Positive electrode active substance for lithium cell
    4.
    发明授权
    Positive electrode active substance for lithium cell 有权
    锂电池用正极活性物质

    公开(公告)号:US08029929B2

    公开(公告)日:2011-10-04

    申请号:US11630259

    申请日:2005-06-20

    IPC分类号: H01M4/50

    摘要: A positive electrode active material for a lithium battery is provided which offers high-temperature storage property and battery properties and comprises manganese dioxide having a crystal structure that exhibits an X-ray diffraction pattern in which peaks having a peak intensity ratio of not less than 0.05 with respect to the peak at 2θ=37.3°±0.5° are present at positions of 2θ=18.2°±0.5°, 19.5°±0.5°, 28.6°±0.5°, 56.6°±0.5°, 59.1°±0.5°, and 65.1°±0.5°, or further at 2θ=22.0°±1.0°, the X-ray diffraction pattern being obtained using a powder X-ray diffraction device (XRD) that uses CuKα1 rays.

    摘要翻译: 提供了一种锂电池用正极活性物质,其具有高温保存性和电池性,并且具有具有X射线衍射图案的晶体结构的二氧化锰,其峰强度比不小于0.05 相对于2θ处的峰值; = 37.3°±0.5°存在于2°的位置; = 18.2°±0.5°,19.5°±0.5°,28.6°±0.5°,56.6°±0.5°,59.1°±0.5° °和65.1°±0.5°,或进一步在2θ= 22.0°±1.0°,使用CuKα1射线的粉末X射线衍射装置(XRD)获得X射线衍射图。

    Positive Electrode Active Substance For Lithium Cell
    5.
    发明申请
    Positive Electrode Active Substance For Lithium Cell 有权
    锂电池正极活性物质

    公开(公告)号:US20080032198A1

    公开(公告)日:2008-02-07

    申请号:US11630259

    申请日:2005-06-20

    IPC分类号: H01M4/50

    摘要: A positive electrode active material for a lithium battery is provided which offers high-temperature storage property and battery properties and comprises manganese dioxide having a crystal structure that exhibits an X-ray diffraction pattern in which peaks having a peak intensity ratio of not less than 0.05 with respect to the peak at 2θ=37.3°±0.5° are present at positions of 2θ=18.2°±0.5°, 19.5°±0.5°, 28.6°±0.5°, 56.6°±0.5°, 59.1°±0.5°, and 65.1°±0.5°, or further at 2θ=22.0°±1.0°, the X-ray diffraction pattern being obtained using a powder X-ray diffraction device (XRD) that uses CuKα1 rays.

    摘要翻译: 提供了一种锂电池用正极活性物质,其具有高温保存性和电池性,并且具有具有X射线衍射图案的晶体结构的二氧化锰,其峰强度比不小于0.05的峰 在2θ= 18.2°±0.5°,19.5°±0.5°,28.6°±0.5°,56.6°±0.5°,59.1°±0.5°的位置存在相对于2θ= 37.3°±0.5°处的峰值。 和65.1°±0.5°,或进一步在2θ= 22.0°±1.0°,使用CuKalpha1射线的粉末X射线衍射装置(XRD)获得X射线衍射图。