公开(公告)号:US5501807A
公开(公告)日:1996-03-26
申请号:US211777
申请日:1994-07-12
Applicant: Rainer Benda , Edouard M. Mathieu , Olivier Letailleur
Inventor: Rainer Benda , Edouard M. Mathieu , Olivier Letailleur
IPC: C07C51/41 , C09D5/08 , C09D7/12 , C10L1/30 , C10M159/20 , C10N10/04 , C10N30/04 , C10N30/06 , C10N30/10 , C10N30/12 , C10N40/20 , C10N70/00
CPC classification number: C10M159/20 , C07C51/414
Abstract: High basicity calcium carboxylates useful as lubricant and fuel additives and in paints are obtained by carbonating a mixture of a C.sub.7 to C.sub.15 carboxylic preferably branched chain oxo-acid and excess calcium at from 15.degree. to 60.degree. C. in the presence of a volatile solvent. Products with a basicity of from 4 to 8 may be obtained.
Abstract translation: 用作润滑剂和燃料添加剂的高碱度羧酸钙和涂料是通过在挥发性溶剂存在下,将C 15 -C 15羧酸优选支链含氧酸和过量的钙的混合物在15至60℃下进行碳酸化 。 碱度为4〜8的产品可以获得。
-
公开(公告)号:US5283276A
公开(公告)日:1994-02-01
申请号:US778855
申请日:1992-02-19
Applicant: Robert D. M. Best , Pierre H. Fillastre , Edouard M. Mathieu
Inventor: Robert D. M. Best , Pierre H. Fillastre , Edouard M. Mathieu
IPC: C08K5/42 , C07C303/32 , C07C309/31 , C07G99/00 , C08K5/41 , C08L23/08 , C08L33/06 , C08L77/00 , C08L77/08 , C08L101/00 , C09D5/08 , C09D7/12 , C09D123/08 , C09D127/04 , C09D127/06 , C09D133/00 , C09D133/04 , C09D133/06 , C09D177/00 , C09D177/08 , C09D201/00 , C10M159/24 , C10N30/06 , C10N30/08 , C10N30/12 , C10N40/20 , C10N70/00 , C23F11/00
CPC classification number: C10M159/24 , C07G17/008 , C09D5/08
Abstract: A corrosion protection composition a dispersion or solution of (a) colloidal size amorphous overbased sulfonate, (b) solvent or plasticizer, and (c) polymeric material soluble in the solvent or compatible with the plasticizer is disclosed. The composition comprises at least about 70% solids, by weight, and the particle size if the colloidal overbased sulfonate is up to about 100 A. Preferably, the composition is free from any mineral oil. Metal surfaces having the herein disclosed composition applied thereto, or having the applied thereto the composition from which the solvent has been removed also is disclosed.
Abstract translation: PCT No.PCT / GB90 / 00978 Sec。 371日期:1992年2月19日 102(e)日期1992年2月19日PCT提交1990年6月25日PCT公布。 第WO91 / 00319号公报 1991年1月10日,1991年1月10日公开了一种抗腐蚀组合物,(a)胶体尺寸无定形高碱性磺酸盐,(b)溶剂或增塑剂的分散体或溶液,和(c)可溶于溶剂或与增塑剂相容的聚合材料。 组合物包含至少约70重量%的固体,如果胶体高碱性磺酸盐高达约100A,则其粒径。优选地,组合物不含任何矿物油。 本发明公开的组合物的金属表面被施加到其上,或者已经向其施加已除去溶剂的组合物。
-