one blade-type golf iron head having the blade with a minimum thickness of 3.5-5.0 mm. The weight of the blade-type golf iron head is reduced by 0.9-2.5%, and the center of gravity of the blade-type golf iron head is lowered by 0.2-0.75 mm.