摘要:
A lead-free piezoelectric ceramic material has the general chemical formula xBi(Zn0.5Ti0.5)O3-y(Bi0.5K0.5)TiO3-z(Bi0.5Na0.5)TiO3, wherein x+y+z=1 and x, y, z≠0.
摘要翻译:无铅压电陶瓷材料具有一般化学式xBi(Zn0.5Ti0.5)O3-y(Bi0.5K0.5)TiO3-z(Bi0.5Na0.5)TiO3,其中x + y + z = 1 x,y,z <0。
摘要:
The present invention relates to a method for identifying a solid solution ceramic material of a plurality of perovskite compounds which exhibits an electric field induced strain derived from a reversible phase transition, as well as a method for making such ceramic materials and ceramic materials obtainable therefrom. In particular, the present invention is directed to a method of identifying a solid solution ceramic material of at least three perovskite compounds which exhibits an electric field induced strain derived from a reversible phase transition; said method comprising the steps of: i) determining a molar ratio of at least one tetragonal perovskite compound to at least one non-tetragonal perovskite compound which, when combined to form a solid solution, provides a ceramic material comprising a major portion of a tetragonal phase having an axial ratio c/a of greater than 1.005 to 1.04; and ii) determining a molar ratio of at least one additional non-tetragonal perovskite compound to the combination of perovskite compounds from step i) at the determined molar ratio which, when combined to form a solid solution, provides a ceramic material comprising a major portion of a pseudo-cubic phase having an axial ratio c/a of from 0.995 to 1.005 and/or a rhombohedral angle of 90±0.5 degrees.
摘要:
A lead-free piezoelectric ceramic material has the general chemical formula xBi(A0.5Ti0.5)O3-y(Bi0.5K0.5)TiO3-z(Bi0.5Na0.5)TiO3, wherein x+y+z=1, x≠0, and A=Ni or Mg.
摘要翻译:无铅压电陶瓷材料具有一般化学式xBi(A0.5Ti0.5)O3-y(Bi0.5K0.5)TiO3-z(Bi0.5Na0.5)TiO3,其中x + y + z = 1 ,x <0,A = Ni或Mg。
摘要:
The present invention relates to a bismuth-based solid solution ceramic material, as well as a process for preparing the ceramic material and uses thereof, particularly in an actuator component employed, for example, in a droplet deposition apparatus. In particular, the present invention relates to a ceramic material having a general chemical formula (I): (I): x(Bi0.5Na0.5)TiO3-y(Bi0.5K0.5)TiO3-z1SrHfO3-z2SrZrO3, wherein x+y+Z1+Z2=1; y, (z1+z2)≠0; x≥0. In embodiments, the present invention also relates to a ceramic material having a general chemical formula (II): x(Bi0.5Na0.5)TiO3-y(Bi0.5K0.5)TiO3-y(Bi0.5K0.5)TiO3-ZiSrHfO3-z2SrZrO3, wherein x+y+z−i+z2=1; x, y, fa+z2)≠0; as well as a ceramic material of general formula (III): y(Bi0.5K0.5)TiO3-z1SrHfO3-z2SrZrO3, wherein y+z1,+z2=1; y, (z1+z2)≠0.
摘要:
A lead-free piezoelectric ceramic material has the general chemical formula xBi(A0.5Ti0.5)O3-y(Bi0.5K0.5)TiO3-z(Bi0.5Na0.5)TiO3, wherein x+y+z=1, x≠0, and A=Ni or Mg.
摘要翻译:无铅压电陶瓷材料具有一般化学式xBi(A0.5Ti0.5)O3-y(Bi0.5K0.5)TiO3-z(Bi0.5Na0.5)TiO3,其中x + y + z = 1 ,x≠0,A = Ni或Mg。
摘要:
The present invention relates to a method for identifying a solid solution ceramic material of a plurality of perovskite compounds which exhibits an electric field induced strain derived from a reversible phase transition, as well as a method for making such ceramic materials and ceramic materials obtainable therefrom. In particular, the present invention is directed to a method of identifying a solid solution ceramic material of at least three perovskite compounds which exhibits an electric field induced strain derived from a reversible phase transition; said method comprising the steps of: i) determining a molar ratio of at least one tetragonal perovskite compound to at least one non-tetragonal perovskite compound which, when combined to form a solid solution, provides a ceramic material comprising a major portion of a tetragonal phase having an axial ratio c/a of greater than 1.005 to 1.04; and ii) determining a molar ratio of at least one additional non-tetragonal perovskite compound to the combination of perovskite compounds from step i) at the determined molar ratio which, when combined to form a solid solution, provides a ceramic material comprising a major portion of a pseudo-cubic phase having an axial ratio c/a of from 0.995 to 1.005 and/or a rhombohedral angle of 90±0.5 degrees.
摘要:
The present invention relates to a bismuth-based solid solution ceramic material, as well as a process for preparing the ceramic material and uses thereof, particularly in an actuator component employed, for example, in a droplet deposition apparatus. In particular, the present invention relates to a ceramic material having a general chemical formula (I): (I): x(Bi0.5Na0.5)TiO3-y(Bi0.5K0.5)TiO3-z1SrHfO3-z2SrZrO3, wherein x+y+Z1+Z2=1; y, (z1+z2)≠0; x≥0. In embodiments, the present invention also relates to a ceramic material having a general chemical formula (II): x(Bi0.5Na0.5)TiO3-y(Bi0.5K0.5)TiO3-y(Bi0.5K0.5)TiO3-ZiSrHfO3-z2SrZrO3, wherein x+y +z-i+z2=1; x, y, fa+z2)≠0; as well as a ceramic material of general formula (III): y(Bi0.5K0.5)TiO3-z1SrHfO3-z2SrZrO3, wherein y+z1,+z2=1; y, (z1+z2)≠0.