公开(公告)号:US4915885A
公开(公告)日:1990-04-10
申请号:US210261
申请日:1988-06-23
CPC分类号: C08J5/18 , B29C55/005 , C08L67/02 , B29C2071/022 , B29C71/02 , B29K2067/00 , C08J2367/02
摘要: A process of preparing a homogeneous amorphous polymeric blend of polyethyleneterephthalate (PET) and polybutyleneterephthalate (PBT) which includes intimately mixing the PET and PBT at a weight ratio of about 10:90-90:10, melting the mixture at 290.degree.-330.degree. C., cooling the mixture to 0.degree.--194.degree. C. by extruding it onto rollers maintained in a cooling bath and orienting the polymer of the resulting continuous shaped object at room temperature to a draw ratio of about 5:1, with subsequent annealing at about 120.degree.-180.degree. C. for about one hour.