Nanoparticle synthesis by solvothermal process
    4.
    发明授权
    Nanoparticle synthesis by solvothermal process 有权
    通过溶剂热法合成纳米颗粒

    公开(公告)号:US07959885B2

    公开(公告)日:2011-06-14

    申请号:US12032590

    申请日:2008-02-15

    IPC分类号: C01F13/00

    摘要: A solvothermal process for making inorganic nanoparticles is described. Inorganic nanoparticles can be produced by forming a suspension or solution comprising at least one group II-IV and lanthanide metal inorganic salt in a first medium, disposing the suspension or solution in a sealed chamber having an interior pressure, elevating the interior pressure of the sealed chamber to an initial interior pressure prior to the heating, heating the suspension or solution to a peak temperature higher than the normal boiling point of the first medium, optionally adding a second medium to the suspension or solution after the heating.

    摘要翻译: 描述了制备无机纳米颗粒的溶剂热法。 可以通过在第一介质中形成包含至少一种II-IV族和镧系元素金属无机盐的悬浮液或溶液来制备无机纳米颗粒,将悬浮液或溶液设置在具有内部压力的密封室中,提高密封的内部压力 在加热之前,将悬浮液或溶液加热到高于第一介质的标准沸点的峰值温度,任选地在加热后向悬浮液或溶液中加入第二种介质。

    NANOPARTICLE SYNTHESIS BY SOLVOTHERMAL PROCESS
    8.
    发明申请
    NANOPARTICLE SYNTHESIS BY SOLVOTHERMAL PROCESS 有权
    通过SOLVOTHERMAL过程的纳米级合成

    公开(公告)号:US20090208398A1

    公开(公告)日:2009-08-20

    申请号:US12032590

    申请日:2008-02-15

    IPC分类号: C01F17/00

    摘要: A solvothermal process for making inorganic nanoparticles is described. Inorganic nanoparticles can be produced by forming a suspension or solution comprising at least one group II-IV and lanthanide metal inorganic salt in a first medium, disposing the suspension or solution in a sealed chamber having an interior pressure, elevating the interior pressure of the sealed chamber to an initial interior pressure prior to the heating, heating the suspension or solution to a peak temperature higher than the normal boiling point of the first medium, optionally adding a second medium to the suspension or solution after the heating.

    摘要翻译: 描述了制备无机纳米颗粒的溶剂热法。 可以通过在第一介质中形成包含至少一种II-IV族和镧系元素金属无机盐的悬浮液或溶液来制备无机纳米颗粒,将悬浮液或溶液设置在具有内部压力的密封室中,提高密封的内部压力 在加热之前,将悬浮液或溶液加热到高于第一介质的标准沸点的峰值温度,任选地在加热后向悬浮液或溶液中加入第二种介质。