    摘要: A process for preparing grit blasting particles coated with titanium dioxide by sinter-fusing titanium dioxide on the surface of grit blasting particles made of a base material. A mixture of finely divided titanium dioxide and grit blasting particles is passed continuously through the flame in a flame reactor, with the aid of conveying air, wherein the titanium dioxide is sinter-fused on the surface of the grit blasting particles over an average residence time of 0.1 to 5 seconds in a temperature range from 600 to 1200° C. An increase in the adhesive bond between metal framework and a facing material made of plastics in dentures can be achieved when metal framework is grit blasted with a grit blasting agent containing titanium dioxide coated grit blasting particles and then the grit blasted and titanium dioxide coated surface is treated with a silane bonding agent.

    摘要翻译: 通过在由基材制成的喷砂颗粒的表面上烧结二氧化钛来制备用二氧化钛涂覆的喷砂颗粒的方法。 在火焰反应器中,借助于输送空气,将细碎的二氧化钛和喷砂颗粒的混合物连续通过火焰,其中二氧化钛在平均停留时间内烧结熔合在喷砂颗粒的表面上 在600至1200℃的温度范围内为0.1至5秒。当金属框架用含有钛的喷砂剂进行喷砂处理时,可以实现金属框架和由假牙塑料制成的面层材料之间的粘合剂粘结的增加 二氧化硅涂层喷砂颗粒,然后用硅烷粘合剂处理喷砂和二氧化钛涂层表面。