Molybdenum sulfide cathode structure
    1.
    发明授权
    Molybdenum sulfide cathode structure 失效
    硫化钼阴极结构

    公开(公告)号:US4237204A

    公开(公告)日:1980-12-02

    申请号:US88828

    申请日:1979-10-29

    CPC classification number: H01M10/05 H01M4/02 H01M4/762

    Abstract: The present invention is directed to an electric current-producing cell which contains:(a) an anode having as its anode-active material one or more metals selected from a group consisting of Periodic Table Group Ia metals, Group Ib metals, Group IIa metals and Group IIb metals;a cathode, comprising:(i) metalized containment means having a plurality of apertures therein, said apertures having an average cross-sectional dimension of about 1 to about 100 microns; and(ii) cathode-active molybdenum sulfide contained within said metalized containment means; and(c) an electrolyte which is chemically inert with respect to said anode and said cathode and which permits the migration of ions between said anode and said cathode.

    Abstract translation: 本发明涉及一种电流产生电池,其包含:(a)阳极,其具有作为其阳极活性材料的一种或多种金属,其选自周期表第Ia族金属,第Ib族金属,第IIa族金属 和IIb族金属; 阴极,包括:(i)金属化的容纳装置,其中具有多个孔,所述孔具有约1至约100微米的平均横截面尺寸; 和(ii)包含在所述金属化容纳装置内的阴极活性硫化钼; 和(c)相对于所述阳极和所述阴极化学惰性的电解质,并允许离子在所述阳极和所述阴极之间迁移。

    Aromatics hydrogenation with a new class of metal oxides
    2.
    发明授权
    Aromatics hydrogenation with a new class of metal oxides 失效
    芳烃氢化与一类新型的金属氧化物

    公开(公告)号:US5767037A

    公开(公告)日:1998-06-16

    申请号:US516890

    申请日:1995-08-18

    Abstract: The present invention is directed toward a highly active aromatics hydrogenation catalyst and its use. The catalyst composition is prepared by: (a) decomposing a catalyst precursor selected from the group consisting of metal amine molybdates, metal amine tungstates and mixtures thereof, wherein said metal amine catalyst precursor has the general formula ML(Mo.sub.y W.sub.1-y O.sub.4)a where M is Cr and/or one or more divalent promoter metals selected from the group consisting of Mn, Fe, Co, Ni, Cu and Zn; L is one or more neutral nitrogen containing ligands at least one of which is a chelating polydentate ligand; 0.ltoreq.y.ltoreq.1; and a=1 for non-chromium containing catalysts and wherein 0.5.ltoreq.a.ltoreq.3 for chromium containing catalysts, at a temperature of about 200.degree. to about 400.degree. C. in an inert atmosphere; and (b) reducing at a temperature of about 300.degree. to about 450.degree. C. said metal amine catalyst precursor to form a catalyst. The catalyst as prepared above may be used in an aromatics hydrogenation process. The invention is further directed to the use of such catalysts in aromatics hydrogenation processes.

    Abstract translation: 本发明涉及高活性芳烃氢化催化剂及其用途。 催化剂组合物通过以下步骤制备:(a)分解选自钼酸金属胺,钨酸金属胺及其混合物的催化剂前体,其中所述金属胺催化剂前体具有通式ML(MoyW1-yO4)a其中M 是选自Mn,Fe,Co,Ni,Cu和Zn中的Cr和/或一种或多种二价助催化剂金属; L是一种或多种中性含氮配体,其中至少一种是螯合多齿配体; 0