公开(公告)号:US09932705B2
公开(公告)日:2018-04-03
申请号:US13634672
申请日:2011-03-09
申请人: Gen Koide , Katsufumi Yanai
发明人: Gen Koide , Katsufumi Yanai
CPC分类号: D06N3/0004 , C08J9/0085 , C08J9/06 , C08J2205/044 , C08J2375/04 , D06N3/005 , D06N3/14 , D06N2205/023 , D06N2205/04 , D06N2205/243 , D06N2211/10 , D06N2211/14 , D06N2211/261 , D06N2211/28
摘要: Disclosed is a sheet-like material which is produced by an environmentally friendly procedure and has an elegant appearance with piloerection, good wear resistance and good texture. Specifically disclosed is a sheet-like material containing a water-dispersed polyurethane within a fibrous base that contains extra-fine fibers having an average single fiber diameter of 0.3-7 um. The inside of the water-dispersed polyurethane is provided with pores each having a diameter of 10-200 um. Also specifically disclosed is a method for producing a sheet-like material by applying a polyurethane liquid to a fibrous base, wherein the polyurethane liquid is a water-dispersed polyurethane liquid that contains a foaming agent and a dry film of the polyurethane that constitutes the polyurethane liquid has a 100% modulus of 3-8 MPa.
-
公开(公告)号:US09394630B2
公开(公告)日:2016-07-19
申请号:US13393710
申请日:2010-08-30
CPC分类号: D01F8/14 , D01F1/10 , D01F6/62 , D01F6/92 , D06N3/0004 , D06N3/0036 , D06N2211/28 , Y10T428/2395
摘要: An artificial leather is provided having a raised nap to give an elegant appearance, and further has a good pilling-resistance without affecting the spinning performance. The pilling-resistant artificial leather is a sheet-form object including a microfiber having a monofilament diameter of 0.3 to 10 μm and a polymeric elastomer, and having a raised nap made of the microfiber. The microfiber includes inorganic particles in a proportion of 0.01 to 5% by mass relative to 100% by mass of the microfiber, and a silicone oil in a proportion of 0.001 to 1% by mass relative to 100% by mass of the microfiber. The microfiber contains a polyester microfiber in a proportion of 90% by mass or more thereof.
摘要翻译: 提供具有凸起的绒毛以提供优雅的外观的人造革,并且还具有良好的起球抗性,而不影响纺丝性能。 起绒抗人造革是包括单丝直径为0.3〜10μm的超细纤维和高分子弹性体的片状物,具有由超细纤维制成的凸起绒毛。 超细纤维包含相对于超细纤维100质量%为0.01〜5质量%的无机粒子,相对于超细纤维100质量%为0.001〜1质量%的硅油。 超细纤维含有90质量%以上的聚酯超细纤维。
-
公开(公告)号:US20130005848A1
公开(公告)日:2013-01-03
申请号:US13634672
申请日:2011-03-09
申请人: Gen Koide , Katsufumi Yanai
发明人: Gen Koide , Katsufumi Yanai
CPC分类号: D06N3/0004 , C08J9/0085 , C08J9/06 , C08J2205/044 , C08J2375/04 , D06N3/005 , D06N3/14 , D06N2205/023 , D06N2205/04 , D06N2205/243 , D06N2211/10 , D06N2211/14 , D06N2211/261 , D06N2211/28
摘要: Disclosed is a sheet-like material which is produced by an environmentally friendly procedure and has an elegant appearance with piloerection, good wear resistance and good texture. Specifically disclosed is a sheet-like material containing a water-dispersed polyurethane within a fibrous base that contains extra-fine fibers having an average single fiber diameter of 0.3-7 um. The inside of the water-dispersed polyurethane is provided with pores each having a diameter of 10-200 um. Also specifically disclosed is a method for producing a sheet-like material by applying a polyurethane liquid to a fibrous base, wherein the polyurethane liquid is a water-dispersed polyurethane liquid that contains a foaming agent and a dry film of the polyurethane that constitutes the polyurethane liquid has a 100% modulus of 3-8 MPa.
摘要翻译: 公开了一种片状材料,其通过环境友好的方法制造,具有优雅的外观,具有良好的耐磨性和良好的质感。 具体公开了一种片状材料,其含有在纤维基体内的水分散性聚氨酯,其含有平均单纤维直径为0.3-7μm的超细纤维。 水分散聚氨酯的内部设有直径为10-200μm的孔。 还具体公开了一种通过将聚氨酯液体涂布在纤维基材上来制造片状材料的方法,其中聚氨酯液体是含有发泡剂的水分散聚氨酯液体和构成聚氨酯的聚氨酯的干膜 液体的100%模量为3-8MPa。
-
公开(公告)号:US20120156416A1
公开(公告)日:2012-06-21
申请号:US13393710
申请日:2010-08-30
IPC分类号: D06C11/00
CPC分类号: D01F8/14 , D01F1/10 , D01F6/62 , D01F6/92 , D06N3/0004 , D06N3/0036 , D06N2211/28 , Y10T428/2395
摘要: An artificial leather is provided having a raised nap to give an elegant appearance, and further has a good pilling-resistance without affecting the spinning performance. The pilling-resistant artificial leather is a sheet-form object including a microfiber having a monofilament diameter of 0.3 to 10 μm and a polymeric elastomer, and having a raised nap made of the microfiber. The microfiber includes inorganic particles in a proportion of 0.01 to 5% by mass relative to 100% by mass of the microfiber, and a silicone oil in a proportion of 0.001 to 1% by mass relative to 100% by mass of the microfiber. The microfiber contains a polyester microfiber in a proportion of 90% by mass or more thereof.
摘要翻译: 提供具有凸起的绒毛以提供优雅的外观的人造革,并且还具有良好的起球抗性,而不影响纺丝性能。 起绒抗人造革是包括单丝直径为0.3〜10μm的超细纤维和高分子弹性体的片状物,具有由超细纤维制成的凸起绒毛。 超细纤维包含相对于超细纤维100质量%为0.01〜5质量%的无机粒子,相对于超细纤维100质量%为0.001〜1质量%的硅油。 超细纤维含有90质量%以上的聚酯超细纤维。
-
-
-