Reel-to-reel passivation of stainless steel wire
    1.
    发明授权
    Reel-to-reel passivation of stainless steel wire 失效
    卷对卷钝化不锈钢丝

    公开(公告)号:US5607520A

    公开(公告)日:1997-03-04

    申请号:US516858

    申请日:1995-08-18

    Inventor: David G. Tipton

    CPC classification number: C25D11/34

    Abstract: A method and apparatus for performing continuous reel-to-reel passivation of a stainless steel wire usable in an underwater electromechanical or optical cable of a mine hunting sonar or similar marine system, which supplies the stainless steel wire, under tension, immerses a first portion of the stainless steel wire in 10-20% nitric acid bath at ambient temperature; applies a current from a DC power supply to the immersed first portion of the stainless steel wire, advances the stainless steel wire, under tension, to repeat the immersing and current supplying on a second portion of the stainless steel wire, washes the first portion of the stainless steel wire in a flowing water wash, dries the first portion of the stainless steel wire with forced air, advances the stainless steel wire, under tension, to repeat the washing and drying on the second portion of the stainless steel wire, and stores the stainless steel wire under tension.

    Abstract translation: 一种用于执行不可拉制的不锈钢丝的方法和装置,该不锈钢丝可用于在张力下供应不锈钢丝的地雷狩猎声纳或类似海洋系统的水下机电或光缆中浸入第一部分 的不锈钢丝在环境温度为10-20%的硝酸浴中; 将来自直流电源的电流施加到不锈钢丝的浸没的第一部分,使不锈钢丝在张力下前进,以在不锈钢丝的第二部分上重复浸渍和电流供应,将第一部分 不锈钢丝在流水洗涤中,用强制空气干燥不锈钢丝的第一部分,在张力下使不锈钢丝前进,重复不锈钢丝的第二部分的洗涤和干燥,并存储 不锈钢丝在张力下。

    Hiscor alloy
    2.
    发明授权
    Hiscor alloy 失效
    希科合金

    公开(公告)号:US4784831A

    公开(公告)日:1988-11-15

    申请号:US892937

    申请日:1986-08-04

    CPC classification number: C22C30/00

    Abstract: A highly carburization resistant alloy characterized by good structural stability at elevated temperatures and other desired properties, the alloy containing correlated percentages of iron, nickel, chromium, molybdenum, carbon, titanium, etc.

    Abstract translation: 一种高耐渗碳合金,其特征在于在高温下具有良好的结构稳定性和其它所需性能,该合金含铁,镍,铬,钼,碳,钛等相关百分比。

    Method of dissimilar metal attachment to ship hulls
    3.
    发明授权
    Method of dissimilar metal attachment to ship hulls 失效
    不同金属附着在船体上的方法

    公开(公告)号:US5782194A

    公开(公告)日:1998-07-21

    申请号:US745983

    申请日:1996-11-08

    Inventor: David G. Tipton

    Abstract: A bimetallic hull mount assembly (10) for reducing galvanic corrosion of a hull (12), including a foundation (14), made of a first material, welded to the hull (12), also made of the first material; and an insert (16), made of a second material, different from the first material, welded to the foundation (14); wherein a weld area (15) between the insert (16) and the foundation (14) is covered with paint (19), and where the insert (16) is welded to the foundation (14) in a controlled welding manufacturing environment, utilizing high performance dissimilar welding techniques to produce a dissimilar metal weld and the foundation (14) is welded to the hull (12) with a standard shipyard weld.

    Abstract translation: 一种用于减少船体(12)的电偶腐蚀的双金属船体安装组件(10),其包括由第一材料制成的基座(14),焊接到船体(12),其也由第一材料制成; 以及焊接到所述基座(14)上的与所述第一材料不同的第二材料制成的插入件(16)。 其特征在于,所述插入件(16)和所述基座(14)之间的焊接区域(15)被涂料(19)覆盖,并且在受控焊接制造环境中将所述插入件(16)焊接到所述基座(14) 产生不同金属焊接的高性能不同的焊接技术,并且基础(14)用标准船厂焊接焊接到船体(12)。

    Heat resistant low expansion alloy
    4.
    发明授权
    Heat resistant low expansion alloy 失效
    耐热低膨胀合金

    公开(公告)号:US4200459A

    公开(公告)日:1980-04-29

    申请号:US860298

    申请日:1977-12-14

    CPC classification number: C22C19/05 C22C19/007 C22C38/105

    Abstract: Nickel-iron base alloy characterized by controlled thermal expansion coefficient and inflection temperature and by desirable high strength in age-hardened condition has composition specially restricted to overcome detrimental sensitivity to stress-concentrating geometries and aid resistance to long-enduring stress in heated oxidizing atmospheres. The alloy contains, by weight, 34% to 55.3% nickel, up to 25.2% cobalt, 1% to 2% titanium, 1.5% to 5.5% of columbium plus 1/2 the weight percent of any tantalum, up to 1% chromium, not more than 0.2% aluminum and the balance essentially iron.

    Abstract translation: 镍 - 铁基合金的特征在于受控的热膨胀系数和拐点温度以及在老化硬化条件下所需的高强度,其组成特别受到限制,以克服对应力集中几何的有害敏感性,并有助于耐受热氧化气氛中长时间的应力。 该合金含有重量百分比为34%至55.3%的镍,至多25.2%的钴,1%至2%的钛,1.5%至5.5%的铌加上1/2的任何钽的重量百分比,至多1%的铬 ,不超过0.2%的铝和余量基本上是铁。