1.
公开(公告)号:US07923527B1
公开(公告)日:2011-04-12
申请号:US12579007
申请日:2009-10-14
Applicant: Cheng-Chien Yang , Jui-Ming Yeh , Chia-Shiang Yang , Yuen-Hsin Peng , Kuan-Yeh Huang
Inventor: Cheng-Chien Yang , Jui-Ming Yeh , Chia-Shiang Yang , Yuen-Hsin Peng , Kuan-Yeh Huang
IPC: C08G69/28
CPC classification number: C08G73/105 , B82Y30/00 , C08G73/0266 , C08G73/1042 , C08K3/041 , C08L79/08 , C08L2203/20
Abstract: The invention provides a carbon nanotube compound and method for producing the same. The method of the invention comprises the following steps. Firstly, Aniline-trimer and DMAc(dimethyl acetamide) solution are mixed to form a first solution. Secondly, Dianhydride and DMAc solution are mixed to form a second solution. The first solution and the second are mixed to form a third solution. Additionally, carboxyl-multiwall carbon nanotubes (c-MWNT), Diaminodiphenylether and DMAc solution are mixed to form a fourth solution. The third solution and the fourth are mixed to form a polyamic acid/CNT solution. Some polyamic acid/CNT solution is spread on a substrate and processed by a thermal treatment, and a carbon nanotube compound is eventually produced.
Abstract translation: 本发明提供一种碳纳米管化合物及其制造方法。 本发明的方法包括以下步骤。 首先,将苯胺 - 三聚体和DMAc(二甲基乙酰胺)溶液混合以形成第一溶液。 其次,将二酐和DMAc溶液混合以形成第二溶液。 将第一溶液和第二溶液混合以形成第三溶液。 另外,将羧基 - 多壁碳纳米管(c-MWNT),二氨基二苯醚和DMAc溶液混合以形成第四溶液。 将第三溶液和第四溶液混合以形成聚酰胺酸/ CNT溶液。 将一些聚酰胺酸/ CNT溶液涂布在基材上,通过热处理进行处理,最终生成碳纳米管化合物。
-
2.
公开(公告)号:US20110086960A1
公开(公告)日:2011-04-14
申请号:US12579007
申请日:2009-10-14
Applicant: Cheng-Chien Yang , Jui-Ming Yeh , Chia-Shiang Yang , Yuen-Hsin Peng , Kuan-Yeh Huang
Inventor: Cheng-Chien Yang , Jui-Ming Yeh , Chia-Shiang Yang , Yuen-Hsin Peng , Kuan-Yeh Huang
IPC: C08K5/09
CPC classification number: C08G73/105 , B82Y30/00 , C08G73/0266 , C08G73/1042 , C08K3/041 , C08L79/08 , C08L2203/20
Abstract: The invention provides a carbon nanotube compound and method for producing the same. The method of the invention comprises the following steps. Firstly, Aniline-trimer and DMAc (dimethyl acetamide) solution are mixed to form a first solution. Secondly, Dianhydride and DMAc solution are mixed to form a second solution. The first solution and the second are mixed to form a third solution. Additionally, carboxyl-multiwall carbon nanotubes (c-MWNT), Diaminodiphenylether and DMAc solution are mixed to form a fourth solution. The third solution and the fourth are mixed to form a polyamic acid/CNT solution. Some polyamic acid/CNT solution is spread on a substrate and processed by a thermal treatment, and a carbon nanotube compound is eventually produced.
Abstract translation: 本发明提供一种碳纳米管化合物及其制造方法。 本发明的方法包括以下步骤。 首先,将苯胺 - 三聚体和DMAc(二甲基乙酰胺)溶液混合以形成第一溶液。 其次,将二酐和DMAc溶液混合以形成第二溶液。 将第一溶液和第二溶液混合以形成第三溶液。 另外,将羧基 - 多壁碳纳米管(c-MWNT),二氨基二苯醚和DMAc溶液混合以形成第四溶液。 将第三溶液和第四溶液混合以形成聚酰胺酸/ CNT溶液。 将一些聚酰胺酸/ CNT溶液涂布在基材上,通过热处理进行处理,最终生成碳纳米管化合物。
-