Production of poly(phenylene sulfide) of an improved reactivity
    1.
    发明授权
    Production of poly(phenylene sulfide) of an improved reactivity 失效
    生产具有改善的反应性的聚(苯硫醚)

    公开(公告)号:US5219959A

    公开(公告)日:1993-06-15

    申请号:US815858

    申请日:1992-01-02

    IPC分类号: C08G75/02

    CPC分类号: C08G75/0295

    摘要: A poly(phenylene sulfide) material containing predominantly para-phenylene sulfide structural units and having a melt viscosity of at least 5 poises (at 300.degree. C.) may be treated or reacted with an alkali metal sulfide and/or hydrosulfide in a polar aprotic solvent at a relatively low temperature in the range of 150.degree.-230.degree. C. so as to introduce an increased amount of reactive thiolate or thiol end groups to the polymer molecule and hence to enhance the reactivity of the polymer material. The thus modified and highly reactive poly(phenylene sulfide) material exhibits an improved compatibility with other polymers and is expected to be useful in preparation of polymer alloys of improved or modified physical and chemical properties.

    摘要翻译: 主要含有对亚苯基硫化物结构单元并且具有至少5泊(在300℃)的熔体粘度的聚(苯硫醚)材料可以与极性非质子中的碱金属硫化物和/或氢硫化物反应 溶剂在150-230℃的较低温度下进行,从而将增加量的反应性硫醇盐或硫醇端基引入聚合物分子,从而提高聚合物材料的反应性。 如此改性和高反应性聚(苯硫醚)材料表现出与其它聚合物的改善的相容性,并且预期可用于制备具有改进或改性的物理和化学性质的聚合物合金。

    Polyethylene and method of production thereof
    2.
    发明授权
    Polyethylene and method of production thereof 失效
    聚乙烯及其生产方法

    公开(公告)号:US5412046A

    公开(公告)日:1995-05-02

    申请号:US212337

    申请日:1994-03-14

    摘要: A polyethylene, having 1 to 60 methyl branches and 1 to 60 hexyl or higher branches per 1000 carbon atoms, a g-value of 0.5 to 0.8, and a limiting viscosity [.eta.] of 0.005 to 20.0 dl/g as measured at 140.degree. C. in o-dichlorobenzene, and a method for producing the same by polymerizing ethylene using a catalyst system comprising a coordination nickel compound of zero- or two-valent nickel and an aminobis(imino)phosphorane represented by a general formula (I): ##STR1## where R.sub.1, R.sub.2, R.sub.3 and R.sub.4 may be the same as or different from each other and are respectively n-alkyl, isoalkyl, aryl or trialkylsilyl, in the presence of .alpha.-olefin.

    摘要翻译: 聚乙烯,每1000个碳原子具有1至60个甲基支链和1至60个己基或更高的支链,g值为0.5至0.8,极限粘度η为0.005至20.0dl / g,在140℃下测量 以及其通过使用包含由0或2价镍构成的配位镍化合物和由通式(I)表示的氨基双(亚氨基)正膦)的催化剂体系使乙烯聚合的制备方法: (I)其中R 1,R 2,R 3和R 4可以彼此相同或不同,并且在α-烯烃的存在下分别为正烷基,异烷基,芳基或三烷基甲硅烷基。

    Easily crystallizable polyphenylene sulfide copolymer and preparation
thereof
    3.
    发明授权
    Easily crystallizable polyphenylene sulfide copolymer and preparation thereof 失效
    易结晶聚苯乙烯磺化共聚物及其制备方法

    公开(公告)号:US5120804A

    公开(公告)日:1992-06-09

    申请号:US596661

    申请日:1990-10-11

    IPC分类号: C08G75/02

    CPC分类号: C08G75/0254 C08G75/0245

    摘要: There are disclosed a class of halogen-ended polyalkylene glycols and halogen-ended polyolefins (II) which are copolymerizable with polyarylene sulfides or sulfone-based polymers. These halogen-ended polymers may be readily copolymerized with polyarylene sulfides or sulfone-based polymers to provide polyphenylene sulfide copolymers (I) exhibiting increased crystallization speeds. These high crystallization speeds enable the copolymers to be molded in a low-temperature mold, for example, at 100.degree. C. or less, while providing fully crystallized moldings having excellent heat resistance properties.