Non-heat treated rolled steel and drawn wire rod with excellent toughness, and method for manufacturing the same
    1.
    发明授权
    Non-heat treated rolled steel and drawn wire rod with excellent toughness, and method for manufacturing the same 有权
    非热处理轧制钢和韧性优良的拉丝线材及其制造方法

    公开(公告)号:US08715429B2

    公开(公告)日:2014-05-06

    申请号:US13384779

    申请日:2010-08-04

    Abstract: There is provided a rolled steel with excellent toughness, a drawn wire rod prepared by drawing the rolled steel, and a method for manufacturing the same, in which even if a heating step is omitted, the toughness of the steel can be improved by securing a degenerated pearlite structure in an internal structure of the rolled steel by controlling a content of Mn among components and cooling conditions, and then preventing C diffusion. The rolled steel according to the present invention includes C: 0.15˜0.30%, Si: 0.1˜0.2%, Mn: 1.8˜3.0%, P: 0.035% or less, S: 0.040% or less, the remainder Fe, and other inevitable impurites, as a percentage of weight, in which the microstucture of the rolled steel is composed of ferrite and pearlite including cementite with 150 nm or less of thickness.

    Abstract translation: 提供具有优异韧性的轧制钢,通过拉制轧制钢制备的拉丝线及其制造方法,其中即使省略加热步骤,也可以通过确保钢的韧性来提高钢的韧性 通过控制成分中的Mn含量和冷却条件,然后防止C扩散,在轧制钢的内部结构中退化珠光体组织。 根据本发明的轧制钢包括C:0.15〜0.30%,Si:0.1〜0.2%,Mn:1.8〜3.0%,P:0.035%以下,S:0.040%以下,剩余部分Fe等 不可避免的杂质占重量的百分比,其中轧制钢的组织由铁素体和珠光体组成,包括厚度在150nm以下的渗碳体。

    NON-HEAT TREATED ROLLED STEEL AND DRAWN WIRE ROD WITH EXCELLENT TOUGHNESS, AND METHOD FOR MANUFACTURING THE SAME
    2.
    发明申请
    NON-HEAT TREATED ROLLED STEEL AND DRAWN WIRE ROD WITH EXCELLENT TOUGHNESS, AND METHOD FOR MANUFACTURING THE SAME 有权
    具有优异韧性的非热处理的轧制钢丝和拉丝线及其制造方法

    公开(公告)号:US20120118443A1

    公开(公告)日:2012-05-17

    申请号:US13384779

    申请日:2010-08-04

    Abstract: There is provided a rolled steel with excellent toughness, a drawn wire rod prepared by drawing the rolled steel, and a method for manufacturing the same, in which even if a heating step is omitted, the toughness of the steel can be improved by securing a degenerated pearlite structure in an internal structure of the rolled steel by controlling a content of Mn among components and cooling conditions, and then preventing C diffusion. The rolled steel according to the present invention includes C: 0.15˜0.30%, Si: 0.1˜0.2%, Mn: 1.8˜3.0%, P: 0.035% or less, S: 0.040% or less, the remainder Fe, and other inevitable impurites, as a percentage of weight, in which the microstucture of the rolled steel is composed of ferrite and pearlite including cementite with 150 nm or less of thickness.

    Abstract translation: 提供具有优异韧性的轧制钢,通过拉制轧制钢制备的拉丝线及其制造方法,其中即使省略加热步骤,也可以通过确保钢的韧性来提高钢的韧性 通过控制成分中的Mn含量和冷却条件,然后防止C扩散,在轧制钢的内部结构中退化珠光体组织。 根据本发明的轧制钢包括C:0.15〜0.30%,Si:0.1〜0.2%,Mn:1.8〜3.0%,P:0.035%以下,S:0.040%以下,剩余部分Fe等 不可避免的杂质占重量的百分比,其中轧制钢的组织由铁素体和珠光体组成,包括厚度在150nm以下的渗碳体。