公开(公告)号:US4123504A
公开(公告)日:1978-10-31
申请号:US784593
申请日:1977-04-04
Applicant: Alexandr A. Shulzhenko , Anatoly F. Getman
Inventor: Alexandr A. Shulzhenko , Anatoly F. Getman
CPC classification number: B01J3/062 , B01J2203/061 , B01J2203/0655 , B01J2203/068
Abstract: A method of diamond synthesis, by which a reaction mixture is prepared comprising, taken in direct contact, a carbon-containing material and a combination of components selected from the group containing silver chloride, calcium carbonate, calcium oxide and from a group containing aluminium and boron. Then the reaction mixture is subjected to the action of a temperature of at least about 1800.degree. C and a pressure corresponding to a selected temperature within the diamond stable region during the time required for forming a diamond.
Abstract translation: 一种金刚石合成方法,通过该方法制备反应混合物,其包括直接接触含碳材料和选自含氯化银,碳酸钙,氧化钙和含有铝的组的组分的组合,以及 硼。 然后在形成金刚石所需的时间内将反应混合物进行至少约1800℃的温度和对应于金刚石稳定区域内的选定温度的压力。
-
公开(公告)号:US4349517A
公开(公告)日:1982-09-14
申请号:US199273
申请日:1980-10-21
Applicant: Vladislav S. Lysanov , Viktor V. Digonsky , Leon I. Feldgun , Valery M. Davidenko , Nikolai V. Novikov , Alexandr I. Borimsky , Alexandr A. Shulzhenko , Valerian D. Yakimenko , Eduard Y. Dovgal , Vitaly Y. Egorov , Vyacheslav S. Rovsha , Alexei I. Prikhna , Alexandr N. Sokolov
Inventor: Vladislav S. Lysanov , Viktor V. Digonsky , Leon I. Feldgun , Valery M. Davidenko , Nikolai V. Novikov , Alexandr I. Borimsky , Alexandr A. Shulzhenko , Valerian D. Yakimenko , Eduard Y. Dovgal , Vitaly Y. Egorov , Vyacheslav S. Rovsha , Alexei I. Prikhna , Alexandr N. Sokolov
IPC: C04B35/5831 , C01B35/14
CPC classification number: C04B35/5831
Abstract: Disclosed is a method of producing cubic boron nitride, which comprises the steps of subjecting to a pressure of from 40 to 70 kilobars and to a temperature of from 1100.degree. to 2000.degree. C. a charge including hexagonal boron nitride and a conversion initiator selected from the group consisting of alkali and alkaline earth metals and borides of the foregoing metals, doping the charge with crystallohydrate in the form of a compound selected from the group consisting of sulfur-, halogen- or nitrogen-containing salts and their mixtures incorporating at least 5 molecules of crystallization water. According to another embodiment, the aforesaid charge is doped with a member selected from the group consisting of alkali metal hydroxide or alkaline earth metal hydroxide.
Abstract translation: 公开了一种制备立方氮化硼的方法,其包括以下步骤:施加40至70千巴的压力和1100至2000℃的温度。包含六方氮化硼和选自以下的转化引发剂的电荷 由碱金属和碱土金属组成的组和前述金属的硼化物,以选自硫,卤素或含氮盐的化合物形式的晶体水合物掺杂电荷,并且其混合物至少掺入5 分子结晶水。 根据另一个实施方案,上述电荷掺杂有选自碱金属氢氧化物或碱土金属氢氧化物的成员。
-