Heat-accumulating heater
    1.
    发明申请
    Heat-accumulating heater 审中-公开
    蓄热式加热器

    公开(公告)号:US20090229593A1

    公开(公告)日:2009-09-17

    申请号:US12320473

    申请日:2009-01-27

    申请人: Kunihiko Komiya

    发明人: Kunihiko Komiya

    IPC分类号: F24J1/00

    摘要: A heat-accumulating heater includes a powdery paraffinic latent heat storage substance sealed in a bag-shaped container. The bag-shaped container includes a plurality of inner container members formed of sheets impermeable to the heat storage substance and water and permeable to air. The inner container members are each received in one of first substantially rectangular outer container members made of rubber that are connected to each other in a row so as to be bendable relative to each other. An air layer is present between each inner container member and the corresponding first outer container member, thereby preventing the inner container member from being pressed against the first outer container member. The first outer container members are in turn received in a second outer container member made of cloth.

    摘要翻译: 蓄热加热器包括密封在袋形容器中的粉状石蜡潜热储存物质。 袋形容器包括多个内部容器构件,该内部容器构件由不可渗透储热物质的片材和水形成并且可渗透空气。 内部容器构件分别容纳在彼此相对连接的第一大致矩形的由橡胶制成的外部容器构件中,以便能相对于彼此弯曲。 在每个内部容器构件和相应的第一外部容器构件之间存在空气层,从而防止内部容器构件被压靠在第一外部容器构件上。 第一外部容器构件又被容纳在由布制成的第二外部容器构件中。

    Ink occlusion material for writing utensils
    5.
    发明授权
    Ink occlusion material for writing utensils 失效
    用于书写用具的油墨封闭材料

    公开(公告)号:US5169467A

    公开(公告)日:1992-12-08

    申请号:US569949

    申请日:1990-09-27

    IPC分类号: B43K1/12 B43K5/02 B43K8/03

    摘要: According to the present invention, the ink occlusion material for writing utensils comprises a fiber bundle of a mixture of (a) and acrylic synthetic fiber and (b) at least one hydrophobic fiber selected from the group consisting of polyester fibers and polypropylene fibers in a weight ration of 20 to 70:80 to 30. The two fibers are drawn so as to show a sea-island form in the cross-section of the fiber bundle, spot-adhered by the partial melt-adhesion of the acrylic synthetic fiber, and the fiber bundle is twisted at a rate of 1 to 30 T/M.

    摘要翻译: 根据本发明,用于书写用具的油墨封闭材料包括(a)和丙烯酸合成纤维的混合物的纤维束和(b)至少一种选自聚酯纤维和聚丙烯纤维的疏水性纤维,其中 重量比为20〜70:80〜30。两根纤维被拉伸以在纤维束的横截面中显示海岛形状,通过丙烯酸类合成纤维的部分熔融粘合点粘附, 纤维束以1〜30T / M的速度捻合。

    Anti-vibration steel material and a production method therefor
    7.
    发明授权
    Anti-vibration steel material and a production method therefor 失效
    防振钢材及其制作方法

    公开(公告)号:US4087289A

    公开(公告)日:1978-05-02

    申请号:US781000

    申请日:1977-03-24

    摘要: Anti-vibration steel materials containing not more than 0.1% of carbon and not more than 0.5% of manganese and having an .alpha. value of not lower than 55, said value being a product of the yield point or stress at 0.2% strain and the grain size number, and a method for producing the same which comprises hot rolling a steel slab, billet or bloom containing not more than 0.1% of carbon, not more than 0.5% of manganese, giving not more than 10% of strain to the hot rolled steel, annealing the hot rolled steel thus strain given at a temperature not lower than its recrystallization temperature but not higher than its A.sub.3 transformation point for at least one minute and controlling the .alpha. value as defined herein to a value not more than 55.

    摘要翻译: 含有不超过0.1%的碳和不超过0.5%的锰并且具有不低于55的α值的抗振钢材,所述值是在0.2%应变下的屈服点或应力的产物和晶粒 尺寸数及其制造方法,其特征在于,将钢坯,含有不超过0.1%的碳,不超过0.5%的锰的钢坯或坯料进行热轧,给予热轧不超过10%的应变 钢,因此在不低于其再结晶温度但不高于其A3相变点的温度下施加至少1分钟的温度下给出的应变,并将本文定义的α值控制为不大于55的值。