1.
公开(公告)号:US20120114516A1
公开(公告)日:2012-05-10
申请号:US13292132
申请日:2011-11-09
申请人: Jörg HACHENBERG , Rudi STEINKE , Markus VOLLMANN , Irmgard WISSEL , Gerhard ZELLMANN , Elmar HOCK , Stefan FECHER , Lothar VOLKL
发明人: Jörg HACHENBERG , Rudi STEINKE , Markus VOLLMANN , Irmgard WISSEL , Gerhard ZELLMANN , Elmar HOCK , Stefan FECHER , Lothar VOLKL
CPC分类号: A61C13/0022 , A61K6/04 , B22F3/02 , B22F3/1021 , B22F3/11 , B22F3/16 , B22F3/24 , B22F2003/247 , B22F2003/248 , B22F2301/15 , C22C19/05 , C22C19/053 , C22C19/055 , C22C19/07
摘要: A method for manufacturing a shaped body, comprising creating a mixture of a metal powder and binding agent, compacting the mixture to form a green compact, heating the green compact to a debinding start temperature T1, debinding the green compact by controlled heating of the green compact from start temperature T1 to end temperature T2 at a heat-up rate R1, presintering the debindered green compact to the presinter end temperature TVS at a heat-up rate RHVS, cooling the green compact from the presinter end temperature TVS at a cool-down rate RKVS, whereby at least the heat-up rate RHVS, the presinter end temperature TVS, and the cool-down rate RKVS are tuned relative to each other in such a way that the presintered green compact forming a blank has a surface porosity of 16% to 22% after presintering, and machining and sintering of the blank to form the shaped body.
摘要翻译: 一种成型体的制造方法,其特征在于,制造金属粉末和粘合剂的混合物,压制混合物以形成生坯,将生坯压坯加热至脱脂开始温度T1,通过控制加热绿色坯料脱模生坯 以加热速率R1从起始温度T1到结束温度T2压缩,以加热速率RHVS预先烧结脱粘的绿色压坯到预端温度TVS,在冷端温度下将生坯从预端温度TVS冷却, 降低速率RKVS,由此至少使加热速率RHVS,预端温度TVS和冷却速率RKVS相对于彼此调节,使得形成坯料的预烧结压坯具有表面孔隙率 预烧结后为16%〜22%,加工和烧结坯料以形成成型体。
-
2.
公开(公告)号:US09393088B2
公开(公告)日:2016-07-19
申请号:US13292132
申请日:2011-11-09
申请人: Jörg Hachenberg , Rudi Steinke , Markus Vollmann , Irmgard Wissel , Gerhard Zellmann , Elmar Hock , Stefan Fecher , Lothar Volkl
发明人: Jörg Hachenberg , Rudi Steinke , Markus Vollmann , Irmgard Wissel , Gerhard Zellmann , Elmar Hock , Stefan Fecher , Lothar Volkl
CPC分类号: A61C13/0022 , A61K6/04 , B22F3/02 , B22F3/1021 , B22F3/11 , B22F3/16 , B22F3/24 , B22F2003/247 , B22F2003/248 , B22F2301/15 , C22C19/05 , C22C19/053 , C22C19/055 , C22C19/07
摘要: A method for manufacturing a shaped body, comprising creating a mixture of a metal powder and binding agent, compacting the mixture to form a green compact, heating the green compact to a debinding start temperature T1, debinding the green compact by controlled heating of the green compact from start temperature T1 to end temperature T2 at a heat-up rate R1, presintering the debindered green compact to the presinter end temperature TVS at a heat-up rate RHVS, cooling the green compact from the presinter end temperature TVS at a cool-down rate RKVS, whereby at least the heat-up rate RHVS, the presinter end temperature TVS, and the cool-down rate RKVS are tuned relative to each other in such a way that the presintered green compact forming a blank has a surface porosity of 16% to 22% after presintering, and machining and sintering of the blank to form the shaped body.
摘要翻译: 一种成型体的制造方法,其特征在于,制造金属粉末和粘合剂的混合物,压制混合物以形成生坯,将生坯压坯加热至脱脂开始温度T1,通过控制加热绿色坯料脱模生坯 以加热速率R1从起始温度T1到结束温度T2压缩,以加热速率RHVS预先烧结脱粘的绿色压坯到预端温度TVS,在冷端温度下将生坯从预端温度TVS冷却, 降低速率RKVS,由此至少使加热速率RHVS,预端温度TVS和冷却速率RKVS相对于彼此调节,使得形成坯料的预烧结压坯具有表面孔隙率 预烧结后为16%〜22%,加工和烧结坯料以形成成型体。
-