COATING METHOD, COATER, AND METHOD FOR MANUFACTURING PLANOGRAPHIC PRINTING PLATE
    1.
    发明申请
    COATING METHOD, COATER, AND METHOD FOR MANUFACTURING PLANOGRAPHIC PRINTING PLATE 有权
    涂料方法,涂料和制造平版印刷板的方法

    公开(公告)号:US20100247759A1

    公开(公告)日:2010-09-30

    申请号:US12750238

    申请日:2010-03-30

    IPC分类号: B05D5/06 B05D3/00 B05C1/00

    摘要: A coating method of forming a plurality of layers on a belt-like support continuously traveling, comprising: a step of applying a first coating liquid onto a front surface of the support to form a lower layer on the support; a drying step of removing a solvent in the lower layer until an amount of the residual solvent reaches not more than 100 mg/m2; a step of applying a second coating liquid onto the lower layer after drying to form an upper layer; and a drying step of removing moisture of the upper layer; wherein the drying step of removing moisture of the upper layer comprises: a first drying step of removing moisture in the upper layer until a moisture content of the upper layer reaches not more than 10% of moisture at the time of application within a range in which a following conditional expression (1) is satisfied: (1) temperature (Tw) of the support≦average softening temperature (T0) of the lower layer+10° C.; and a second drying step of raising the temperature (Tw) of the support to remove remaining moisture of the upper layer.

    摘要翻译: 一种在连续行进的带状载体上形成多个层的涂布方法,包括:将第一涂布液施加到载体的前表面上以在载体上形成下层的步骤; 干燥步骤,除去下层的溶剂直到残留溶剂的量达到不超过100mg / m 2; 干燥后将第二涂布液涂布在下层上形成上层的工序; 和去除上层水分的干燥步骤; 其中去除上层的水分的干燥步骤包括:第一干燥步骤,除去上层中的水分,直到上层的水分含量在施用时达到不超过10%的水分,其范围为 满足以下条件表达式(1):(1)载体的温度(Tw)<下层的平均软化温度(T0)+ 10℃; 以及第二干燥步骤,用于提高载体的温度(Tw)以除去上层的剩余水分。

    Coating device and coating method
    2.
    发明授权
    Coating device and coating method 失效
    涂布装置和涂布方法

    公开(公告)号:US07048969B2

    公开(公告)日:2006-05-23

    申请号:US10254842

    申请日:2002-09-26

    IPC分类号: B05D1/28 B05D1/40 B05C11/02

    摘要: A coating device and a coating method are provided. The coating device comprises a coating station for coating a coating liquid on a band-shaped substrate running continuously, and a coat-adjusting station disposed downstream of the coating station for adjusting the coating liquid on the substrate so that the coating liquid layer is coated on the substrate at a predetermined thickness. The coating station and the coat-adjusting station comprise first and second bars for respectively coating and measuring the liquid agent. The coating liquid can be coated on evenly and in a stable manner even if the coating operation is performed with the substrate running at a high speed.

    摘要翻译: 提供涂布装置和涂布方法。 所述涂布装置包括:涂布台,用于在连续运行的带状基材上涂布涂布液;以及涂布调整台,设置在所述涂布台的下游,用于调节所述基材上的涂布液,使得所述涂布液层涂布在 基板以预定的厚度。 涂覆站和涂层调整站包括用于分别涂布和测量液体试剂的第一和第二条。 即使在基板高速运转的情况下进行涂布操作,也可以均匀地且均匀地涂布涂布液。

    Coating method, coater, and method for manufacturing planographic printing plate
    3.
    发明授权
    Coating method, coater, and method for manufacturing planographic printing plate 有权
    涂布方法,涂布机和制造平版印刷版的方法

    公开(公告)号:US08445069B2

    公开(公告)日:2013-05-21

    申请号:US12750238

    申请日:2010-03-30

    IPC分类号: B05D3/02

    摘要: A coating method of forming a plurality of layers on a belt-like support continuously traveling, comprising: a step of applying a first coating liquid onto a front surface of the support to form a lower layer on the support; a drying step of removing a solvent in the lower layer until an amount of the residual solvent reaches not more than 100 mg/m2; a step of applying a second coating liquid onto the lower layer after drying to form an upper layer; and a drying step of removing moisture of the upper layer; wherein the drying step of removing moisture of the upper layer comprises: a first drying step of removing moisture in the upper layer until a moisture content of the upper layer reaches not more than 10% of moisture at the time of application within a range in which a following conditional expression (1) is satisfied: (1) temperature (Tw) of the support≦average softening temperature (T0) of the lower layer+10° C.; and a second drying step of raising the temperature (Tw) of the support to remove remaining moisture of the upper layer.

    摘要翻译: 一种在连续行进的带状载体上形成多个层的涂布方法,包括:将第一涂布液施加到载体的前表面上以在载体上形成下层的步骤; 干燥步骤,除去下层的溶剂直到残留溶剂的量达到不超过100mg / m 2; 干燥后将第二涂布液涂布在下层上形成上层的工序; 和去除上层水分的干燥步骤; 其中去除上层的水分的干燥步骤包括:第一干燥步骤,除去上层中的水分,直到上层的水分含量在施用时达到不超过10%的水分,其范围为 满足以下条件表达式(1):(1)下层+ 10℃的载体平均软化温度(T0)的温度(Tw)。 以及第二干燥步骤,用于提高载体的温度(Tw)以除去上层的剩余水分。

    Bar coating apparatus and bar coating method
    4.
    发明授权
    Bar coating apparatus and bar coating method 有权
    棒涂装置和棒涂法

    公开(公告)号:US06815008B2

    公开(公告)日:2004-11-09

    申请号:US10241612

    申请日:2002-09-12

    IPC分类号: B05D128

    摘要: A bar coating apparatus includes a coating bar for contacting an object to be coated, which object is conveyed in a constant direction, so as to apply a coating solution to and remove excess coating solution from the object to be coated, a weir member for forming a bead of the coating solution between the object to be coated and the coating bar, the weir member being disposed upstream of the coating bar in a direction in which the object to be coated is conveyed, a pressing member for pressing the object to be coated from a side thereof opposite from the coating bar, the pressing member being disposed near the coating bar; and a moving device for moving the pressing member in a thickness direction of the object to be coated.