PROCESS FOR MANUFACTURING MODIFIED CONJUGATED DIENE POLYMER, COMPOSITION COMPRISING THE POLYMER, AND TIRE COMPRISING THE COMPOSITION
    1.
    发明申请
    PROCESS FOR MANUFACTURING MODIFIED CONJUGATED DIENE POLYMER, COMPOSITION COMPRISING THE POLYMER, AND TIRE COMPRISING THE COMPOSITION 有权
    制造改性共轭二烯聚合物的方法,包含聚合物的组合物和包含组合物的轮胎

    公开(公告)号:US20100210760A1

    公开(公告)日:2010-08-19

    申请号:US12593164

    申请日:2008-03-25

    IPC分类号: C08L9/00 C08F8/32 C08K3/04

    摘要: The present invention has an object to provide a conjugated diene-based polymer, subjected to a vulcanization treatment to make a vulcanized rubber, the vulcanized rubber useful as a material for tire treads excellent in the balance among wet skid characteristics, low hysteresis loss, abrasion resistance, breaking strength and rigidity, and to provide its manufacturing process. According to the present invention, there is provided the process for manufacturing a modified conjugated diene-based polymer having a modifying group in its molecule, the process including a step of obtaining a conjugated diene-based polymer by polymerizing a conjugated diene compound, or a conjugated diene compound and an aromatic vinyl compound, by using an alkaline metal-based initiator or an alkaline earth metal-based initiator in a hydrocarbon solvent, and a step of reacting active terminals of the polymer with a glycidylamino group-containing low molecular compound having two or more tertiary amino groups and three or more glycidyl groups bonded to the amino groups in a molecule of the compound, and an oligomer of a dimmer or more of the low molecular compound as modifying agents, wherein the reaction is performed using 75 to 95% by mass of the low molecular compound and 25 to 5% by mass of the oligomer based on the total amount of the modifying agents.

    摘要翻译: 本发明的目的是提供一种经硫化处理以制备硫化橡胶的共轭二烯系聚合物,硫化橡胶可用作轮胎胎面的材料,其湿滑特性之间的平衡优异,低滞后损失,磨损 电阻,断裂强度和刚性,并提供其制造工艺。 根据本发明,提供了在其分子中具有改性基团的改性共轭二烯系聚合物的制造方法,该方法包括通过使共轭二烯化合物聚合获得共轭二烯系聚合物的工序,或 共轭二烯化合物和芳香族乙烯基化合物,通过在烃溶剂中使用碱金属类引发剂或碱土金属类引发剂,以及使聚合物的活性末端与含缩水甘油基氨基的低分子化合物反应的步骤, 两个或更多个叔氨基和与化合物分子中的氨基键合的三个或更多个缩水甘油基,以及二聚体或更多个低分子化合物的低聚物作为改性剂,其中反应使用75至95 质量%的低分子化合物和25〜5质量%的低聚物,基于改性剂的总量。

    Process for manufacturing modified conjugated diene polymer, composition comprising the polymer, and tire comprising the composition
    2.
    发明授权
    Process for manufacturing modified conjugated diene polymer, composition comprising the polymer, and tire comprising the composition 有权
    制备改性共轭二烯聚合物的方法,包含聚合物的组合物和包含该组合物的轮胎

    公开(公告)号:US08278395B2

    公开(公告)日:2012-10-02

    申请号:US12593164

    申请日:2008-03-25

    IPC分类号: C08F8/32 C08F4/48 C08F236/10

    摘要: The present invention has an object to provide a conjugated diene-based polymer, subjected to a vulcanization treatment to make a vulcanized rubber, the vulcanized rubber useful as a material for tire treads excellent in the balance among wet skid characteristics, low hysteresis loss, abrasion resistance, breaking strength and rigidity, and to provide its manufacturing process. According to the present invention, there is provided the process for manufacturing a modified conjugated diene-based polymer having a modifying group in its molecule, the process including a step of obtaining a conjugated diene-based polymer by polymerizing a conjugated diene compound, or a conjugated diene compound and an aromatic vinyl compound, by using an alkaline metal-based initiator or an alkaline earth metal-based initiator in a hydrocarbon solvent, and a step of reacting active terminals of the polymer with a glycidylamino group-containing low molecular compound having two or more tertiary amino groups and three or more glycidyl groups bonded to the amino groups in a molecule of the compound, and an oligomer of a dimmer or more of the low molecular compound as modifying agents, wherein the reaction is performed using 75 to 95% by mass of the low molecular compound and 25 to 5% by mass of the oligomer based on the total amount of the modifying agents.

    摘要翻译: 本发明的目的是提供一种经硫化处理以制备硫化橡胶的共轭二烯系聚合物,硫化橡胶可用作轮胎胎面的材料,其湿滑特性之间的平衡优异,低滞后损失,磨损 电阻,断裂强度和刚性,并提供其制造工艺。 根据本发明,提供了在其分子中具有改性基团的改性共轭二烯系聚合物的制造方法,该方法包括通过使共轭二烯化合物聚合获得共轭二烯系聚合物的工序,或 共轭二烯化合物和芳香族乙烯基化合物,通过在烃溶剂中使用碱金属类引发剂或碱土金属类引发剂,以及使聚合物的活性末端与含缩水甘油基氨基的低分子化合物反应的步骤, 两个或更多个叔氨基和与化合物分子中的氨基键合的三个或更多个缩水甘油基,以及二聚体或更多个低分子化合物的低聚物作为改性剂,其中反应使用75至95 质量%的低分子化合物和25〜5质量%的低聚物,基于改性剂的总量。