    摘要: A viewing screen (100) for a display device (115) includes a glass substrate (110) having a thermal coefficient of expansion within a range of 3.5×10−6−4.5×10−6 °C.−1. Viewing screen (100) further includes a black matrix (111), which is affixed to glass substrate (110), and which includes a black surround, a ductile metal, and lead titanate. A method for fabricating viewing screen (100) includes the steps of: adding to a black surround paste a ductile metal paste, adding to the black surround paste lead titanate particles, depositing the black surround paste on glass substrate (110), and heating the black surround paste and glass substrate (110) to affix the black surround paste to glass substrate (110), thereby forming black matrix (111). The ductile metal paste and lead titanate particles are added in amounts sufficient to realize an extent of cracking in black matrix (111) upon repeated heating to a temperature within a range of 450-600° C. that is significantly less than that exhibited by an unimproved black matrix, which is made only from the material of the black surround paste.

    摘要翻译: 用于显示装置(115)的观察屏(100)包括具有在3.5×10-6-4.5×10 -6℃-1范围内的热膨胀系数的玻璃基板(110)。 观看屏幕(100)还包括固定在玻璃基板(110)上的黑色矩阵(111),其包括黑色环绕部分,延性金属和钛酸铅。1.一种用于制造观察屏幕(100)的方法,包括: 步骤:向黑色环绕糊料中加入延性金属糊料,加入黑色环绕糊状钛酸铅颗粒,将黑色环绕糊剂沉积在玻璃基板(110)上,并加热黑色环绕糊状物和玻璃基板(110)以贴附 黑色环绕糊状物到玻璃基板(110),由此形成黑色矩阵(111)。 延展性金属糊料和钛酸铅颗粒的添加量足以在反复加热至450-600℃范围内的温度下实现黑色矩阵(111)中的开裂程度,这显着小于由 未经改进的黑色矩阵,仅由黑色环绕糊的材料制成。

    Viewing screen for a display device and method for the fabrication thereof
    2.
    发明授权
    Viewing screen for a display device and method for the fabrication thereof 失效
    显示装置的观看屏幕及其制造方法

    公开(公告)号:US06660324B2

    公开(公告)日:2003-12-09

    申请号:US10123765

    申请日:2002-04-16

    IPC分类号: B05D500

    CPC分类号: H01J29/085 H01J9/2278

    摘要: A method for fabricating viewing screen (100) includes the steps of: adding to a black surround paste a ductile metal paste, adding to the black surround paste lead titanate particles, depositing the black surround paste on glass substrate (110), and heating the black surround paste and glass substrate (110) to affix the black surround paste to glass substrate (110), thereby forming black matrix (111). The ductile metal paste and lead titanate particles are added in amounts sufficient to realize an extent of cracking in black matrix (111) upon repeated heating to a temperature within a range of 450-600° C. that is significantly less than that exhibited by an unimproved black matrix, which is made only from the material of the black surround paste.

    摘要翻译: 一种用于制造观察屏(100)的方法包括以下步骤:向黑色环绕糊状物添加延性金属浆料,将黑色环绕糊状铅酸铅颗粒添加到玻璃基板(110)上,并将黑色环绕糊料沉积在玻璃基板 黑色环绕糊状物和玻璃基板(110),以将黑色环绕糊状物贴合到玻璃基板(110)上,从而形成黑色矩阵(111)。 延展性金属糊料和钛酸铅颗粒的添加量足以在反复加热至450-600℃范围内的温度下实现黑色矩阵(111)中的开裂程度,这显着小于由 未经改进的黑色矩阵,仅由黑色环绕糊的材料制成。