公开(公告)号:US08231757B2
公开(公告)日:2012-07-31
申请号:US12739014
申请日:2008-01-24
申请人: Hai Lin , Xufeng Xu , Jiuhong Jin , Hongzheng Liu
发明人: Hai Lin , Xufeng Xu , Jiuhong Jin , Hongzheng Liu
CPC分类号: B27J1/003 , B27M3/006 , B32B7/12 , B32B9/02 , B32B2307/54 , B32B2307/72 , Y10T156/1052 , Y10T156/1056 , Y10T156/1057 , Y10T156/1062 , Y10T156/1067
摘要: A method of manufacturing laminated bamboo sliver lumber comprises steps of: preparing bamboo slivers; performing moth-proofing, mildew-proofing, and antiseptic treatments to the bamboo slivers and then drying the bamboo slivers to a moisture content of about 6-15%; machining each dried bamboo sliver to a thickness of about 0.5-3.5 mm (0.02-0.14 in) and a width of about 5-22 mm (0.20-0.87 in) and then dehumidifying the machined bamboo slivers to a moisture content of about 3-10%; applying a glue to the bamboo slivers by glue-coating or “immerging” process, in which a ratio of the glue to an absolute dry weight of the bamboo slivers is about 3-16%; and arranging the glued bamboo slivers with their “width” direction consistent with the “vertical” direction and then pressing the arranged bamboo slivers and curing the glue under a “side” pressure of about 3-15 MPa (0.44-2.18 ksi) and a “top” pressure of about 1-6 MPa (0.15-0.87 ksi) so as to form the laminated bamboo sliver lumber.
摘要翻译: 层压竹条木材的制造方法,包括:制作竹条; 对竹条进行防虫,防霉,防腐处理,然后将竹条干燥至含水量约6-15%; 将每根干燥的竹条加工成约0.5-3.5毫米(0.02-0.14英寸)的厚度和约5-22毫米(0.20-0.87英寸)的宽度,然后将机加工的竹条除湿至约3- 10%; 通过胶水涂布或“浸泡”工艺将竹胶条施加在竹条上,其中胶条与竹条绝对干重的比例约为3-16%; 并按照“垂直”方向将“竹宽”方向排列成“宽”方向,然后在排列的竹条上按压约3-15MPa(0.44-2.18ksi)的“侧”压力并固化胶 “顶部”压力约为1-6MPa(0.15-0.87ksi),以形成层压竹条。
-
2.
公开(公告)号:US20100258243A1
公开(公告)日:2010-10-14
申请号:US12739014
申请日:2008-01-24
申请人: Hai Lin , Xufeng Xu , Jiuhong Jin , Hongzheng Liu
发明人: Hai Lin , Xufeng Xu , Jiuhong Jin , Hongzheng Liu
IPC分类号: B32B38/04
CPC分类号: B27J1/003 , B27M3/006 , B32B7/12 , B32B9/02 , B32B2307/54 , B32B2307/72 , Y10T156/1052 , Y10T156/1056 , Y10T156/1057 , Y10T156/1062 , Y10T156/1067
摘要: A method of manufacturing laminated bamboo sliver lumber, comprising steps of: selecting and using the bamboo outer slivers obtained from a bamboo and having an air dry density no less than about 0.95 g/cm3 and removing siliceous and wax layers thereon to obtain bamboo slivers having a width of about 1-4 mm. Drying the bamboo slivers to a moisture content of about 6-15%, machining the dried bamboo slivers to a thickness of about 0.5-3.5 mm and a width of about 5-22 mm, then dehumidifying the bamboo slivers to a moisture content of about 3-10%. Applying a glue to the bamboo slivers in which a ratio of the glue to an absolute dry weight of the bamboo slivers may be about 3-16%. A arranging the glued bamboo slivers with their width direction consistent with the vertical direction, then pressing the arranged bamboo slivers and curing the glue under a side pressure of about 3-15 MPa and a top pressure of about 1-6 MPa.
摘要翻译: 一种制造层压竹条木材的方法,包括以下步骤:选择和使用从竹子获得的竹外条,空气干密度不小于约0.95g / cm 3,并且在其上除去硅质和蜡层以获得具有 宽度约1-4毫米。 将竹条干燥至约6-15%的水分含量,将干竹条加工至厚度约0.5-3.5毫米,宽度约5-22毫米,然后将竹条除湿至约含水量 3-10%。 在竹条上涂上胶水,其中胶条与竹条绝对干重的比值约为3-16%。 将宽度方向与垂直方向一致的胶布竹条布置,然后在排列的竹条上按压约3-15MPa的侧压,约1〜6MPa的顶压。
-