    摘要: A composite material for a lateral rigid member of a track belt for use in a snowmobile. A glycidylamine epoxy resin that is a polyfunctional epoxy thermosetting resin and has a molecular weight of about 250 to 1000 is included in an amount of 100 parts by weight. A 2-functional epoxy resin having a molecular weight of about 100 to 600 is included in an amount of 12 to 14.5 parts by weight. An aromatic polycarbonate thermoplastic resin having a molecular weight of about 12000 to 80000, a glass transition point of 130.degree. C. or more, a melting point of 220.degree. C. to 240.degree. C. is included in an amount of 5 to 45 parts by weight. An acid anhydride curing agent is included in an amount of 90 to 130 parts by weight. The composite material also includes reinforcing fiber.

    摘要翻译: 一种用于雪地车辆的轨道带的侧向刚性构件的复合材料。 作为多官能环氧热固性树脂的分子量为约250〜1000的缩水甘油胺环氧树脂的含量为100重量份。 分子量为约100〜600的2官能环氧树脂的含量为12〜14.5重量份。 分子量为约12000〜80000,玻璃化转变温度为130℃以上,熔点为220〜240℃的芳族聚碳酸酯热塑性树脂的含量为5〜45份 重量。 酸酐固化剂的含量为90〜130重量份。 复合材料还包括增强纤维。