Method for producing optical fiber having formyl groups on core surface
thereof
    1.
    发明授权
    Method for producing optical fiber having formyl groups on core surface thereof 失效
    在其芯表面上具有甲酰基的光纤的制造方法

    公开(公告)号:US5354574A

    公开(公告)日:1994-10-11

    申请号:US80615

    申请日:1993-06-22

    CPC分类号: G01N33/547 G01N33/545

    摘要: The present invention is directed to a method for producing an optical fiber having formyl groups on a core surface. In one embodiment, a plastic optical fiber having formyl groups on a core surface is obtained by immersing the core surface of the plastic optical fiber in a treating solution containing at least a 0.5 to 40 mM alkali metal hydroxide and a compound having formyl groups in water or lower alcohol solvent. In the other embodiment, a plastic optical fiber having formyl groups on a core surface is obtained by introducing a vic-diol group, a primary hydroxyl group or an alkenyl group on the core surface, and then oxidizing it. Turbidity on the core surface of the optical fiber thus obtained is minimized, thereby reducing the transmittance losses of light.

    摘要翻译: 本发明涉及一种在芯表面上制备具有甲酰基的光纤的方法。 在一个实施方案中,通过将塑料光纤的芯表面浸渍在含有至少0.5至40mM碱金属氢氧化物和在水中具有甲酰基的化合物的处理溶液中来获得在芯表面上具有甲酰基的塑料光纤 或低级醇溶剂。 在另一实施方式中,通过在芯表面上引入邻二醇基,伯羟基或烯基,然后将其氧化来获得在芯表面上具有甲酰基的塑料光纤。 由此获得的光纤的芯表面上的浊度最小化,从而降低光的透射率损失。