公开(公告)号:US4183320A
公开(公告)日:1980-01-15
申请号:US825472
申请日:1977-08-17
申请人: Edwin Erben , Ladislav Koydl
发明人: Edwin Erben , Ladislav Koydl
CPC分类号: C23C16/16 , B04B5/08 , C23C16/455 , C23C16/45578
摘要: A method and apparatus for the nickel-plating of components, in which the finished component, which is to be nickel-plated, is heated to a temperature between 150.degree. and 200.degree. C. and is at the same time subjected to a continuously flowing gas stream containing nickeltetracarbonyl (Ni(CO).sub.4) and an entrainment gas. In this procedure nickel is constantly desposited from the gas phase on the heated surface from the gas stream which continuously flows around the finished component and consists of an entrainment gas and nickeltetracarbonyl. The nickel coating produced by this procedure adheres well, given normal pre-cleaning, and is practically seal-tight even in very thin coating thicknesses (0.1-1.mu.).
摘要翻译: 一种用于镀镍部件的方法和装置,其中将要镀镍的成品部件加热至150至200℃的温度,并同时经受连续流动 含有四羰基(Ni(CO)4)的气流和夹带气体。 在这个过程中,镍从被加热的表面上的气相中不断地从连续地流过最终成分的气流中去除并由夹带气体和四羰基镍组成。 通过这种方法生产的镍涂层在正常的预清洁下保持良好,并且即使在非常薄的涂层厚度(0.1-1μm)下也实际上是密封的。