公开(公告)号:US08101535B2
公开(公告)日:2012-01-24
申请号:US12019348
申请日:2008-01-24
IPC分类号: C04B35/573 , F41H5/00
CPC分类号: C04B35/573 , C04B35/6261 , C04B35/62828 , C04B35/62839 , C04B2235/3217 , C04B2235/3804 , C04B2235/3813 , C04B2235/3821 , C04B2235/3826 , C04B2235/425 , C04B2235/428 , C04B2235/5436 , C04B2235/6027 , C04B2235/6581 , C04B2235/80
摘要: A ceramic ballistic material and method of manufacture is disclosed. A filler material is provided. The filler material is divided into filler granules collectively having a median diameter approximately 10 microns or less. An amount of carbon is provided. The carbon is divided into carbon particles and the carbon particles are allowed to coat the filler granules. The mixture of carbon-coated filler granules is formed into a ballistic armor shape. The formed mixture is placed in a substantial vacuum. The mixture is introduced to a pre-selected amount of silicon and the mixture of carbon-coated filler granules and silicon is heated to a temperature at or above the melting point of the silicon.
摘要翻译: 公开了一种陶瓷弹道材料及其制造方法。 提供填充材料。 填充材料被分成一个共同具有大约10微米或更小的中值直径的填料颗粒。 提供了一定量的碳。 将碳分成碳颗粒,并且使碳颗粒涂覆填料颗粒。 碳涂覆的填料颗粒的混合物形成为防弹装甲形状。 将形成的混合物置于基本真空中。 将混合物引入预选量的硅中,将碳涂覆的填料颗粒和硅的混合物加热至等于或高于硅熔点的温度。
-
公开(公告)号:US20080145293A1
公开(公告)日:2008-06-19
申请号:US11957839
申请日:2007-12-17
申请人: John Carberry , Jennifer Norwood , Katherine T. Leighton , Kyle Hoff , Carl Cline , Edgar L. Aleshire
发明人: John Carberry , Jennifer Norwood , Katherine T. Leighton , Kyle Hoff , Carl Cline , Edgar L. Aleshire
IPC分类号: C04B35/565 , B02C23/06 , C04B35/563
CPC分类号: C04B35/565 , C04B35/573 , C04B35/6261 , C04B35/62828 , C04B35/62839 , C04B2235/3217 , C04B2235/3804 , C04B2235/3813 , C04B2235/3821 , C04B2235/3826 , C04B2235/425 , C04B2235/5436 , C04B2235/6027 , C04B2235/6581 , C04B2235/80
摘要: A method for producing a ceramic material product. A filler material is provided. The filler material is divided into filler granules collectively having a median diameter approximately 10 microns or less. An amount of carbon is provided. The carbon is divided into carbon particles and the carbon particles are allowed to coat the filler granules. The mixture of carbon-coated filler granules is formed into a selected shape. The formed mixture is placed in a substantial vacuum. The mixture is introduced to a pre-selected amount of silicon and the mixture of carbon-coated filler granules and silicon is heated to a temperature at or above the melting point of the silicon.
摘要翻译: 陶瓷材料制品的制造方法。 提供填充材料。 填充材料被分成一个共同具有大约10微米或更小的中值直径的填料颗粒。 提供了一定量的碳。 将碳分成碳颗粒,并且使碳颗粒涂覆填料颗粒。 将碳涂覆的填料颗粒的混合物形成为选定的形状。 将形成的混合物置于基本真空中。 将混合物引入预选量的硅中,将碳涂覆的填料颗粒和硅的混合物加热至等于或高于硅熔点的温度。
-
公开(公告)号:US08262981B2
公开(公告)日:2012-09-11
申请号:US11957839
申请日:2007-12-17
申请人: John Carberry , Jennifer Norwood , Katherine T. Leighton , Kyle Hoff , Carl Cline , Edgar L. Aleshire
发明人: John Carberry , Jennifer Norwood , Katherine T. Leighton , Kyle Hoff , Carl Cline , Edgar L. Aleshire
IPC分类号: C04B35/83 , C04B35/563 , C04B35/567
CPC分类号: C04B35/565 , C04B35/573 , C04B35/6261 , C04B35/62828 , C04B35/62839 , C04B2235/3217 , C04B2235/3804 , C04B2235/3813 , C04B2235/3821 , C04B2235/3826 , C04B2235/425 , C04B2235/5436 , C04B2235/6027 , C04B2235/6581 , C04B2235/80
摘要: A method for producing a ceramic material product. A filler material is provided. The filler material is divided into filler granules collectively having a median diameter approximately 10 microns or less. An amount of carbon is provided. The carbon is divided into carbon particles and the carbon particles are allowed to coat the filler granules. The mixture of carbon-coated filler granules is formed into a selected shape. The formed mixture is placed in a substantial vacuum. The mixture is introduced to a pre-selected amount of silicon and the mixture of carbon-coated filler granules and silicon is heated to a temperature at or above the melting point of the silicon.
摘要翻译: 陶瓷材料制品的制造方法。 提供填充材料。 填充材料被分成一个共同具有大约10微米或更小的中值直径的填料颗粒。 提供了一定量的碳。 将碳分成碳颗粒,并且使碳颗粒涂覆填料颗粒。 将碳涂覆的填料颗粒的混合物形成为选定的形状。 将形成的混合物置于基本真空中。 将混合物引入预选量的硅中,将碳涂覆的填料颗粒和硅的混合物加热至等于或高于硅熔点的温度。
-
公开(公告)号:US20110314997A1
公开(公告)日:2011-12-29
申请号:US12019348
申请日:2008-01-24
IPC分类号: F41H5/02
CPC分类号: C04B35/573 , C04B35/6261 , C04B35/62828 , C04B35/62839 , C04B2235/3217 , C04B2235/3804 , C04B2235/3813 , C04B2235/3821 , C04B2235/3826 , C04B2235/425 , C04B2235/428 , C04B2235/5436 , C04B2235/6027 , C04B2235/6581 , C04B2235/80
摘要: A ceramic ballistic material and method of manufacture is disclosed. A filler material is provided. The filler material is divided into filler granules collectively having a median diameter approximately 10 microns or less. An amount of carbon is provided. The carbon is divided into carbon particles and the carbon particles are allowed to coat the filler granules. The mixture of carbon-coated filler granules is formed into a ballistic armor shape. The formed mixture is placed in a substantial vacuum. The mixture is introduced to a pre-selected amount of silicon and the mixture of carbon-coated filler granules and silicon is heated to a temperature at or above the melting point of the silicon.
摘要翻译: 公开了一种陶瓷弹道材料及其制造方法。 提供填充材料。 填充材料被分成一个共同具有大约10微米或更小的中值直径的填料颗粒。 提供了一定量的碳。 将碳分成碳颗粒,并且使碳颗粒涂覆填料颗粒。 碳涂覆的填料颗粒的混合物形成为防弹装甲形状。 将形成的混合物置于基本真空中。 将混合物引入预选量的硅中,将碳涂覆的填料颗粒和硅的混合物加热至等于或高于硅熔点的温度。
-
-
-