摘要: A method of activating an iron Fischer-Tropsch catalyst by introducing an inert gas into a reactor comprising a slurry of the catalyst at a first temperature, increasing the reactor temperature from the first temperature to a second temperature at a first ramp rate, wherein the second temperature is in the range of from about 150° C. to 250° C., introducing synthesis gas having a ratio of H2:CO to the reactor at a space velocity, and increasing the reactor temperature from the second temperature to a third temperature at a second ramp rate, wherein the third temperature is in the range of from about 270° C. to 300° C. The iron Fischer-Tropsch catalyst may be a precipitated unsupported iron catalyst, production of which is also provided.
摘要翻译: 一种通过将惰性气体引入反应器中来激活铁费 - 托催化剂的方法,所述反应器包括在第一温度下的催化剂浆料,以第一升高速率将反应器温度从第一温度升至第二温度,其中第二 温度在约150℃至250℃的范围内,以空间速度将具有H 2 :CO比例的合成气引入反应器,并将反应器温度从第二温度升至第三温度 第二斜坡率,其中第三温度在约270℃至300℃的范围内。费 - 托催化剂铁可以是沉淀的未负载的铁催化剂,也提供其生产。
-
2.
公开(公告)号:US07915193B2
公开(公告)日:2011-03-29
申请号:US12272960
申请日:2008-11-18
申请人: Belma Demirel , Charles B. Benham , Dan Fraenkel , Richard Bley , Jesse W. Taylor , Bahman Rejai , Sara Rolfe , Harold A. Wright
发明人: Belma Demirel , Charles B. Benham , Dan Fraenkel , Richard Bley , Jesse W. Taylor , Bahman Rejai , Sara Rolfe , Harold A. Wright
IPC分类号: B01J23/42
CPC分类号: B01J37/18 , B01J21/08 , B01J23/745 , B01J23/78 , B01J37/03 , C10G2/332 , C10G2300/4006 , C10G2300/703
摘要: A method of activating an iron Fischer-Tropsch catalyst by introducing an inert gas into a reactor comprising a slurry of the catalyst at a first temperature, increasing the reactor temperature from the first temperature to a second temperature at a first ramp rate, wherein the second temperature is in the range of from about 150° C. to 250° C., introducing synthesis gas having a ratio of H2:CO to the reactor at a space velocity, and increasing the reactor temperature from the second temperature to a third temperature at a second ramp rate, wherein the third temperature is in the range of from about 270° C. to 300° C. The iron Fischer-Tropsch catalyst may be a precipitated unsupported iron catalyst, production of which is also provided.
摘要翻译: 一种通过将惰性气体引入反应器中来激活铁费 - 托催化剂的方法,所述反应器包括在第一温度下的催化剂浆料,以第一升高速率将反应器温度从第一温度升至第二温度,其中第二 温度在约150℃至250℃的范围内,以空间速度将具有H 2 :CO比例的合成气引入反应器,并将反应器温度从第二温度升至第三温度 第二斜坡率,其中第三温度在约270℃至300℃的范围内。费 - 托催化剂铁可以是沉淀的未负载的铁催化剂,也提供其生产。
-